Thickness Measurements on Rubber Hoses & Tubing

Thickness measurements on rubber tubes or hoses are important for quality control reasons. With no need for cutting up the part, ultrasonic thickness gauges are capable of providing instant thickness measurements by coupling an ultrasonic transducer to one side of the part.

Minimum diameter of the tube is usually limited to 0.080 in. (2.0 mm), although thin walled rubber tubing can be flattened to aid in making thickness measurements. In some rubber hoses, reinforcing materials such as fibers or steel wires make total wall thickness measurements more difficult or even impossible, especially in the case of woven fabric reinforcement.

Equipment: The recommendation for instrument and transducer selection depends on many variables of which hose diameter, thickness range and type of rubber are the most important. Typically, a rubber hose with a minimum diameter of 0.080 in. (2.0 mm) or a maximum thickness of 0.125 in. (3 mm) can be gauged with a Model 35DL or Model 35 and a 10 MHz or 20MHz contact transducer to a calibrated accuracy of ±0.002 in. (±0.05 mm), or better.

For thickness measurements on rubber tubing with walls thicker than 0.125 in. (3 mm) it may be necessary to use the Models 35DL-HP or 35HP and an M106 contact transducer. It is recommended that Panametrics be consulted for final selection of instrumentation.

Products used for this application

35

袖珍型35是一款手持式超声测厚仪。这款仪器使用单晶探头可对金属、塑料、橡胶、玻璃及复合材料进行精确的测量。具有宽泛的厚度范围:0.08毫米~635.0毫米(0.0030英寸~25.0英寸)。 具有可选的实时波形和调整模式功能。

35DL

袖珍型35DL是一款手持式超声测厚仪。这款仪器使用单晶探头可对金属、塑料、橡胶、玻璃及复合材料进行精确的测量。具有与35型仪器相同的功能,并带有内置数据记录器。

35DL-HP

袖珍型35DL-HP(高穿透)是一款手持式超声测厚仪,用于对纤维玻璃、铸铁和橡胶等较厚或声束衰减性较强的材料进行测量。使用单晶探头。具有与35型仪器相同的功能,并带有内置数据记录器。

35HP

袖珍型35HP(高穿透)是一款手持式超声测厚仪,用于对纤维玻璃、铸铁和橡胶等较厚或声束衰减性较强的材料进行测量。使用单晶探头。具有与35DL-HP型仪器相同的功能,不带内置数据记录器。

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어