Immersion probes are designed to be used with a water wedge or in an immersion tank when the test part is partially or wholly immersed. They are longitudinal wave probes that can be set up for refracted shear-wave inspections using a Rexolite wedge.

Advantages

  • Acoustic impedance matches water
  • Design allows fitting on water wedges for easier coupling on many surfaces and an adjustable water path (when the part to be inspected cannot be immersed in a tank).
  • Linear scanning allows coverage of 30 mm to 90 mm in one line, with very high accuracy.
  • Corrosion-resistant stainless steel case
  • Waterproof guaranteed up to 1 m (3.28 ft) under water

Typical Applications

  • Inspection of thin plate or tubing (steel, aluminum, or other)
  • Composite inspection for delamination, disbonding, etc.
  • Inline thickness gaging
  • Automated scanning

Probe Specifications and Dimensions

Part Number Item Number Frequency
(MHz)
Number of Elements Pitch
(mm)
Active Aperture
(mm)
Elevation
(mm)
External Dimensions
mm (in.)
L W H
5L64-I1 U8330323 5.0 64 0.60 38.4 10.0 50 (1.97) 19 (0.75) 25 (0.98)
10L64-I1 U8330012 10.0 64 0.50 32.0 7.0 50 (1.97) 19 (0.75) 25 (0.98)
5L128-I2 U8330031 5.0 128 0.60 76.8 10.0 83 (3.27) 21 (0.83) 35 (1.38)
10L128-I2 U8330004 10.0 128 0.50 64.0 7.0 83 (3.27) 21 (0.83) 35 (1.38)
2.25L128-I3 U8330351 2.25 128 0.75 96.0 12.0 102 (4.02) 21 (0.83) 35 (1.38)
5L128-I3 U8330379 5.0 128 0.75 96.0 10.0 102 (4.02) 21 (0.83) 35 (1.38)
7.5L60-I4 U8330955 7.5 64 1.0 64.0 7.0 73 (2.87) 24 (0.94) 25 (0.98)