Overview

Olympus manufactures custom immersion flat with radius (IFWR) phased array probes to increase coverage, improve detectability, and simplify data analysis. Mistras Group Inc. has increased productivity by using a single custom Olympus 3.5MHz 64 element IFWR probe; replacing two probes in their composite inspection setup. Mistras Group Inc. provided the following details and graphics outlining their success.

Old Technique

Mistras previously used 1 linear 64 element, 1 concave 32 element probe, and the OmniScan MX to inspect 8 zones across a composite part. The inspection with two probes took approximately 2.5 hours.

Figure 1: 8 zones to cover the entire composite piece
Figure 1: 8 zones to cover the entire composite piece

Firgure 2: Two setups required to cover the entire partFirgure 2: Two setups required to cover the entire part


Firgure 2: Two setups required to cover the entire part

The C-scan data recored from multiple probes and passes becomes more difficult to record and analyze. Each scan must be properly identified to ensure acurrate analysis.

Figure 3: C-scan data is recored for each zone
Figure 3: C-scan data is recored for each zone

New Technique

Using the Olympus custom IFWR probe, inspection of all 8 zones can be completed with one probe in two passes; reducinig inspection time by approximately 50%.

Figure 4: Custom Immersion Flat With Radius (IFWR) probe setup
Figure 4: Custom Immersion Flat With Radius (IFWR) probe setup

Reducing quantity of probes while increasing coverage has proven to simplify recording and analyzing data. Each part now has only two C-scan’s to analyze.

Figure 5: Data captured from one pass covers 4 zones
Figure 5: Data captured from one pass covers 4 zones

Conclusion

Olympus has worked with Mistras Group Inc. to provide a custom probe which has proven to reduce inspection time, improve detectability, and simplify data analysis. Olympus has the capability to manufacture IFWR probes to customer specifications and specific part requirements.

To inquire for custom probe possibilities specific to your application please contact SCE.PM@olympusndt.com or submit details via our online custom probe form.

Olympus IMS

Productos para la aplicación

Cada detector de defectos de la serie OmniScan™ X3 es una completa caja de herramientas por ultrasonido multielemento (Phased Array). Las innovadoras y avanzadas técnicas TFM y PA permiten identificar defectos con confianza, mientras que las potentes herramientas de software y los sencillos flujos de trabajo mejoran su productividad.

Este equipo ligero de un solo canal proporciona una pantalla táctil fácil de leer de 8,4" (21,3 cm) y soluciones bastante rentables en el plano precio-rendimiento. Viene en dos modelos: SX PA y SX UT. El modelo SX PA es una unidad 16:64PR que, al igual que el modelo SX UT [con un solo canal UT], también está equipado con una canal UT para inspecciones de pulso-eco (pulse-echo), emisión-recepción (pitch-catch) y TOFD.
Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.