Olympus manufactures custom immersion flat with radius (IFWR) phased array probes to increase coverage, improve detectability, and simplify data analysis. Mistras Group Inc. has increased productivity by using a single custom Olympus 3.5MHz 64 element IFWR probe; replacing two probes in their composite inspection setup. Mistras Group Inc. provided the following details and graphics outlining their success.

Old Technique

Mistras previously used 1 linear 64 element, 1 concave 32 element probe, and the OmniScan MX to inspect 8 zones across a composite part. The inspection with two probes took approximately 2.5 hours.

Figure 1: 8 zones to cover the entire composite piece
Figure 1: 8 zones to cover the entire composite piece

Firgure 2: Two setups required to cover the entire partFirgure 2: Two setups required to cover the entire part


Firgure 2: Two setups required to cover the entire part

The C-scan data recored from multiple probes and passes becomes more difficult to record and analyze. Each scan must be properly identified to ensure acurrate analysis.

Figure 3: C-scan data is recored for each zone
Figure 3: C-scan data is recored for each zone

New Technique

Using the Olympus custom IFWR probe, inspection of all 8 zones can be completed with one probe in two passes; reducinig inspection time by approximately 50%.

Figure 4: Custom Immersion Flat With Radius (IFWR) probe setup
Figure 4: Custom Immersion Flat With Radius (IFWR) probe setup

Reducing quantity of probes while increasing coverage has proven to simplify recording and analyzing data. Each part now has only two C-scan’s to analyze.

Figure 5: Data captured from one pass covers 4 zones
Figure 5: Data captured from one pass covers 4 zones

Conclusion

Olympus has worked with Mistras Group Inc. to provide a custom probe which has proven to reduce inspection time, improve detectability, and simplify data analysis. Olympus has the capability to manufacture IFWR probes to customer specifications and specific part requirements.

To inquire for custom probe possibilities specific to your application please contact SCE.PM@olympusndt.com or submit details via our online custom probe form.

Olympus IMS

Produkty použité pro tuto aplikaci

Každý defektoskop řady OmniScan™ X3 má kompletní sadu funkcí phased array.

Inovativní TFM a pokročilé funkce PA vám pomohou s jistotou identifikovat defekty, zatímco výkonné softwarové nástroje a jednoduché pracovní postupy zvyšují vaši produktivitu.

The single group, lightweight OmniScan SX features an easy-to-read 8.4 inch (21.3 cm) touch screen and provides cost-effective solutions. The OmniScan SX comes in two models: the SX PA and SX UT. The SX PA is a 16:64PR unit, which, like the UT-only SX UT, is equipped with a conventional UT channel for P/E, P-C or TOFD inspections.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country