Immersion special transducers refer to a variety of transducers that conduct many specific applications such as measuring wall thickness, inspection of aluminum plating, or multi-element array flaw detection.This group contains the following transducer types: side looking case, paintbrush, i-R style and XMS.
Part
Numbers |
Freq.
|
Nominal
Element Size |
Focus
| |
MHz
|
inches
|
mm
| inches | |
V3591 |
10
|
0.125
|
3
| 0.50 OLF |
V3343 |
20
|
0.125
|
3
| 0.50 OLF |
Note: All above side looking immersion transducers have straight Microdot connectors.
Accuscan Paintbrush
| Transducer Dimensions (in inches)
For 7.5 MHz and 10 MHz, case height (A) is 0.62" |
*Please select a specific focus between min max.
**If a focus is required, select a focal length between min max
To view point target foci, click here.
Frequency (MHz) | Nominal Element Size | ACCUSCAN-S | ||||
---|---|---|---|---|---|---|
in. | mm | Part / Item No. | ||||
2.25 | 2.00 x 0.25 | 51 x 6 | A340S-SUU8421045
|
The XMS transducer is an extremely small 10 MHz immersion transducer with a 3 mm (0.118") diameter by 3 mm (0.118") long case. This transducer is ideal for extremely tight access areas or for multi-element array flaw detection. The transducer assembly has a special connector attached to the 1 m (38") long potted cable. An adaptor is also available to interface with most commercial ultrasonic equipment.
Frequency |
Nominal Element Size
| Part Number | Included Adapter | |
MHz | inches | mm | ||
10 | .080 | 2 | XMS-310-B | BNC |
10 | .080 | 2 | XMS-310-L | Lemo ® 01 |
i-R Style Housings0.50 inches (10 mm) element diameters in 0.75 inches (19 mm) x 0.75 inches (19 mm) rectangular housings with side mount (right angle), UHF connectors, and 303 stainless steel case housings are available. Transducer Configurator*To view transducer point target focus, click here. |
Frequency (MHz) | Nominal Element Size | Power Series | Resolution Series | Standard Series | ||||||
---|---|---|---|---|---|---|---|---|---|---|
in. | mm | Part / Item No. | Part / Item No. | Part / Item No. | ||||||
0.5 | 0.5 | 13 | IR-0008-P-RUU8518044
| |||||||
1 | 0.5 | 13 | IR-0108-P-RUU8518046
| |||||||
2.25 | 0.5 | 13 | IR-0208-P-RUU8518050
| |||||||
5 | 0.5 | 13 | IR-0508-R-RUU8518057
| IR-0508-S-RUU8518058
| ||||||
10 | 0.5 | 13 | IR-1008-R-RUU8518061
| IR-1008-S-RUU8518062
|
You are being redirected to our local site.