Special Applications Transducers include combination longitudinal/shear mode transducers, polymer (PVDF) immersion transducers, captive water column transducers and many more. They provide solutions for a variety of applications in flaw detection, thickness gaging, and materials research.

Roller transducers are used in testing metallic or non-metallic materials for bonding/segregation in CFRP/GRP including Kevlar®, rubber friction materials, and high density products such as glass, and metallic and plastic weldments. This series includes roller and contact type transducers at 0.5 MHz and 1.25 MHz. Contact units are available in 5, 10, and 15 mm diameters, while the roller transducers incorporate a 5 mm crystal giving a 10 mm footprint through the replaceable tire. Both styles are fitted with axial mounted Microdot connectors (other connectors available on request). The roller transducer can be ordered with either a single or dual yoke design.

Frequency (MHz)
Size
Yoke
Wheel Diameter
Part Number
in.
mm
in.
mm
1.25
0.187
5
Single
1.0
25
RT-0105-16SY
1.25
0.187
5
Dual
1.0
25
RT-0105-16DY
0.50
0.187
5
Single
1.0
25
RT-0005-SY
0.50
0.187
5
Dual
1.0
25
RT-0005-DY

Spare Tires
Part Number
Wheel Diameter
RT-16-10T
1.0 in.
25 mm

Roller transducers are used in through transmission mode for fast linear scans of parts without the need for an immersion setup. Roller transducers are typically used in applications looking for de-laminations in multilayer materials and are available in either single or dual yoke designs feature a removable and replaceable tire.

Polymer (PVDF) Immersion Transducers

High frequency polymer (PVDF) transducers are focused immersion transducers with very broad bandwidth, whose element provides an excellent impedance match to water that results in a better transfer of sound energy. These transducers also eliminate the need for the fused silica delay lines typically found in high frequency immersion transducers, removing the echo multiples associated with delay lines. Note: Polymer transducer center frequencies are based on the film thickness of the polymer film element. Performance is highly dependent on pulser and cable characteristics and effective center frequency may be 15 - 25% lower than the nominal value.

Frequency Nominal
Element Size
Part Number Standard Focal Lengths
MHz inches inches
15 0.25 PI15-2-RX.XX" 1.00
20 0.25 PI20-2-RX.XX" 0.50, 1.00, 1.50, 2.00
35 0.25 PI35-2-RX.XX" 0.50, 0.75, 1.00, 1.50, 2.00
50 0.25 PI50-2-RX.XX" 0.50, 0.75, 1.00, 1.50, 2.00
75 0.125 PI75-1-RX.XX" 0.50, 1.00

Note: Please replace X.XX" with the standard focal length of your choice.
• Due to the fact that polymer transducers are inherently broadband, their center frequency may be lower than the frequency indicated on the transducer

Continuous High Temperature
Delay Line Transducer

This transducer can continuously withstand temperatures as high as 350°F (175°C) and pressures up to 85 PSIG. One typical application is to monitor the cure of materials in autoclave.
Part number is X2002, (2.25 MHz, 0.5 inch, 13 mm diameter)

Low Frequency Narrowband Transducers

Meant for use in pairs for through transmission in materials such as concrete, wood, and geological samples, these are available in frequencies of 50 kHz (X1021), 100 kHz (X1020), and 180 kHz (X1019). Recommended instruments are high voltage pulser-receivers such as the Model 5058PR or 5077PR Square Wave Pulser

Combination Longitudinal/Shear Mode Transducers

These transducers generate simultaneous longitudinal waves and shear waves in either single element, dual element or three element arrangement. They can be custom designed for different frequencies and element sizes.

500 kHz Broadband/Highly Damped Transducers

This highly damped transducer measures the thickness of fiberglass, composites, and other attenuating materials. This transducer can also be used with a NWC-302 Nylon Wear Cap for flaw detection on thick or rough surfaced casting materials.
Part number is M2008, (1 inch, 25 mm diameter).

Variable Angle Beam Wedge

The Variable Angle Beam Wedge allows the user to adjust the incident angle from 0° to 50° to create refracted angles in steel from 0° to 90°. The wedge is to be used with the 0.50" x 1.00" Standard Angle Beam Transducers (see Angle Beam Transducers).
Wedge Part Number = ABWX-2001

Loading...

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어