Handheld XRF for FAC Corrosion Prediction by Cr in Carbon Steel


The DELTA Takes Detection Limits of Chromium (Cr) in Carbon Steel to an All Time Low!

It has been shown that small amounts of Cr in carbon steel pipes significantly reduce the rate of flow accelerated corrosion. Consequently, highly accurate measurements of low levels of Cr in carbon steel are critical for predicting the end of life in these pipes. In general, Cr is present in carbon steels as a residual tramp element ranging from 0 to 0.25%. The critical level of Cr monitored for FAC prediction is at about 0.04% (400ppm). The DELTA Premium, the latest development in HHXRF, goes to an all time high in accuracy and an all time low in detection limits for Cr and other metals. It detects trace levels of Cr as low as 0.004% (40ppm) in alloys; and 0.01% (100ppm) in carbon steel for FAC inspections. Although HHXRF is a non-destructive technique, accurate low Cr analysis of in-service and oxidized pipes can require some sample preparation to remove surface material before measurements. Portable angle grinders with alumina grinder disks are recommended.

power plant smoke stack

Comparison of DELTA Premium Handheld XRF with Certified Assays of Trace Cr in Carbon Steel

Standard Certified %Cr HHXRF Measured %Cr HHXRF %Cr +/-
IARM 229A 0.015 0.015 0.002
IARM 28E 0.079 0.080 0.005
IARM 33D 0.139 0.139 0.006
IARM 35F 1.160 1.210 0.006

DELTA Premium Analysis Time: 120sec Beam 1; 30 sec Beam 2

corrosion car steel DELTA accuracy chart

Delta Handheld XRF Analyzer in hip holster

Excellent Accuracy and Low Levels of Detection are Critical for Predicting Accelerated Corrosion

In addition to testing for flow accelerated corrosion, the power supply industry depends on HHXRF analyzers for startups, shutdowns, general maintenance, and trouble shooting. Managers cannot afford to depend on out-of-date and unreliable equipment, or untimely support of equipment. They also cannot afford to fall behind the technology curve. The analytical capabilities of HHXRF continue expanding, and new features continually enable operators to be more effective and efficient. Upgrade your HHXRF to the DELTA - the latest HHXRF loaded with innovative features and backed by the industry's best service and support.

Handheld XRF for Metals & Alloys Industries

Iron & Steel Non-ferrous Scrap & Secondary

Iron and steel are the most widely used of metals and alloys. Lighter metals, non-ferrous, newly developed and exotic alloys are also utilized extensively, but iron and steel are considered the basic raw materials for the majority of industrial goods and construction. Although produced from ores mined around the globe, steel is one of the most recycled materials in the world. From base form to recycled materials to finished products, metals and alloys are integral to the fabric of society, the consumption of which is often considered a primary indicator of development and economic progress.

Metals Alloys is a serious, dynamic business.

The DELTA XRF analyzer is an essential tool for all businesses involved in the trade or use of metals alloys. In seconds, you can nondestructively measure 25+ elements. Turnings, shavings, rods, wires, small parts, components, sizeable materials and large structures can all be analyzed directly, non-destructively. How you get them, how you make them, how you use them, how you sell them is how you measure them. Whether you check purity, chemistry, or grade ID for highest value, maximum recovery, quality, conformance, or maintenance and safety, our DELTA XRF analyzer will give you immediate answers to take action on now.

Delta Handheld XRF testing for alloys
Olympus IMS
应用所使用的产品

DELTA合金与金属手持式X射线荧光分析仪可以进行专业性极强的材料化学分析,可快速精确地辨别合金级别和纯金属。这款分析仪在数秒钟之内就可做出合金化学成分的辨别及定级。从简单的分拣到复杂的级别划分,从来料检测到最后产品的核查,都可用到这款分析仪。
DELTA Element是一款性价比极高的手持式X射线荧光(XRF)分析仪,这是一款经过优化的分析仪,可以进行废料金属的分拣、材料成份的辨别(PMI)、合金的质量保证和质量控制,以及贵金属的分析。
DELTA Professional将硅漂移探测器(SDD)和一个4W优化X射线管结合在一起使用,可在检测速度、检出限及可检元素的范围方面提供极为优质的性能。它可以分析合金和矿石中镁(Mg)及原子数更高的元素。DELTA Professional是Olympus所生产的最具问题解决价值的手持式XRF分析仪。
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK