Defektoskopy

Curved Array Probes

Curved array probes are made with a corrosion-resistant stainless steel case and are guaranteed waterproof up to 1 m underwater. The acoustic impedance of these probes matches water. They are compatible with adjustable immersion wedges and are used for the inspection of carbon fiber reinforced polymers (CFRP) corners and in addition to the inspection of composite for delamination.

Advantages

  • Acoustic impedance matches water.
  • High circumferential resolution around the radius
  • Corrosion-resistant stainless steel case
  • Waterproof guaranteed up to 1 m (3.28 ft) underwater
  • Compatible with adjustable immersion wedges

Typical Applications

  • Inspection of carbon fiber reinforced polymers (CFRP) corners
  • Composite inspection for delamination

Probe Specifications and Dimensions

Part Number Item Number Casing Type Frequency (MHz) Number of Element Pitch (mm) Elevation (mm) Radius (mm) (R) Angle (°) (A) Inspection Type
3.5CC10.2-16-R1 U8330453 R1 3.5 16 1.0 5.0 10.2 90 ID
5CC10.2-16-R1 U8330709 R1 5.0 16 1.0 5.0 10.2 90 ID
3.5CC25-32-R4 U8330629 R4 3.5 32 1.32 6.0 25.0 90 ID, OD
5CC25-32-R4 U8330479 R4 5.0 32 1.32 6.0 25.0 90 ID, OD
3.5CC50-64-R5 U8330630 R5 3.5 64 1.65 6.0 50.0 121 OD
5CC50-64-R5 U8330636 R5 5.0 64 1.65 6.0 50.0 121 OD
These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths.
Loading...

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어

Zaawansowane rozwiązania NDT

Defektoskopy

Zintegrowane systemy badań