Flaw Detectors

Integral Angle Beam

Integral Angle Beam Transducer

Integral angle beam transducers provide superior signal-to-noise characteristics and contain durable plastic wear. Both Right Microdot and Straight Microdot connectors are available on some styles.

Integral Angle Beam Transducers

  • Durable plastic wear surface extends transducer life and avoids scratching of critical components
  • Small approach distance and overall transducer height provides an excellent choice for limited access applications
  • Superior signal-to-noise characteristics for such small integral transducers
  • Finger ring included with Micro-Miniature-RM case style transducers

A592S-SM

0.25", SM STYLE for Aluminum

A5952S-RM.tif A592S-RM

0.25", RM STYLE for Aluminum

Transducer Configurator

*A564S-RM, A574S-RM and A5053 create surface waves in steel and aluminum.


0.187", RM STYLE

A5023
0.187 Intergral
0.187", SM STYLE

A5014

0.25", RM STYLE for Steel

Frequency (MHZ)
Nominal Element Size (in)
Transducer Type
Frequency
(MHz)
Nominal Element Size ACCUSCAN-S
in.mmPart /
Item No.
2.25 0.25 x 0.25 6 x 6
A564S-RM

U8431044

Angle Beam Transducer, 2.25 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A561S-RM

U8431041

Angle Beam Transducer, 2.25 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A562S-RM

U8431042

Angle Beam Transducer, 2.25 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A563S-RM

U8431043

Angle Beam Transducer, 2.25 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
2.25 0.187 x 0.187 5 x 5
A5050

U8438010

Angle Beam Transducer, 45° Shear Wave in Steel, 2.25 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A5053

U8438011

Angle Beam Transducer, 90° Shear Wave in Steel, 2.25 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
5 0.25 x 0.25 6 x 6
A591S-RM  

U8431051

Angle Beam Transducer, 5 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate  
A592S-RM

U8431053

Angle Beam Transducer, 5 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate  
A593S-RM

U8431055

Angle Beam Transducer, 5 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A571S-RM

U8431045

Angle Beam Transducer, 5 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A572S-RM

U8431046

Angle Beam Transducer, 5 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, 60 Degree Shear in Steel, Right Microdot Connector, Includes Test Form Certificate
A573S-RM

U8431047

Angle Beam Transducer, 5 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A574S-RM

U8431048

Angle Beam Transducer, 5 MHz, 0.25" x 0.25" Element Diameter, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A591S-SM

U8431052

Angle Beam Transducer, 5 MHz, 0.25 in. x 0.25 in. element size, 45° sheer wave in Aluminum, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
A593S-SM

U8431056

Angle Beam Transducer, 5 MHz, 0.25 in. x 0.25 in. element size, 70° Sheer Wave in Aluminum, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
5 0.187 x 0.187 5 x 5
A5013

U8860363

Angle Beam Transducer, 70° Shear Wave in Steel, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
A5014

U8438001

Angle Beam Transducer, 60° Shear Wave in Steel, 5 MHz, 0.187 in. x 0.187 in. Element Diameter, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
A5015

U8438002

Angle Beam Transducer, 45° Shear Wave in Steel, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
A5020

U8438003

Angle Beam Transducer, 45° Shear Wave in Steel, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A5021

U8438004

Angle Beam Transducer, 70° Shear Wave in Steel, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A5023

U8438005

Angle Beam Transducer, 60° Shear Wave in Steel, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Right Microdot Connector Includes Test Form Certificate
A5067

U8438014

Angle Beam Transducer, 45° Shear Wave in Aluminum, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
A5068

U8438015

Angle Beam Transducer, 60° Shear Wave in Aluminum, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
A5069

U8438016

Angle Beam Transducer, 70° Shear Wave in Aluminum, 5 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
5 0.25 x 0.25 6 x 6 A592S-SM

U8431054

Angle Beam Transducer, 5 MHz, 0.25 in. x 0.25 in. element size, 60° Sheer Wave in Aluminum, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate
10 0.187 x 0.187 5 x 5 A5054

U8438012

Angle Beam Transducer, 70° Shear Wave in Steel, 10 MHz, 0.187 in. x 0.187 in. element size, Integral Case Style, Straight Microdot Connector Includes Test Form Certificate

Harisonic Style

Miniature potted angle beam transducers provide an excellent balance between size and performance by utilizing integral angle beam shear wave wedges. Overall size and footprint are reduced compared to a screw-in style transducer and wedge with little or no sacrifice in performance. Epoxy housings prevent test surface scratching caused by the transducer.
Connectors are available in either top (straight) or side (right angle) mount depending on application requirements. Four standard shear wave angles of 45°, 60°, 70°, and 90° or custom angles are available upon request.

The sub-miniature (HS-225) and ultra-miniature (HS-877) angle beam transducers are supplied in frequencies from 2.25 to 10.0 MHz with angles from 45° through 90°. Epoxy housings prevent the transducer from causing scratches to the test surface. These transducers are ideal for inspection of small diameter welded tubes and applications where the requirement is for a shear-wave transducer with a very small footprint. Depending on the type selected, either top or side mounted, Microdot connectors are available. When ordering, please specify part number, frequency, angle, material to be inspected, and connector location.

Transducer Housing Dimensions

Sub-Miniature:

0.375 in. L x 0.425 in. H x .0325 in. W
Ultra-Miniature:
0.375 in. L x 0.375 in. H x 0.250 in. W

Transducers Configurator

Frequency (MHZ)
Nominal Element Size (in)
Transducer Type
Search Results
Item NumberPart CodeFrequency
(MHz)
Nominal Element Size (mm)Nominal Element Size (in)Angle (°)Connector Type

U8503076

Miniature Integral Angle Beam Transducers, Standard Series, 2.25 MHz, 0.250 in. x 0.250 in.; 90° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0204-90-ST-RM
2.25 4 x 4 0.250 x 0.250 90° Shear Wave in Steel Right Microdot

U8503183

Miniature Integral Angle Beam Transducers, Standard Series, 2.25 MHz, 0.250 in. x 0.250 in.; 60° shear in Aluminum, Right Microdot Connector.
PAB-0204-60-AL-RM
2.25 6 x 6 0.250 x 0.250 60° Shear Wave in Steel Right Microdot

U8503051

Sub Miniature Integral Angle Beam Transducers, Standard Series, 2.25 MHz, 0.120 in. x 0.250 in.; 70° shear in Aluminum, Right Angle Microdot Connector.
HS-225-2-70-AL-RM
2.25 3 x 4 0.120 x 0.250 70° Shear Wave in Aluminum Right Microdot

U8503066

Ultra Miniature Integral Angle Beam Transducers, Standard Series,2.25 MHz, 0.187 in. x 0.187 in. (5 mm x 5mm) element size; 90° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
HS-877-2-90-ST-RM
2.25 5 x 5 0.187 x 0.187 90° Shear Wave in Steel Right Microdot

U8430041

Sub Miniature Integral Angle Beam Transducers, Standard Series, 2.25 MHz, 0.120 in. x 0.250 in.; 60° shear in Steel, Right Angle Microdot Connector.
HS-225-2-60-ST-RM
2.25 3 x 6 0.120 x 0.250 60° Shear Wave in Steel Right Microdot

U8430040

Sub Miniature Integral Angle Beam Transducers, Standard Series, 2.25 MHz, 0.120 in. x 0.250 in.; 70° shear in Steel, Right Angle Microdot Connector.
HS-225-2-70-ST-RM
2.25 3 x 6 0.120 x 0.250 70° Shear Wave in Steel Right Microdot

U8435043

Sub Miniature Integral Angle Beam Transducers, Standard Series, 2.25 MHz, 0.120 in. x 0.250 in.; 90° shear in Steel, Right Angle Microdot Connector.
HS-225-2-90-ST-RM
2.25 3 x 6 0.120 x 0.250 90° Shear Wave in Steel Right Microdot

U8503124

Sub Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.120 in. x 0.250 in.; 45° shear in Aluminum, Right Angle Microdot Connector Includes Test Form Certificate
HS-225-5-45-AL-RM
5 3 x 6 0.120 x 0.250 45° Shear Wave in Aluminum Right Microdot

U8503134

Sub Miniature, 5 MHz, 0.120 in. x 0.250 in. Includes Test Form Certificate
HS-225-5-45-AL-SM
5 3 x 6 0.120 x 0.250 45° Shear in Aluminum Straight Microdot

U8503053

Sub Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.120 in. x 0.250 in.; 60° shear in Aluminum, Right Angle Microdot Connector. Includes Test Form Certificate
HS-225-5-60-AL-RM
5 3 x 4 0.120 x 0.250 60° Shear Wave in Aluminum Right Microdot

U8503054

SubMiniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.120 in. x 0.250 in. (3 mm x 6 mm) element size; 60° shear in Aluminum, Straight Microdot Connector. Includes Test Form Certificate
HS-225-5-60-AL-SM
5 3 x 6 0.120 x 0.250 60° Shear Wave in Aluminum Straight Microdot

U8435041

Sub Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.120 in. x 0.250 in.; 60°, shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
HS-225-5-60-ST-RM
5 3 x 6 0.120 x 0.250 60° Shear Wave in Steel Right Microdot

U8503123

Sub Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.120 in. x 0.250 in.; 70° Shear in Aluminum, Right Microdot Connector, includes Test Form Certificate
HS-225-5-70-AL-RM
5 3 x 6 0.120 x 0.250 70° Shear Wave in Aluminum Right Microdot

U8503056

Sub Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.120 in. x 0.250 in. (3 mm x 6 mm) element size; 70° shear in Aluminum, Straight Microdot Connector. Includes Test Form Certificate
HS-225-5-70-AL-SM
5 3 x 6 0.120 x 0.250 70° Shear Wave in Aluminum Straight Microdot

U8435040

Sub Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.120 in. x 0.250 in.; 70°, shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
HS-225-5-70-ST-RM
5 3 x 6 0.120 x 0.250 70° Shear Wave in Steel Right Microdot

U8503077

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 45° shear in Aluminum, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0503-45-AL-RM
5 5 x 5 0.187 x 0.187 45° Shear Wave in Aluminum Right Microdot

U8503078

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 45° shear in Aluminum, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0503-45-AL-SM
5 5 x 5 0.187 x 0.187 45° Shear Wave in Aluminum Right Microdot

U8503079

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 45° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0503-45-ST-RM
5 5 x 5 0.187 x 0.187 45° Shear Wave in Steel Right Microdot

U8503080

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 45° shear in Steel, Straight Microdot Connector.
PAB-0503-45-ST-SM
5 5 x 5 0.187 x 0.187 45° Shear Wave in Steel Straight Microdot

U8503081

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 60° shear in Aluminum, Right Microdot Connector. Includes Test Form Certificate
PAB-0503-60-AL-RM
5 5 x 5 0.187 x 0.187 60° Shear Wave in Aluminum Right Microdot

U8503082

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 60° shear in Aluminum, Straight Connector. Includes Test Form Certificate
PAB-0503-60-AL-SM
5 5 x 5 0.187 x 0.187 60° Shear Wave in Aluminum Straight Microdot

U8503083

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 60° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0503-60-ST-RM
5 5 x 5 0.187 x 0.187 60° Shear Wave in Steel Right Microdot

U8503084

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 60° shear in Steel, Straight Microdot Connector.
PAB-0503-60-ST-SM
5 5 x 5 0.187 x 0.187 60° Shear Wave in Steel Straight Microdot

U8503085

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 70° shear in Aluminum, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0503-70-AL-RM
5 5 x 5 0.187 x 0.187 70° Shear Wave in Aluminum Right Microdot

U8503086

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 70° shear in Aluminum, Straight Microdot Connector. Includes Test Form Certificate
PAB-0503-70-AL-SM
5 5 x 5 0.187 x 0.187 70° Shear Wave in Aluminum Straight Microdot

U8503087

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 70° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0503-70-ST-RM
5 5 x 5 0.187 x 0.187 70° Shear Wave in Steel Right Microdot

U8503088

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 70° shear in Steel, Straight Microdot Connector.
PAB-0503-70-ST-SM
5 5 x 5 0.187 x 0.187 70° Shear Wave in Steel Straight Microdot

U8503167

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 90° shear in Straight, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0503-90-ST-RM
5 5 x 5 0.187 x 0.187 90° Shear Wave in Straight Right Microdot

U8503107

Angle Beam Transducer, 5.0 MHz, 0.250 in. x 0.250 in. (6 mmx 6 mm) element size, 45° Shear in Aluminum, Right Microdot Connector Includes Test Form Certificate
PAB-0504-45-AL-RM
5 6 x 6 0.250 x 0.250 45° Shear Wave in Aluminum Right Microdot

U8503106

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in. element size; 45° shear in Aluminum, Straight Microdot Connector
PAB-0504-45-AL-SM
5 6 x 6 0.250 x 0.250 45° Shear Wave in Aluminum Straight Microdot

U8430039

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 45 ° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0504-45-ST-RM
5 6 x 6 0.250 x 0.250 45° Shear Wave in Steel Right Microdot

U8503089

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 45° shear in Steel, Straight Microdot Connector. Includes Test Form Certificate
PAB-0504-45-ST-SM
5 6 x 6 0.250 x 0.250 45° Shear Wave in Steel Straight Microdot

U8503109

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 60° shear in Aluminum, Right Angle Microdot Connector
PAB-0504-60-AL-RM
5 6 x 6 0.250 x 0.250 60° Shear Wave in Aluminum Straight Microdot

U8503110

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 60° shear in Aluminum, Straight Microdot Connector
PAB-0504-60-AL-SM
5 6 x 6 0.250 x 0.250 60° Shear Wave in Aluminum Straight Microdot

U8503163

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 60° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0504-60-ST-RM
5 6 x 6 0.250 x 0.250 60° Shear Wave in Steel Right Microdot

U8503090

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 60° shear in Steel, Straight Microdot Connector. Includes Test Form Certificate
PAB-0504-60-ST-SM
5 6 x 6 0.250 x 0.250 60° Shear Wave in Steel Straight Microdot

U8503091

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 70° shear in Aluminum, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0504-70-AL-RM
5 6 x 6 0.250 x 0.250 70° Shear Wave in Aluminum Right Microdot

U8503092

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 70° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0504-70-ST-RM
5 6 x 6 0.250 x 0.250 70° Shear Wave in Steel Right Microdot

U8503093

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 70° shear in Steel, Straight Microdot Connector. Includes Test Form Certificate
PAB-0504-70-ST-SM
5 6 x 6 0.250 x 0.250 70° Shear Wave in Steel Straight Microdot

U8503094

Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.250 in. x 0.250 in.; 90° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-0504-90-ST-RM
5 6 x 6 0.250 x 0.250 90° Shear Wave in Steel Right Microdot

U8503067

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.187 in. x 0.187 in.; 45° shear in Aluminum, Straight Microdot Connector.
HS-877-5-45-AL-SM
5 5 x 5 0.187 x 0.187 45° Shear Wave in Aluminum Straight Microdot

U8503127

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 45° shear in Steel, Right Angle Microdot Connector Includes Test Form Certificate
HS-877-5-45-ST-RM
5 5 x 5 0.187 x 0.187 45° Shear Wave in Steel Right Microdot

U8503068

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 45° shear in Steel, Straight Microdot Connector.
HS-877-5-45-ST-SM
5 5 x 5 0.187 x 0.187 45° Shear Wave in Steel Straight Microdot

U8503070

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5 MHz, 0.187 in. x 0.187 in.; 60° shear in Aluminum, Straight Microdot Connector.
HS-877-5-60-AL-SM
5 5 x 5 0.187 x 0.187 60° Shear Wave in Aluminum Straight Microdot

U8503120

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in., 60° shear in Steel, Straight Microdot Connector.
HS-877-5-60-ST-SM
5 5 x 5 0.187 x 0.187 60° Shear Wave in Steel Straight Microdot

U8503122

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in.; 70° shear in Aluminum, Straight Microdot Connector.
HS-877-5-70-AL-SM
5 5 x 5 0.187 x 0.187 70° Shear Wave in Aluminum Straight Microdot Connecto

U8503073

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in. (5 mm x 5mm) element size; 90° shear in Steal, Right Angle Microdot Connector. Includes Test Form Certificate
HS-877-5-90-ST-RM
5 5 x 5 0.187 x 0.187 90° Shear Wave in Steel Right Microdot

U8503074

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 5.0 MHz, 0.187 in. x 0.187 in. (5 mm x 5mm) element size; 90° shear in Steal, Straight Microdot Connector. Includes Test Form Certificate
HS-877-5-90-ST-SM
5 5 x 5 0.187 x 0.187 90° Shear Wave in Steel Straight Microdot

U8503095

Miniature Integral Angle Beam Transducers, Standard Series, 10.0 MHz, 0.187 in. x 0.187 in.; 90° shear in Steel, Straight Microdot Connector. Includes Test Form Certificate
PAB-1003-90-ST-SM
10 5 x 5 0.187 x 0.187 90° Shear Wave in Steel Straight Microdot

U8502019

Angle Beam 10.0 MHz, 0.187 in. x 0.187 in. nomnial element size, 60° Shear in Aluminum, Straight Microdot Connector. Includes Test Form Certificate
PAB-1003-60-AL-SM
10 5 x 5 0.187 x 0.187 60° Shear Wave in Aluminum Straight Microdot

U8503096

Miniature Integral Angle Beam Transducers, Standard Series, 10.0 MHz, 0.250 in. x 0.250 in.; 45° shear in Aluminum, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-1004-45-AL-RM
10 6 x 6 0.250 x 0.250 45° Shear Wall in Aluminum Right Microdot

U8503176

Miniature Integral Angle Beam Transducers, Standard Series, 10.0 MHz, 0.250 in. x 0.250 in.; 45° shear in Aluminum, Straight Microdot Connector. Includes Test Form Certificate
PAB-1004-45-AL-SM
10 6 x 6 0.250 x 0.250 45° Shear Wave in Aluminum Straight Microdot

U8503177

Miniature Integral Angle Beam Transducers, Standard Series, 10.0 MHz, 0.250 in. x 0.250 in.; 45° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
PAB-1004-45-ST-RM
10 6 x 6 0.250 x 0.250 45° Shear Wave in Steel Right Microdot

U8502039

Miniature Integral Angle Beam Transducers, Standard Series, 10.0 MHz, 0.250 in. x 0.250 in.; 60° shear in Aluminum, Right Angle Microdot Connector Includes Test Form Certificate
PAB-1004-60-AL-RM
10 6 x 6 0.250 x 0.250 60° Shear Wave in Aluminum Right Microdot

U8503097

Miniature Integral Angle Beam Transducers, Standard Series, 10.0 MHz, 0.250 in. x 0.250 in.; 70° shear in Aluminum, Straight Microdot Connector. Includes Test Form Certificate
PAB-1004-70-AL-SM
10 6 x 6 0.250 x 0.250 70° Shear Wave in Aluminum Straight Microdot

U8503178

Miniature Integral Angle Beam Transducers, Standard Series, 10.0 MHz, 0.250 in. x 0.250 in.; 70° shear in Steel, Right Angle Microdot Connector.
PAB-1004-70-ST-RM
10 6 x 6 0.250 x 0.250 70° Shear Wave in Steel Right Microdot

U8503058

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 10 MHz, 0.187 in. x 0.187 in.; 45° shear in Aluminum, Straight Microdot Connector. Includes Test Form Certificate
HS-877-10-45-AL-SM
10 3 x 4 0.187 x 0.187 45° Shear Wave in Aluminum Straight Microdot

U8503104

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 10 MHz, 0.187 in. x 0.187 in.; 45° shear in Steel, Right Angle Microdot Connector.
HS-877-10-45-ST-RM
10 5 x 5 0.187 x 0.187 45° Shear Wave in Steel Right Microdot

U8435044

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 10 MHz, 0.187 in. x 0.187 in.; 45° shear in Steel, Straight Microdot Connector Includes Test Form Certificate
HS-877-10-45-ST-SM
10 5 x 5 0.187 x 0.187 45° Shear Wave in Steel Straight Microdot

U8503126

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 10 MHz, 0.187 in. x 0.187 in.; 60° shear in Aluminum, Straight Microdot Connector
HS-877-10-60-AL-SM
10 5 x 5 0.187 x 0.187 60° Shear Wave in Aluminum Straight Microdot

U8435045

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 10 MHz, 0.187 in x 0.187 in.; 60° shear in Steel, Straight Microdot Connector<br><br>
HS-877-10-60-ST-SM
10 5 x 5 0.187 x 0.187 10° Shear Wave in Steel Straight Microdot

U8503164

Ultra Miniature Integral Angle Beam Transducer, Standard Series, 10 MHz, 0.187 in. x 0.187 in., 70 ° Shear in Aluminum, Straight Microdot Connector, includes Test Form Certificate
HS-877-10-70-AL-SM
10 5 x 5 0.187 x 0.187 70° Shear Wave in Aluminum Straight Microdot

U8503062

Ultra Miniature Integral Angle Beam Transducers, Standard Series, 10 MHz, 0.187 in. x 0.187 in. (5 mm x 5mm) element size; 90° shear in Steel, Right Angle Microdot Connector. Includes Test Form Certificate
HS-877-10-90-ST-RM
10 5 x 5 0.187 x 0.187 90° Shear Wave in Steel Right Microdot

Loading...

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어

고급 NDT솔루션

Flaw Detectors

통합 검사 시스템

Search Results