AWS transducers and wedges conform to the specific requirements of the American Welding Society's Structural Welding Code for angle beam assemblies used in weld inspection.
|
Nominal
Element Size | Freq. |
Transducer
Part Num* |
Snail Wedge
Part Num* |
Accupath Wedge
Part Num* | |
| inches | MHz | ACCUSCAN | CENTRASCAN | ||
| 0.625 x 0.625 | 2.25 | A430S-SB | C430-SB | ABWS-8 -X° | ABWS-6-X° |
| 0.625 x 0.75 | 2.25 | A431S-SB | C431-SB | ABWS-8 -X° | ABWS-6-X° |
| 0.75 x 0.75 | 2.25 | A432S-SB | C432-SB | ABWS-8 -X° | ABWS-6-X° |
* Wedges are available in standard refracted shear wave angles of 45°, 60° and 70° in steel. Please specify upon ordering.

|
Snail Wedge Dimensions*
(in inches) | ||||
(A) | (B) | (C) | (D) | |
| 45° | 2.15 | 0.62 | 1.78 | 1.25 |
| 60° | 1.91 | 0.65 | 1.81 | 1.25 |
| 70° | 2.17 | 0.67 | 1.92 | 1.25 |
*Distance between screws (center to center) is 1.00".

|
Accupath Wedge Dimensions*
(in inches) | ||||
(A) | (B) | (C) | (D) | |
| 45° | 1.50 | 0.90 | 1.96 | 1.50 |
| 60° | 1.68 | 0.79 | 2.05 | 1.50 |
| 70° | 1.66 | 0.96 | 2.20 | 1.50 |
*Distance between screws (center to center) is 1.062".