Defektoskopy

Near-wall Probes

Near-Wall Probes

Near-wall probes offer a shortened dead zone at both ends of the probe (1.5 mm between center of first or last element and housing edge). They are well suited for composite channel inspections and are used for C-scan inspections of composites (delamination, disbonding, and porosity).

Advantages

  • Shortened dead zone at both ends (1.5 mm between center of first or last element and housing edge)
  • Well suited for composite channel inspections
  • Used for C-scan inspections of composites (delamination, disbonding, and porosity)

Probe Specifications and Dimensions

Part Number Item Number Frequency
(MHz)
Number of Elements Pitch
(mm)
Active Aperture
(mm)
Elevation
(mm)
External Dimensions mm (in.)
L W H
3.5L64-NW1 U8330148 3.5 64 1.0 64.0 7.0 66 (2.60) 19 (0.75) 25 (0.98)
5L64-NW1 U8330134 5.0 64 1.0 64.0 7.0 66 (2.60) 19 (0.75) 25 (0.98)
3.5L24-NW2 U8330965 3.5 24 1.0 24.0 7.0 26 (1.02) 19 (0.75) 30 (1.18)
5L24-NW2 U8330155 5.0 24 1.0 24.0 7.0 26 (1.02) 19 (0.75) 30 (1.18)
3.5L128-NW3 U8330695 3.5 128 1.0 128.0 7.0 130 (5.12) 21 (0.83) 35 (1.38)
5L128-NW3 U8330647 5.0 128 1.0 128.0 7.0 130 (5.12) 21 (0.83) 35 (1.38)
These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths.
Loading...

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어

Zaawansowane rozwiązania NDT

Defektoskopy

Zintegrowane systemy badań