| Frequency (MHz) | Nominal Element Size | VIDEOSCAN | ||||||
|---|---|---|---|---|---|---|---|---|
| in. | mm | Part / Item No. | ||||||
| 1 | 1 | 25 | V1548 | |||||
| 25 | 1 | 25 | V150-RB V150-RM | |||||
| 5 | 1 | 25 | V151-RB V151-RM | |||||
| 1 | 0.5 | 13 | V153-RM V153-RB U8403064
| |||||
| 1 | 1 | 25 | V152-RB V152-RM U8403062
| |||||
| 225 | 0.5 | 13 | V154-RM V154-RB U8403068
| |||||
| 5 | 0.125 | 3 | V157-RM | |||||
| 5 | 0.25 | 6 | V156-RMU8403074
| |||||
| 5 | 0.5 | 13 | V155-RM U8403072
V155-RB U8403071
| |||||
Delay Line Series
|
|
Frequency |
Nominal
| Delay |
Transducer
| |
MHz | inches | mm | µsec | |
5.0 | 0.25 | 6 | 7 | V220-BA-RM |
10 | 0.25 | 6 | 7 | V221-BA-RM |
0.25 | 6 | 7 | V222-BA-RM | |
| 20 | 0.25 | 6 | 7 | V222-BB-RM |
| 0.25 | 6 | 4 | v222-BC-RM | |
SWC |
4 oz.
| Normal Incidence Shear Wave, non-toxic, water soluble organic substance of very high viscosity |