Evident LogoOlympus Logo
자료실
Application Notes
자료로 돌아가기

채굴용 중장비 러그 또는 보어 검사


excavator mining

Surface mining often entails the use of large trucks and shovels including massive Dragline excavators in large scale operations to remove overburden to access coal and other deposits of desired resources. Due to the size of this equipment many of the components are very thick resulting in challenging applications for ultrasound. In addition the preferred test methods are with the components in place and in operation which can mean limited access to the areas that need inspected. Phased Array can offer many benefits to these inspections. There are many lug and bore type components utilized to hold various shafts and pins that allow equipment operation.

Lug and Bore Inspections

Lug and bore inspections typically can be very thick wall (7-12” +). A typical high stress area prone to cracking is the inner bore. It is preferred to inspect these components with the pin or shaft in place to allow continued operation of the piece of equipment. For conventional shear wave ultrasonics this poses a limited access issue and often multiple wedges must be changed to inspect as much of the inner bore as possible.


Typical Lug
Typical Lug in Place in Dragline Excavator


  Typical UT and PA coverage
Typical Coverage from Conventional Ultrasonics and Phased Array. Red line shows possible limited access

Phased Array Benefits

  • Multiple angles allow for single probe and large coverage area in lug bore
  • Better detection of "winding crack"
  • Better coverage when in position with limited access
  • Imaging and data recording for crack monitoring

Typical inspection
Typical Lug for Bore inspection utilizing OmniScan SX. This component has the boom of a dragline excavator.

PA readout
Phased Array allows simultaneous viewing of bore geometry and cracks propagating from the inner surface.

Equipment Used

OmniScan SX or MX2

  • Portable for easy access inside cramped area of excavator
  • Conventional, Phased Array and TOFD capable
  • Manual or encoded data

Phased Array Probes and Wedges

  • Vary on application
  • 2.25 MHz common frequency
  • Shear and 0 degree wedges
  • Contact wear faces for long 0 degree metal paths

Optional Software and Accessories

Olympus IMS

이 애플리케이션에 사용되는 제품
이 새로운 소프트웨어는 옴니스캔 데이터 분석을 위한 가장 효율적이고 저렴한 선택으로, 옴니스캔 온보드 소프트웨어에 제공되는 것과 동일한 분석 도구를 갖추고 있으며, 개인용 컴퓨터에서 실행할 수 있는 유연성이 더해졌습니다.
미니 휠 인코더는 스캔 축의 결함의 위치 결정 및 치수 결정에 사용됩니다. 데이터 수집과 프로브 이동을 동기화시킬 수 있습니다. 또한 방수성이며, Olympus 표준 PA 쐐기와 호환됩니다.
단일 그룹인 경량 옴니스캔 SX는 읽기 쉬운 8.4인치(21.3cm) 터치 스크린을 갖추고 있으며, 비용 효율적인 솔루션을 제공합니다. 옴니스캔 SX는 SX PA와 SX UT의 두 가지 모델로 제공됩니다. SX PA는 UT 전용 SX UT와 마찬가지로 P/E, P-C 또는 TOFD 검사를 위한 재래식 UT 채널을 장착한 16:64PR 장치입니다.