XRD and XRF Analysis of Deep-Sea Polymetallic Manganese Nodules

By 

Portable and benchtop X-ray diffraction (pXRD) analyzers can play an important role in the exploration and analysis of manganese (Mn) nodules. These deep-sea deposits contain high concentrations of valuable metals, including nickel, cobalt, and copper, as well as significant amounts of lithium, vanadium, molybdenum, and yttrium, making them valuable for future extraction in many industries.1

The search for these metals is critical to mineral exploration and mining companies, as many current and future electronics will depend on both these essential metals and some rarer metals. Because these polymetallic deposits contain a very large quantity of both groups, they possess a potential for huge economic viability. Additionally, as these nodules are nearly 100% metallic ore, there are no toxic tailings or mine waste during extraction.2

Location of all known Mn polymetallic nodules.

Figure 1. Location of all known Mn polymetallic nodules, with the five zones of most likely potential industrial exploration outlined in red. Source: National Centers for Environmental Information3.

While commercial extraction and mining has not yet been implemented for a variety of reasons, the high potential economic impact of these deposits cannot be ignored. In order to properly develop this technology, a way to characterize these nodules in the field must be used.

Elemental Analysis of Deep-Sea Nodules Using Vanta pXRF Analyzers

An Olympus Vanta™ pXRF analyzer can identify and quantify nearly every element between magnesium (Mg) and uranium (U), including the high-value first row transition metals, such as vanadium, nickel, copper, and cobalt, and other high-value metals such as molybdenum and yttrium. Other valuable materials, such as near rare earths and iron ore, can also be easily and readily quantified.

Mineral Identification of Manganese Nodules Using Olympus pXRD Analyzers

The Olympus TERRA™ II XRD analyzer is the successor to the world’s first commercial battery-operated, portable XRD instrument. Together with the BTX™ III benchtop XRD analyzer, these pXRD instruments can identify and quantify tens of thousands of various minerals, synthetics, and biologic phases in a single sample. Users can determine the grade, purity, and quantity of specific types of metallic ore in real time onsite, regardless of the chemistry and orientation.

Inline calculation by the Vanta pXRF analyzer of high-value metals in Mn nodules

Figure 2. Inline calculation on the Vanta pXRF analyzer of highvalue metals in Mn nodules.

As shown in the diffractogram below, Olympus pXRD analyzers can quickly identify various phases in deep-sea manganese nodule samples. Each component of the sample can be identified and quantified in real time using the integrated SwiftMin® automated phase ID and quantitative software, or with standalone software packages such as XPowder software. These options make it even easier and faster to quantify phase information and mineralogy.

mn-nodules-3
mn-nodules-4

Figure 3. Diffractograms and quantification taken from the Cu-anode BTX III analyzer of three different deep-sea manganese nodules, some of which were taken from the Clarion-Clipperton Zone (CCZ). Each nodule contains a variety of minerals; the diffraction patterns for the dominant phases are shown.

Users can process this information on-site and in real time to better understand the composition of nodules without the need for expensive and slow laboratory testing. Nearly any naturally occurring phase can be identified and quantified using this technique, including common manganese nodule minerals such as birnessite or todorokite, hydrated sulfates such as jouravskite and halotrichite, and other minerals such as aragonite, calcite, and kaolinite.

3-D structure of birnessite4 (left) and todorokite5 (right)

Figure 4. 3D structure of birnessite44 (left) and todorokite55 (right), which are common minerals in deep sea nodules.

  • Fast acquisition: go from sample prep to analysis in minutes
  • Virtually maintenance-free: runs without the need for compressed gas, water cooling, a secondary chiller, or external transformer to decrease downtime and costs
  • Easy sample prep: simple mortar-and-pestle process can be done by operators of all experience levels in the field quickly and without complex equipment
  • Small sample holder: only requires 15 mg of material compared to the large batch required for conventional XRD

References

  1. McKelvey, V. E., 1983. Analysis of the World Distribution of Metal-Rich Subsea Manganese Nodules. US Department of the Interior, US Geological Survey.
  2. International Seabed Authority, 2010. A Geological Model of Polymetallic Nodule Deposits in the Clarion-Clipperton Fracture Zone. ISA Technical Study Series, International Seabed Authority.
  3. Frazer, Jane and Mary Fisk (1981): Scripps Institution of Oceanography Ferromanganese Nodule Analysis File - IDOE Portion. National Geophysical Data Center, NOAA.
  4. Post, J.E. and Veblen, D.R., 1990. Crystal structure determinations of synthetic sodium, magnesium, and potassium birnessite using TEM and the Rietveld method. American Mineralogist, 75, pp.477-489.
  5. Post, Jeffery E. and Bish, David L., 1988. Rietveld refinement of the todorokite structure. American Mineralogist, 73, pp.861-869.

Application Scientist, XRF Technologies

Josh Litofsky holds a bachelor’s degree in physics from Beloit College and PhD in chemical engineering from Pennsylvania State University. For his PhD, he focused his research on advanced characterization of designer materials using X-ray diffraction. From 2019 to 2022, Josh brought his expertise to Evident as an application scientist, supporting our X-ray fluorescence (XRF) analyzers to provide enhanced solutions to customers. In his free time, Josh enjoys running and has run the fastest 100k in the state of Pennsylvania.

Olympus IMS

この用途に使用される製品
VANTAシリーズは携帯性に優れたハンドヘルドタイプながら、素早く高精度な成分分析が可能で、質の高い分析結果を得ることができます。 IP55またはIP54相当の防塵・防水性能を備え、落下試験にも合格しているため、厳しい環境での分析業務にも対応することができます。

Vanta Element™ハンドヘルド蛍光X線(XRF)分析計シリーズは、高速性、堅牢性、接続性を、費用効果の高い2つのモデルで提供します。 Vanta Element分析計は手頃な価格で合金判定が可能です。Vanta Element-S分析計は軽元素の検出機能が搭載され、合金判定を手頃な価格で行うことができます。 材料および合金品種の判定を数秒で実行でき、スクラップリサイクルや金属製造用途の合金比較も簡単です。

TERRA™ IIは、鉱物の定量分析を行えるポータブルX線回折装置です。 最大6時間のバッテリー寿命と丈夫で防水性に優れたケースを特長とするこの装置は、主要成分や微量成分をフィールドで迅速に分析できるように設計されています。