Appareil de recherche de défauts

Sondes et blocs étalons de conductivité

Conductivity

Les sondes de conductivité sont conçues pour le tri des métaux non-ferreux, ainsi que pour identifier l'état des matériaux après traitement thermique ou les dommages.

Olympus conductivity probes with PowerLink technology are designed to be used with Nortec 500 series instruments*. They are designed for sorting metals and alloys, determining heat-treatment condition or finding damaged areas. The Nortec 500 series instruments allow measurement of conductivity displayed in a digital readout in either %IACS or MS/m while at the same time measuring a coating or liftoff factor in inches or millimeters.

Conductivity probes are available in frequencies of 60 kHz or 480 kHz and are supplied with a 16-pin LEMO connector for PowerLink.

Olympus utilizes a system for measuring and certifying electrical conductivity of metals which operates using the four point DC resistance technique for primary standards. These standards are maintained by Olympus at all times and are re-certified at set intervals to comply with NIST traceability. The primary standards and test pieces are maintained in a 20◦ C (+/-10◦ C) environment and the test pieces are measured using the AC impedance transfer method. The entire system is computer controlled for accuracy and repeatability.

Utilizing this technique of primary standards, Olympus is capable of certifying conductivity standards to high degrees of accuracy. Materials that are below 60% IACS can be certified to 0.35% IACS or better and materials that are above 60% IACS can be certified to 0.5% IACS or better.

*Not compatible with base model Nortec 500 - requires Nortec 500C, 500S, or 500D model for operation.
*Also compatible with Nortec 2000 series.

Conductivity Probes

Dimensions
mm (in.)
Part NumberItem NumberTypeFrequency
kHz
HeightLengthWidthConnector
9222340 U8690027 Right Angle 60 19.1 (0.75) 25.4 (1.00) n.a. 16-pin LEMO
9222341 U8690028 Right Angle 480 19.1 (0.75) 25.4 (1.00) n.a. 16-pin LEMO
9222360 U8690029 Straight 60 7.9 (0.31) 69.9 (2.75) n.a. 16-pin LEMO
9222361 U8690030 Straight 480 7.9 (0.31) 69.9 (2.75) n.a. 16-pin LEMO

Conductivity Standards

Part NumberItem NumberIACS% Value #1
(tolerance)
IACS% Value #2
(tolerance)
IACS% Value #3
(tolerance)
IACS% Value #4
(tolerance)
IACS% Value #5
(tolerance)
CREF2-04100 U8861784 4.6 (±0.4) 100.0 (±10) n.a. n.a. n.a.
CREF2-1742 U8861881 17.2 (±1.5) 42.7 (±4.4) n.a. n.a. n.a.
CREF2-2932 U8861830 29.3 (±3) 32.0 (±3.3) n.a. n.a. n.a.
CREF3-0129100 U8861910 1.5 (±0.1) 29.3 (±3) 100.0 (±10) n.a. n.a.
CREF3-172942 U8861675 17.2 (±1.5) 29.3 (±3) 42.7 (±4.4) n.a. n.a.
CREF3-172959 U8861822 17.2 (±1.5) 29.3 (±3) 59.9 (±6) n.a. n.a.
CREF3-294259 U8861924 29.3 (±3) 42.7 (±4.4) 59.9 (±6) n.a. n.a.
CREF4-17294259 U8861629 17.2 (±1.5) 29.3 (±3) 42.7 (±4.4) 59.9 (±6) n.a.
CREF4-173259100 U8861982 17.2 (±1.5) 32.0 (±3.3) 59.9 (±6) 100.0 (±10) n.a.
CREF5-01293242100 U8861902 1.5 (±0.1) 29.3 (±3) 32.0 (±3.3) 42.7 (±4.4) 100.0 (±10)
CREF5-04174559100 U8861929 4.6 (±0.4) 17.2 (±1.5) 45.7 (±4) 59.9 (±6) 100.0 (±10)
Loading...

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어