Thickness Measurements of Polymer Aircraft Windshields


Inspector measure thickness of aircraft windsheild using a 35Application: Measurement of individual layers and total thickness in multilayer polymer aircraft windshields.

Background: Multilayer plastic construction is commonly employed by the aerospace industry for aircraft windshields, in which two relatively thick layers of acrylic or a similar hard plastic are typically sandwiched around a thinner layer of a soft material such as polyvinyl butyral (PVB) which provides thermal stress relief. The hard plastic layers are typically about 0.4 in. to 0.5 in. (10 to 12.5 mm) thick and the soft inner layer about 0.050 in. (1.25 mm) thick.

Scratches in aircraft windshields are typically removed by polishing during routine maintenance, after which thickness measurement is required to insure that windshield thickness has not been reduced below a specified minimum. Additionally, manufacturers need to measure the soft PVB middle layer to insure that it is within specified thickness.

Equipment: The Model 38 DL PLUS thickness gage with the Multi-Measurement software option is recommended for measurement of individual layers and total part thickness in this application. With this software, the 38DL PLUS gage is capable of using separately programmed setups (including sound velocity, gain, and blanking settings) for each layer being measured to optimize performance. In this test, the gage is normally used with either an M110-RM (5 MHz) or M112-RM (10 MHz) contact transducer.


Typical Procedure: The waveforms below show simultaneous measurement of all three layers of a typical multilayer aircraft windshield using an M110 (5 MHz) contact transducer. The outside layer is measured in Mode 1, to the first negative echo. The thin middle layer is measured in Mode 2, negative peak to positive peak. The bottom layer is also measured in Mode 2, positive to negative. The small echo just to the left of the detected backwall echo in the bottom screen print is not another layer, but rather a second multiple of the backwall echo from the outer layer.

outside polycarbonate layer
outside polycarbonate layer

middle PVB layer
middle PVB layer

bottom polycarbonate layer
bottom polycarbonate layer


As with any ultrasonic thickness measurement, accuracy is dependent on proper sound velocity calibration. Velocity calibration must be performed for each material being measured, on samples of known thickness.

Olympus IMS

Productos para la aplicación

El medidor de espesores ultrasónico 72DL PLUS™ ofrece mediciones de espesor precisas y avanzadas a alta velocidad en un dispositivo portátil y fácil de usar. Compatible con sondas monoelemento de hasta 125 MHz, esta innovadora herramienta de medición de espesores es idónea para determinar el espesor de materiales ultrafinos, como la pintura, los revestimientos y el plástico de múltiples capas. Puede mostrar de forma simultánea el espesor de hasta seis capas.

El 45MG es un avanzado medidor de espesores ultrasónico que cuenta con funciones de medición de serie y opciones de software. Está exclusiva herramienta de medición de espesores es compatible con nuestro rango completo de sondas duales y monoelementos dedicadas a medir espesores.

El versátil medidor de espesores 38DL PLUS™ puede ser usado con sondas duales para medir el espesor de tuberías corroídas, como también para ejecutar mediciones de espesor muy precisas de materiales delgados o multicapa mediante el uso de una sonda monoelemento. 
Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.