Automated QC / PMI Analyzer - For Fast, 100% Testing of Tubes


Tube and pipe manufacturers use many different metals and alloys in their production lines. To eliminate liabilities, avoid material mix-ups and to meet their customers' requirements, they must compare their product against acceptable alloy specifications.

Particularly in the aerospace, petrochemical and nuclear industries, the consequences of processing or fabricating with the wrong alloy material can be catastrophic, resulting in product failure, personal injuries, fatalities, liability claims and eventual loss of business. To protect their business, high volume manufacturers need a fast, non-destructive method that checks each piece prior to shipping. The FOX-IQ Tube & Rod system offers these capabilities in an easy to integrate, easy to use, and reliable solution.

FOX-IQ System

The FOX-IQ is a compact system that integrates easily with existing or new PLC-controlled processes. This robust system is engineered for 24/7 operation in industrial environments - it can endure high levels of vibration, electromagnetic and acoustical noise as well as dust and moisture.

Each FOX-IQ delivers fast, pass/fail tests, accurate grade ID, and chemistry with automated links to the QC/QA reporting system. The FOX-IQ is controlled by a PC for start/stop, data acquisition, decision making and communication to external devices. The FOX-IQ is driven by powerful and intuitive software that has been developed and custom designed specifically for the tube and pipe industry in cooperation with several market leaders. Features include multi-level access, automated retesting, extensive reporting and an intuitive touch screen interface.

FOX IQ System

FOX-IQ Advantages

  • Fast accurate analysis in matter of seconds
  • Remote controlled - no site operation intervention required
  • Integrated automatic analyzer QC and performance verification
  • Compact, robust design fits into most existing operations with minimal infrastructure changes
  • Flexible; simple intuitive control allows for minimal user intervention and makes it easy to add new alloys
  • Minimal downtime - pre-calibrated Probe Head Assemblies can be exchanged in minutes
  • Low power requirements: needs only 110/220V
  • Uses an X-ray tube, eliminating the regulatory headaches of a radioactive source
Basic Specifications and System Description
Source X-ray tube; no radioactive isotopes
Detector Silicon drift detector; <165 eV resolution at 5.95keV Mn K-alpha line
PC Windows XP or Windows 7 operating system
Housing Anodized aluminum. Sealed to moisture & dust. Shielded from EMI emissions
Weight
Probe Head Assembly: 1.8 kg (4 lb)
Electrical Interface: 8 kg (18 lb)
DimensionsMeasurement Head (L × W × H): 30.5cm × 10cm × 10.5cm (12in. × 4in. × 4.125i.)
Electrical Interface (L × W × H): 40.6 cm × 15.88 cm × 50.8 cm (16 in. x 6.25 in. x 20 in.)
Cable LengthProbe Head Assembly - Electrical Interface: up to 30 m (100 ft)
Standard lengths: 15 m
Electrical interface - PC: dependent on customer requirements
Tube Voltage 10 kV - 40 kV
Current 80 µA maximum, 10 µA typical
Tube Filtering Up to five (5) filter positions for optimal analysis on 25+ Elements
Shutter Automatic shutter for safety and internal standardization
Power AC 110-250 V, 50/60 Hz
I/O The user interface runs on a PC equipped with the Olympus PC software that controls the FOX-IQ; this software analyzes sample spectra, manages results, and interfaces with external devices through RS-485 or TCP/IP. There are dry contacts on all outputs and 24V start/stop and interlock signals.
Data Logging Up to 12 fields of information per sample including Job #, Work Order, Part #, etc. Auto tracks alarms, pass/fails, and elemental results within a work order or run. Stores >100,000 tests, including results, sample ID, and spectral data, in a binary, tamper-proof format that meets 21CFR Part 11. The electrical interface supports an external sample trigger input and provides a pass/fail indicator signal that can be used to trigger other line equipment to accept or reject a sample based on the analysis results.
Olympus IMS
应用所使用的产品

FOX-IQ处理和在线XRF系统用于对钙和铀元素进行自动、持续的在线XRF测量。这个系统用于24/7操作工业环境,可优化操作过程、提高生产效率和质量。用于金属、合金材料、液体和其它流体。 安装简便、拥有成本较低。
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK