The X-STREAM and X-STREAM: Glass are high-speed, automated sorting systems for automatic identification and sorting of material by chemical composition. Take metal, glass and mineral recycling to a new level of high speed, accuracy and profitability.
The X-STREAM is a fully automated in-line system based on proven X-ray Fluorescence (XRF) that identifies scrap material by its chemical composition.
A typical automated XRF sorting system is being composed of a conveyor-mounted spectrometer module, typically containing multiple tubes and detectors to provide the ability to detect and analyze every single piece of scrap material. In only a few milliseconds, the chemical composition of each piece is being calculated, after which customer-defined sorting parameters will determine whether or not to divert that piece out of the main stream.
Key specifications include:
The X-STREAM's software configuration offers flexibility allowing quick, on-site software modifications to meet changing criteria and new market demands.
The X-STREAM incorporates automated, high volume technology that sorts scrap and recyclable material based on highly specific material chemistry, not physical property. With XRF, sorting by elemental composition provides the recycling industry with new sorting opportunities and unique solutions for current challenges; increasing the level of scrap sorting and moving closer to the ideal goal of 100% recycling. This unique system works in tandem with eddy current, induction sorters, and media separation equipment to improve recoveries and increase asset value for metal and glass recyclers. It helps provide maximum value for processed material. It's easy, fast and cost-effective.
Automated XRF sensor technology can be applied to many different types of scrap material, and can therefore serve various recycling industries. Extracting copper meatballs from ferrous shred, sorting of non-ferrous metals by composition or alloy grade and sorting glass are a few of many examples where the X-STREAM technology can be beneficial for scrap processors. Olympus Innov-X is expert in XRF technology and aims to focus on developing and manufacturing the X-Stream sensors only. They are currently being used by sorting system manufacturer BT-Wolfgang Binder who implements the X-Stream sensors into their proven sorting systems.
For more information on X-STREAM sorting systems, please visit BT-Wolfgang Binder GmnbH.
The REDWAVE XRF-M analyzes and evaluates materials according to chemical composition to reliably detect and sort unwanted parts. In contrast to other technologies, moisture, color and surface impurities have no negative effect on the detection ability. This technology can be used in sorting processes to recognize an accumulation of element characteristics, including the detection of undesired materials.
For some time, glass ceramics have been causing problems throughout the glass recycling industry. The melting behavior of glass ceramics is different from that of 'normal' glass; therefore, they will not dissolve in the melting tank at the glassworks, or dissolve only with great difficulty. This poses an array of problems; from serious damage and fire-hazard during the production process to defects or inclusions in the final product. The expanded use of glass ceramics and its tendency to turn up in recycling glass is on the rise; and it is problematic for glass collectors and processors to recognize glass ceramics visually when conducting inspection for incoming materials. In conjunction with the rising glass ceramics problem, glass recyclers are also facing the challenge of keeping the lead content of their glass cullet below a certain level, due to the increased stringency of legeslated regulations.
BT-Wolfgang Binder utilizes X-STREAM sensor technology in their REDWAVE XRF G glass sorting systems which offers glass cullet processors the ability to sort glass by elemental composition. The XRF sensor searches for certain elements such as Titanium, Zinc, Zirconium (which are typical markers for glass ceramics) and Lead. The system then efficiently extracts the contaminations by using air jet diversion. The REDWAVE XRF G systems by BT-Wolfgang Binder are capable of processing up to 28 tons/hour of glass cullet, extracting glass ceramics and leaded glass simultaneously.
Copyright OLYMPUS CORPORATION, todos los derechos reservados.
Global | Condiciones de uso | Política de privacidad | Cookies | Acerca de nosotros | Portal de empleo | Portal de empleo | Mapa del sitio
Copyright OLYMPUS CORPORATION, todos los derechos reservados.
Global | Condiciones de uso | Política de privacidad | Cookies | Acerca de nosotros | Imprint | Portal de empleo | Portal de empleo | Mapa del sitio
Este sitio web usa cookies para mejorar su rendimiento, analizar el tráfico y para fines de valoración de anuncios. Si no cambia la configuración de sus opciones web, las cookies seguirán siendo utilizadas por este sitio web. Para obtener más información sobre cómo usamos las cookies en este sitio web y cómo puede restringir nuestro uso de cookies, por favor revise nuestra política de cookies.