Post-Fire Examination of the Notre-Dame de Paris Stone Vaults

저자  -
The Notre-Dame cathedral on fire

The following account of the efforts to restore the Notre-Dame de Paris Cathedral  is based on the article “Notre-Dame de Paris―la pierre des voûtes auscultée,” which appeared in Issue No. 78 of Controls Essais Mesures (CEM) magazine (translated from French).

The Notre-Dame Cathedral Is Burning: A Fire That Shocked the World

On April 15, 2019, a devastating fire ravaged Notre-Dame de Paris, leaving behind profound scars. While the iconic cathedral remained standing, its structural integrity came into question. In the aftermath of the tragedy, Jean-Christophe Mindeguia, a researcher from the University of Bordeaux, embarked on a mission to assess the residual stability of the cathedral's stone vaults.

Notre-Dame restoration. Notre-Dame cathedral (Paris) was damaged by fire on 15 april 2019

Collaborative Efforts for Reconstruction

In collaboration with the Ministry of Culture and the CNRS (French National Centre for Scientific Research), a team of researchers, led by Jean-Christophe Mindeguia, undertook the task of examining the stone vaults to assist in the monument's reconstruction. Describing the team’s mission and the answers they were seeking, Jean-Christophe explains, “What is the current condition of the cathedral? What are the suitable reinforcement techniques? Where can these be applied? We were attempting to provide answers to these questions within the framework of the cathedral's reconstruction.”

Examining the Composition and Condition of the Vaults

The cathedral’s vaults are predominantly composed of stone and mortar joints. While the University of Bordeaux focused on studying the mechanical state of the stone, the Jean Lamour Institute at the University of Lorraine concentrated on the mortar. Jean-Christophe elaborates, “The vaults are mainly composed of two materials: stone and mortar joints. We are interested in the mechanical state of the stone and the stone-joint assembly, with the Jean Lamour Institute working on the mortar.”

Seeking Deeper Insights in Exploring the Vaults

To gain deeper insights into the stone’s condition, Jean-Christophe Mindeguia conducted core drillings in the choir vault in July 2021. Describing the process, Jean-Christophe explains, “The effect of the heat on the vaults can be observed on the surface. However, we wanted to see inside the material. We carried out six core drillings in the choir vault – it had been unaffected by falling objects, but its structure was deformed following the fire. The analysis of these samples allowed us to estimate the temperature reached by the stone. We also noticed that the cores came out in several pieces, so we questioned whether the coring process caused this detachment or were there cracks already present. I contacted Evident about a videoscope to obtain images inside the holes left by the cores. The holes are about fifteen centimeters deep and three centimeters in diameter.”

Restoration workers wearing PPE examine the condition of the vaults of the Notre Dame de Paris cathedral after the fire via borescope inspection

Utilizing Advanced RVI Technology: Our IPLEX NX Video Borescope

To visualize the interior of the drill holes and locate cracks accurately, the team employed the IPEX™ NX video borescope. Jean-Christophe describes the utility of using video borescope inspection technology, stating, “With the naked eye, only the first few centimeters of the hole were visible from the opening. The videoscope gave us an ’eye on the inside.’  It’s compact, which enabled us to navigate through a forest of scaffolding with it. The videoscope offered us the possibility to visualize the inside of the core drill holes on a remote screen.”

Olympus video borescope display showing an image of the wooden beams in the Notre Dame cathedral during restoration work

Progress on the Road to Restoration

Through collaborative efforts and advanced technology, Jean-Christophe Mindeguia and other researchers are making significant strides in assessing the structural integrity of Notre-Dame de Paris. With ongoing modeling of the vaults using collected data, these efforts represent a crucial step toward the cathedral’s restoration and preservation for future generations.

Aerial drone view of Notre-Dame Cathedral during reparation works in Paris, France.

To learn more about our IPLEX series, visit www.olympus-ims.com/remote-visual-inspection/videoscope/

Read about some other interesting applications of our video borescopes at the links below.
 

Related Content

5 Traits a Videoscope Needs to Stand Up to the Rigors of Search and Rescue Operations

A Rat’s-Eye View: Revealing the Secret Lives of Nature’s Covert Creatures with Borescopes and Videoscopes

The Nepal Earthquake: Using Remote Video to Help Save Lives

전속 작가

Sarah는 2013년 Olympus의 마케팅 및 커뮤니케이션 부서에 합류하기 전에, 방송 미디어 업계에서 거의 10년 동안 연구원 및 카피라이터로 근무했습니다. 이제 Sarah는 작가이자 편집자로서 Olympus 제품 및 전문 분야와 관련된 주제에 대해 설득력 있고 뛰어난 품질의 자료를 만드는 데 자신의 전문성을 집중시키고 있습니다. 그녀는 초음파(UT) 및 와전류 검사(ECT), 위상 배열(PA), 전체집속기법(TFM) 및 풀 매트릭스 캡쳐(FMC), 산업 현미경 및 비디오스코프 등의 비파괴 검사(NDT) 저술을 써왔습니다. 그녀는 종종 우리 주변 환경의 수준과 안전을 향상시키는 Olympus 제품의 공헌에 대해 다룹니다. Sarah는 퀘벡시의 사무소에서 근무하며, 배우자인 David와 세 자녀인 Sophie, Anouk, Éloi.와 함께 살고 있습니다.

4월 2, 2024
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
InSight 블로그 가입하기
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
아래 양식을 작성하여 원하는 내용을 알려주십시오.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.