Introduction

Reports are the end result that inspection companies offer their customers. A clear and detailed report can differentiate one company from another by providing more comprehensive results and illustrating concepts that may be difficult to grasp for the end-user.

Challenges in creating a custom report

Since there can be as many types of reports as there are customers, it can be challenging to find one format that fits the needs of every customer. For example, the engineers might need specific calculations to estimate the remaining life of a component to provide their assessment and make educated decisions. Being able to produce this information easily could become critical in some projects.

Solution: export the C-scan

The C-scan export feature is a way to generate a .CSV format file directly from an OmniScan® flaw detector or from OmniPC software. It enables the inspector to export every single data point from an inspection to create a document that contains the entirety of the inspection information.

Users can access the export data function by right clicking in OmniPC software or pressing and holding the C-scan window in an OmniScan flaw detector running MXU 4.2 software and later. A list will appear containing the “Export” option. Once the user clicks or presses “Export,” the .CSV file is generated and saved either on a computer (if using OmniPC software) or on an SD card (if using an OmniScan flaw detector).

Exporting Ultrasonic Data as a .CSV File to Generate Custom Reports

Figure 1. The export option can be selected while in the C-scan view. Right click in OmniPC software or press and hold on the OmniScan screen.

Advantages

The .CSV file can be opened in a variety of programs, such as Microsoft® Excel® software. In Excel software, conditional formatting can be used to make detection and analysis easier and enable the user to look at the same information in different ways.

Exporting Ultrasonic Data as a .CSV File to Generate Custom Reports

Figure 2. A .CSV file opened in Excel software with conditional formatting in color to display corrosion.

Exporting Ultrasonic Data as a .CSV File to Generate Custom Reports

Figure 3. A .CSV file opened in Excel software with conditional formatting in 3D to display corrosion.

Exporting Ultrasonic Data as a .CSV File to Generate Custom Reports

Figure 4. Different options to display data in 3D.

Features such as automatically listing the position of a pit and showing average thickness, minimum thickness, and the proportion of an area under a predefined thickness threshold can easily be implemented using third-party software. The .CSV file format is compatible with a variety of NDT programs as well as pipeline burst pressure calculators.

Conclusion

The export C-scan option in OmniPC software or onboard the OmniScan® flaw detector software (version 4.2 and later) enables users to view and analyze their inspection data and opens up possibilities for displaying important information and providing remaining life calculations.

Olympus IMS
Products used for this application

This new software is the most efficient and affordable option for OmniScan data analysis, and features the same analysis tools provided in the OmniScan onboard software, with the added flexibility of running on a personal computer.
The single group, lightweight OmniScan SX features an easy-to-read 8.4 inch (21.3 cm) touch screen and provides cost-effective solutions. The OmniScan SX comes in two models: the SX PA and SX UT. The SX PA is a 16:64PR unit, which, like the UT-only SX UT, is equipped with a conventional UT channel for P/E, P-C or TOFD inspections.
The OmniScan MX2 now features a new phased array module (PA2) with a UT channel, and a new two-channel conventional ultrasound module (UT2) that can be used for TOFD (Time-of-Flight Diffraction), as well as new software programs that expand the capabilities of the successful OmniScan MX2 platform.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK