Inspection & Measurement Systems

Detectores de Defeitos

Ângulo de Feixe Padrão

Standard Angle Beam Transducers

Standard angle beam transducers are large single element transducers used with a wedge to introduce a refracted shear wave or longitudinal wave into a test piece.

Advantages

  • Large element size allows for inspection of thicker components and provides a large scanning index
  • Transducers available in Accuscan-S, Centrascan, and Videoscan Series
  • Accupath and High Temperature style wedges available
  • Threaded brass screw receptacles ensure firm anchoring of the transducer onto the wedge
  • Available in frequencies as low as 0.5 MHz and 1.0 MHz
  • Captive screws included with the transducer

Standard Angle Beam Transducers

Transducer Dimensions (in inches)

Nominal
Element Size
(A) (B) (C) (D)
1.00 1.25 0.63 1.38 1.65
0.50 x 1.00 0.73 0.63 1.31 1.53
0.50 0.72 0.63 0.81 1.02


Transducer Configurator

Frequency (MHZ)
Nominal Element Size (mm)
Transducer Type
Frequency
(MHz)
Nominal Element Size ACCUSCAN-S CENTRASCAN VIDEOSCAN
in.mmPart /
Item No.
Part /
Item No.
Part /
Item No.
5 0.50 x 1.00 13 x 25 A413S-SB

U8431012

Angle Beam Transducer, 0.5 MHz, 0.50 in. x 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
 V413-SB

U8436010

Angle Beam Transducer, 0.5 MHz, 0.50 in. x 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
5 1 25 A414S-SB

U8431013

Angle Beam Transducer, 0.5 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
 V414-SB

U8436011

Angle Beam Transducer, 0.5 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
1 0.50 x 1.00 13 x 25 A401S-SB

U8431001

Angle Beam Transducer, 1 MHz, 0.50 in. x 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C401-SB

U8435001

Centrascan Composite Angle Beam Transducer, 1.00 MHz, 0.50 in. x 1.00 in.element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V401-SB

U8436001

Angle Beam Transducer, 1 MHz, 0.50 in. x 1.00 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
1 0.5 13 A402S-SB

U8431002

Angle Beam Transducer, 1 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C402-SB

U8435002

Centrascan Composite Angle Beam Transducer, 1.00 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V402-SB

U8436002

Angle Beam Transducer, 1 MHz, 0.50 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
1 1 25 A407S-SB

U8431007

Angle Beam Transducer, 1 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C407-SB

U8435007

Centrascan Composite Angle Beam Transducer, 1.00 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V407-SB

U8436007

Angle Beam Transducer, 1 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
225 0.50 x 1.00 13 x 25 A403S-SB

U8431003

Angle Beam Transducer, 2.25 MHz, 0.50 in. x 1.00 in. Element Size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C403-SB

U8435003

Centrascan Composite Angle Beam Transducer, 2.25 MHz, 0.50 in. X 1.00 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V403-SB

U8436003

Angle Beam Transducer, 2.25 MHz, 0.50 in. x 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
225 0.5 13 A404S-SB

U8431004

Angle Beam Transducer, 2.25 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C404-SB

U8435004

Centrascan Composite Angle Beam Transducer, 2.25 MHz, 0.50 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V404-SB

U8436004

Angle Beam Transducer, 2.25 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
225 1 25 A408S-SB

U8431008

Angle Beam Transducer, 2.25 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C408-SB

U8435008

Centrascan Composite Angle Beam Transducer, 2.25 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V408-SB

U8436008

Angle Beam Transducer, 2.25 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
35 0.50 x 1.00 13 x 25 A412S-SB

U8431011

Angle Beam Transducer, 3.5 MHz, 0.50 in. x 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C412-SB

U8435011

Centrascan Composite Angle Beam Transducer, 3.50 MHz, 0.50 in. X 1.00 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
 
35 0.5 13 A415S-SB

U8431014

Angle Beam Transducer, 3.5 MHz, 0.50 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C415-SB

U8435012

Centrascan Composite Angle Beam Transducer, 3.50 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
 
35 1 25 A411S-SB

U8431010

Angle Beam Transducer, 3.5 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C411-SB

U8435010

Centrascan Composite Angle Beam Transducer, 3.50 MHz, 1.00 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
 
5 0.50 x 1.00 13 x 25
A405S-SB

U8431005

Angle Beam Transducer, 5 MHz, 0.50 in. x 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
A406S-SB

U8431006

Angle Beam Transducer, 5 MHz, 0.50 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C405-SB

U8435005

Centrascan Composite Angle Beam Transducer, 5.00 MHz, 0.50 in. X 1.00 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V405-SB

U8436005

Angle Beam Transducer, 5 MHz, 0.50 in. x 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
5 0.5 13  C406-SB

U8435006

Centrascan Composite Angle Beam Transducer, 5.00 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V406-SB

U8436006

Angle Beam Transducer, 5 MHz, 0.50 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
5 1 25 A409S-SB

U8431009

Angle Beam Transducer, 5 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
C409-SB

U8435009

Centrascan Composite Angle Beam Transducer, 5.00 MHz, 1.00 in. Element Diameter, Standard Case Style, Straight BNC Connector Includes Test Form Certificate
V409-SB

U8436009

Angle Beam Transducer, 5 MHz, 1.00 in. element size, Standard Case Style, Straight BNC Connector Includes Test Form Certificate

Standard Angle Beam Wedges

Nominal
Element Size
Wedge Part Numbers
inches mm Accupath* High Temp*
500°F (260°C)
Very High Temp*
900°F (480°C)
Surface Wave 90°
1.00 25 ABWS-3-X° ABWHT-3-X° ABWVHT-3-X° ABWSL-3-90°
0.50 x 1.00 13 x 25 ABWS-2-X° ABWHT-2-X° ABWVHT-2-X° ABWSL-2-90°
0.50 13 ABWS-1-X° ABWHT-1-X° ABWVHT-1-X° ABWSL-1-90°

*Wedges are available in standard refracted shear wave angles of 30°, 45°, 60°, and 70° in steel at 5.0 MHz.

Accupath and Surface Wave Wedge Dimensions (Standard)

Nominal Element Size (in inches)
1.00 0.50 x 1.00 0.50
(A) (B) (C) (D) (A) (B) (C) (D) (A) (B) (C) (D)
30° 1.69 2.15 1.62 1.15 1.30 1.30 1.60 0.76 1.20 1.42 1.10 0.83
45° 1.47 1.96 1.63 0.97 1.30 1.41 1.60 0.78 1.20 1.31 1.08 0.70
60° 1.50 2.18 1.63 1.00 1.30 1.50 1.60 0.67 1.20 1.48 1.08 0.68
70° 1.50 2.47 1.63 1.13 1.35 1.77 1.60 0.85 1.20 1.58 1.09 0.68
90° 1.50 2.50 1.65 0.44 1.20 1.34 1.60 - 1.20 1.34 1.00 -

Shear Wave Wedges for Aluminum

Compatible with our Miniature Screw-In and Standard Angle Beam transducers

Transducer
Case
Nominal
Element Size
Wedge Part Numbers
inches mm 30° 45° 60° 70° 90°
Screw-In 0.50 13 ABWM-5053T ABWM-5027T ABWM-5028T ABWM-5029T ABWML-5041T
0.375 10 ABWM-7024T ABWM-7025T ABWM-7026T ABWM-7027T ABWML-7028T
0.25 6 ABWM-4086T ABWM-4087T ABWM-4088T ABWM-4089T ABWML-4074T
Standard 1.00 25 ABWS-3028 ABWS-3016 ABWS-3029 ABWS-3030 ABWSL-3039
0.50
x
1.00
13
x
25
ABWS-2021 ABWS-2022 ABWS-2023 ABWS-2024 ABWSL-2056
0.50 13 ABWS-1033 ABWS-1034 ABWS-1035 ABWS-1036 ABWSL-1045

Contoured Wedges

  • Improves coupling on curved surfaces
  • When ordering, please specify wedge type, contour orientation, and contour diameter
  • Example Part #: ABWM-4T-45-COD-1.25IN

AID (Axial Inside Diameter)
AOD (Axial Outside Diameter)
CID (Circumferential Inside Diameter)
COD (Circumferential Outside Diameter)

Loading...

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어