Standard angle beam transducers are large single element transducers used with a wedge to introduce a refracted shear wave or longitudinal wave into a test piece.
Nominal
Element Size | (A) | (B) | (C) | (D) |
1.00 | 1.25 | 0.63 | 1.38 | 1.65 |
0.50 x 1.00 | 0.73 | 0.63 | 1.31 | 1.53 |
0.50 | 0.72 | 0.63 | 0.81 | 1.02 |
Frequency (MHz) | Nominal Element Size | ACCUSCAN-S | CENTRASCAN | VIDEOSCAN | ||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|
in. | mm | Part / Item No. | Part / Item No. | Part / Item No. | ||||||||
0.5 | 0.50 x 1.00 | 13 x 25 | A413S-SBU8431012
| V413-SBU8436010
| ||||||||
0.5 | 1 | 25 | A414S-SBU8431013
| V414-SBU8436011
| ||||||||
1 | 0.50 x 1.00 | 13 x 25 | A401S-SBU8431001
| C401-SBU8435001
| V401-SBU8436001
| |||||||
1 | 0.5 | 6 | A402S-SBU8431002
| C402-SBU8435002
| V402-SBU8436002
| |||||||
1 | 1 | 25 | A407S-SBU8431007
| C407-SBU8435007
| V407-SBU8436007
| |||||||
2.25 | 0.50 x 1.00 | 13 x 25 | A403S-SBU8431003
| C403-SBU8435003
| V403-SBU8436003
| |||||||
2.25 | 0.5 | 13 | A404S-SBU8431004
| C404-SBU8435004
| V404-SBU8436004
| |||||||
2.25 | 1 | 25 | A408S-SBU8431008
| C408-SBU8435008
| V408-SBU8436008
| |||||||
3.5 | 0.50 x 1.00 | 13 x 25 | A412S-SBU8431011
| C412-SBU8435011
| ||||||||
3.5 | 0.5 | 13 | A415S-SBU8431014
| C415-SBU8435012
| ||||||||
3.5 | 1 | 25 | A411S-SBU8431010
| C411-SBU8435010
| ||||||||
5 | 0.50 x 1.00 | 13 x 25 | A405S-SBU8431005
| C405-SBU8435005
| V405-SBU8436005
| |||||||
5 | 0.5 | 13 | A406S-SBU8431006
| C406-SBU8435006
| V406-SBU8436006
| |||||||
5 | 1 | 25 | A409S-SBU8431009
| V409-SBU8436009
|
Nominal
Element Size | Wedge Part Numbers | ||||
inches | mm | Accupath* |
High Temp*
500°F (260°C) |
Very High Temp*
900°F (480°C) | Surface Wave 90° |
1.00 | 25 | ABWS-3-X° | ABWHT-3-X° | ABWVHT-3-X° | ABWSL-3-90° |
0.50 x 1.00 | 13 x 25 | ABWS-2-X° | ABWHT-2-X° | ABWVHT-2-X° | ABWSL-2-90° |
0.50 | 13 | ABWS-1-X° | ABWHT-1-X° | ABWVHT-1-X° | ABWSL-1-90° |
*Wedges are available in standard refracted shear wave angles of 30°, 45°, 60°, and 70° in steel at 5.0 MHz.
Accupath and Surface Wave Wedge Dimensions (Standard) | |||||||||||||||
Nominal Element Size (in inches) | |||||||||||||||
1.00 | 0.50 x 1.00 | 0.50 | |||||||||||||
(A) | (B) | (C) | (D) | (A) | (B) | (C) | (D) | (A) | (B) | (C) | (D) | ||||
30° | 1.69 | 2.15 | 1.62 | 1.15 | 1.30 | 1.30 | 1.60 | 0.76 | 1.20 | 1.42 | 1.10 | 0.83 | |||
45° | 1.47 | 1.96 | 1.63 | 0.97 | 1.30 | 1.41 | 1.60 | 0.78 | 1.20 | 1.31 | 1.08 | 0.70 | |||
60° | 1.50 | 2.18 | 1.63 | 1.00 | 1.30 | 1.50 | 1.60 | 0.67 | 1.20 | 1.48 | 1.08 | 0.68 | |||
70° | 1.50 | 2.47 | 1.63 | 1.13 | 1.35 | 1.77 | 1.60 | 0.85 | 1.20 | 1.58 | 1.09 | 0.68 | |||
90° | 1.50 | 2.50 | 1.65 | 0.44 | 1.20 | 1.34 | 1.60 | - | 1.20 | 1.34 | 1.00 | - |
Compatible with our Miniature Screw-In and Standard Angle Beam transducers
Transducer
Case |
Nominal
Element Size | Wedge Part Numbers | |||||
inches | mm | 30° | 45° | 60° | 70° | 90° | |
Screw-In | 0.50 | 13 | ABWM-5053T | ABWM-5027T | ABWM-5028T | ABWM-5029T | ABWML-5041T |
0.375 | 10 | ABWM-7024T | ABWM-7025T | ABWM-7026T | ABWM-7027T | ABWML-7028T | |
0.25 | 6 | ABWM-4086T | ABWM-4087T | ABWM-4088T | ABWM-4089T | ABWML-4074T | |
Standard | 1.00 | 25 | ABWS-3028 | ABWS-3016 | ABWS-3029 | ABWS-3030 | ABWSL-3039 |
0.50
x 1.00 |
13
x 25 | ABWS-2021 | ABWS-2022 | ABWS-2023 | ABWS-2024 | ABWSL-2056 | |
0.50 | 13 | ABWS-1033 | ABWS-1034 | ABWS-1035 | ABWS-1036 | ABWSL-1045 |
Copyright OLYMPUS CORPORATION, Tous droits réservés.
Global | Modalités d'utilisation | Déclaration de confidentialité | Fichiers de témoins | À notre sujet | Carrières | Carrières | Plan de site
Copyright OLYMPUS CORPORATION, Tous droits réservés.
Global | Modalités d'utilisation | Déclaration de confidentialité | Fichiers de témoins | À notre sujet | Imprint | Carrières | Carrières | Plan de site
Ce site utilise des témoins de connexion pour augmenter la performance, mesurer le nombre de visiteurs et vérifier la pertinence des publicités. À moins de modifier les paramètres de votre navigateur, ces témoins continueront d’être utilisés pour ce site. Pour en savoir plus sur la façon dont nous les utilisons et sur la façon d’en restreindre l’usage, veuillez consulter notre politique sur les témoins de connexion.