近壁探头的两端具有较短的盲区(第一晶片的中心和最后晶片的中心到与它们最近的探头外壳边缘的距离是1.5毫米)。 它们可以极好地适用于复合材料的通道检测,并用于复合材料的C扫描检测(分层、脱胶和多孔性)。
| Part Number | Item Number |
Frequency
(MHz) | Number of Elements |
Pitch
(mm) |
Active Aperture
(mm) |
Elevation
(mm) | External Dimensions mm (in.) | ||
| L | W | H | |||||||
| 3.5L64-NW1 | U8330148 | 3.5 | 64 | 1.0 | 64.0 | 7.0 | 66 (2.60) | 19 (0.75) | 25 (0.98) |
| 5L64-NW1 | U8330134 | 5.0 | 64 | 1.0 | 64.0 | 7.0 | 66 (2.60) | 19 (0.75) | 25 (0.98) |
| 3.5L24-NW2 | U8330965 | 3.5 | 24 | 1.0 | 24.0 | 7.0 | 26 (1.02) | 19 (0.75) | 30 (1.18) |
| 5L24-NW2 | U8330155 | 5.0 | 24 | 1.0 | 24.0 | 7.0 | 26 (1.02) | 19 (0.75) | 30 (1.18) |
| 3.5L128-NW3 | U8330695 | 3.5 | 128 | 1.0 | 128.0 | 7.0 | 130 (5.12) | 21 (0.83) | 35 (1.38) |
| 5L128-NW3 | U8330647 | 5.0 | 128 | 1.0 | 128.0 | 7.0 | 130 (5.12) | 21 (0.83) | 35 (1.38) |
| These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths. | |||||||||