The Fault with Cobalt: Overcoming the Challenges of Battery Metal Exploration

By  -
Overcoming the Challenges of Battery Metal Exploration

Cobalt is an important element used to manufacture rechargeable batteries. Cobalt has unique properties that help improve thermal stability, which is critical for the batteries to function properly. It also helps improve some batteries’ energy density, so they can last longer.

The demand for cobalt is high, so geologists need fast, accurate tools to help them meet these requirements. Portable X-ray fluorescence (pXRF) analyzers are one of these tools, as they provide on-the-spot material chemistry results.

Why Choose Portable XRF for Cobalt Exploration?

Portable XRF provides rapid, in situ, multielement geochemistry for immediate results in the field. This is useful for greenfield and brownfield exploration, ore grade and process control, environmental monitoring and remediation, and researching/teaching within the geological/environmental sciences.

For battery metal exploration, portable XRF provides decision-quality data faster than traditional, lab-based XRF, and also enables more discriminatory laboratory sampling, helping reduce costs and improve ROI. With sample preparation, pXRF produces high-quality quantitative data that is comparable to laboratory analysis.

Challenges with Analyzing Cobalt

XRF is prone to inter-element interferences. Iron (Fe) on cobalt (Co) and nickel (Ni) on cobalt (Co) are two common examples. This means that when a lot of iron is present, it becomes difficult for XRF to identify cobalt at low levels. Likewise, the presence of nickel also makes it difficult for XRF to ID cobalt. Unfortunately, cobalt is routinely explored for in the presence of significant amounts of iron and nickel.

To solve this challenge, we developed a GeoChem method for Vanta pXRF analyzers that offers improved analysis for battery metals exploration by being able to detect cobalt in the presence of iron and nickel. This innovative method overcomes the interference that has historically made it very difficult for portable XRF analyzers to detect cobalt in the presence of these other elements.

The method we developed for the Vanta analyzer is built on the current GeoChem method, but with a more sophisticated way of deconvoluting the iron/cobalt/nickel peaks. Before deploying this solution, we tested it on client samples to make sure that it produced good results.

Test Results

We analyzed 16 samples with high iron content—9% < Fe < 50%, 50 ≤ Co ≤ 6000 ppm, Ni < 500 ppm. We also analyzed 50 samples with a moderate amount of iron—0.5% < Fe < 15%, 16 < Ni < 8000 ppm, 50 ppm < Co < 2.3%. The samples were pulps in XRF cups, and they were analyzed using 60 seconds per beam with no corrections.

The graphs below show excellent agreement between the results obtained from a lab and results obtained using a Vanta portable XRF analyzer, indicating that the modified GeoChem method can accurately detect the presence of cobalt when it’s in the presence of both large and moderate amounts of the interfering elements iron and nickel. Geologists now have another important tool that they can rely on when exploring for new sources of this vital element.

Vanta M Series analyzer docked in a field stand and connected to a PC.
Vanta M Series analyzer docked in a field stand and connected to a PC.

Results - Co

Vanta M Series analyzer docked in a field stand and connected to a PC.

Results - Fe

Vanta M Series analyzer docked in a field stand and connected to a PC.

Results - Co

Vanta M Series analyzer docked in a field stand and connected to a PC.

Results - Fe

Vanta M Series analyzer docked in a field stand and connected to a PC.

Results - Ni

Vanta M Series analyzer docked in a field stand and connected to a PC.

Related Content

The Power of pXRF for Cost-Effective Decisions for Mineral Exploration Programs

Identifying Rock Types and Mineralization with XRF at the Mount Pleasant Mine

Portable XRF Geological Logging with Vanta Analyzers

Marketing Specialist, Analytical Instruments

Michelle has more than 9 years experience in marketing communications and works in Olympus' Analytical Instruments business to promote X-ray fluorescence and X-ray diffraction analyzers. She works with product, engineering, and applications groups for new product launches, to create webinars, and to write application notes.
May 7, 2019
InSight Blog Sign-up

By clicking subscribe you are agreeing to our privacy policy which can be found here.

Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK