CARTER super magnetic bias probes offer an ultradurable construction with hardened steel wear surface for a long life in harsh environments. These probes are designed to suppress permeability noise in mildly ferritic material such as Monel, 3RE60, SEA‑CURE, and 400-series stainless.
TEO are limited to mildly ferritic tube inspection of thicknesses below 1.5 mm. In other contexts, the probe is not likely to provide adequate magnetic saturation of the tube wall.
Use the nomenclature and the chart below to configure your part number.

| Probe Type |
Probe Diameter
(use mm in part ID) | Center Frequency | Cable Length | |
| mm | in. | |||
| TEO: Carter probe | Standard 11 mm to 22.2 mm by 0.2 mm | Standard 0.433 in. to 0.874 in. by 0.008 in. |
015 (Low)
050 (Mid) 250 (High) 600 (Very High) |
15 m (50 ft)
20 m (65 ft) 30 m (100 ft) |