Inspection & Measurement Systems

Rilevatore di difetti

Immersione

Immersion Transducers

An immersion transducer is a single element longitudinal wave transducer with a 1/4 wavelength layer acoustically matched to water. Immersion transducers are specifically designed to transmit ultrasound in applications where the test parts are partially or wholly immersed in water, which allows a uniform and fast coupling technique for rapid scanning of parts. Focusing lens can be added to increase transducer sensitivity and performance in a particular area of a part. Immersion transducers can be focused either spherically or cylindrically upon request within the allowable focal range for a given frequency and element size.

Advantages:

  • The immersion technique provides a means of uniform coupling
  • Quarter wavelength matching layer increases sound energy output
  • Corrosion resistant 303 stainless steel case with chrome-plated brass connectors
  • Proprietary RF shielding for improved signal-to-noise characteristics in critical applications
  • All immersion transducers, except paintbrush, can be focused spherically (spot) or cylindrically (line) (see Technical Notes page 45)
  • Customer specified focal length concentrates the sound beam to increase sensitivity to small reflectors

Applications:

  • Automated scanning
  • On-line thickness gaging
  • High speed flaw detection in pipe, bar, tube, plate, and other similar components
  • Time-of-flight and amplitude based imaging
  • Through transmission testing
  • Material analysis and velocity measurements

Usage Note: Transducers should not be submerged for periods exceeding 8 hours. Allow 16 hours of dry time to ensure the life of the unit.

Large Diameter Case

  • Large element diameters increase near field length allowing for longer focal lengths
  • Larger diameters can increase scanning index
  • Low frequency, large element diameter designs available for challenging applications

Transducer Dimensions (in inches)

Nominal Element Size (A) (B) (C)
1.50 1.75 1.81 1.50
1.13 1.38 1.44 1.25
1.00 1.25 1.31 1.25
0.75 1.00 1.06 1.25

I-4, 1-7 and i-8 Style Housings

Various element and case sizes with straight UHF connectors and 303 stainless steel case housings are available.

Transducer Dimensions

Element Diameter (inches) A B
0.75 1.00 1.375
0.50, 0.625 0.748 1.375
1.00, 1.125 1.25 1.375

Transducer Configurator

*Please select a specific focus between min max.
**If a focus is required, select a focal length between min max

To view point target foci, click here.

Frequency (MHZ)
Nominal Element Size (in)
Transducer Type
Frequency
(MHz)
Nominal Element Size ACCUSCAN-S CENTRASCAN Power Series Resolution Series Standard Series VIDEOSCAN
in.mmPart /
Item No.
Part /
Item No.
Part /
Item No.
Part /
Item No.
Part /
Item No.
Part /
Item No.
5 0.75 19   I7-0012-P-SU

U8517150

Immersion Transducer, Power Series, I-7 style case, 0.500 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
  V318-SU

U8423038

Immersion Transducer, 0.5 MHz, 0.75 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 1 25 A301S-SU

U8421001

Immersion Transducer, 0.5 MHz, 1.00 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
 I8-0016-P-SU

U8517173

Immersion Transducer, Power Series, I-8 style case, 0.500 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
 I8-0016-S-SU

U8517174

Immersion Transducer, Standard Series, I-8 style case, 0.500 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
V301-SU

U8423001

Immersion Transducer, 0.5 MHz, 1.00 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 1.125 29 A391S-SU

U8421056

Immersion Transducer, 0.5 MHz, 1.125 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
 I8-0018-P-SU

U8517176

Immersion Transducer, Power Series, I-8 style case, 0.500 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
 I8-0018-S-SU

U8517177

Immersion Transducer, Standard Series, I-8 style case, 0.500 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
V391-SU

U8423073

Immersion Transducer, 0.5 MHz, 1.125 in. Element Diameter, Standard Case Style, Straight UHF Connector
5 1.5 39 A389S-SU

U8421055

Immersion Transducer, 0.5 MHz, 1.50 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
    V389-SU

U8423071

Immersion Transducer, 0.5 MHz, 1.50 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
1 0.5 13   I4-0108-P-SU

U8517083

Immersion Transducer, Power Series, I-4 style case, 1.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0108-R-SU

U8517084

Immersion Transducer, Resolution Series, I-4 style case, 1.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0108-S-SU

U8420054

Immersion Transducer, Standard Series, I-4 style case, 1.0 MHz, 0.500 in. dia; Straight UHF Connector
 
1 0.625 16   I4-0110-P-SU

U8517086

Immersion Transducer, Power Series, I-4 style case, 1.0 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0110-R-SU

U8517087

Immersion Transducer, Resolution Series, I-4 style case, 1.0 MHz, 0.625 in. element size; Straight UHF Connector
I4-0110-S-SU

U8517088

Immersion Transducer, Standard Series, I-4 style case, 1.0 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
 
1 0.75 19 A314S-SU

U8421029

Immersion Transducer, 1 MHz, 0.75 in. element size, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
 I7-0112-P-SU

U8517152

Immersion Transducer, Power Series, I-7 style case, 1.00 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
I7-0112-R-SU

U8520004

Immersion Transducer, 1.00 MHz, 0.750 in. Includes Test Form Certificate
I7-0112-S-SU

U8517153

Immersion Transducer, Standard Series, I-7 style case, 1.00 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
V314-SU

U8423029

Immersion Transducer, 1 MHz, 0.75 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
1 1 25  C302-SU

U8422001

Centrascan Composite Immersion Transducer, 1.00 MHz, 1.00 in. element size, Large Case Style, Straight UHF Connector Includes Test Form Certificate
I8-0116-P-SU

U8517179

Immersion Transducer, Power Series, I-8 style case, 1.0 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0116-R-SU

U8517180

Immersion Transducer, Resolution Series, I-8 style case, 1.0 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0116-S-SU

U8517181

Immersion Transducer, Standard Series, I-8 style case, 1.0 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
V302-SU

U8423003

Immersion Transducer, 1 MHz, 1.00 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
1 1.125 29 A394S-SU

U8421058

Immersion Transducer, 1 MHz, 1.125 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
 I8-0118-P-SU

U8517183

Immersion Transducer, Power Series, I-8 style case, 1.0 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0118-R-SU

U8517184

Immersion Transducer, Resolution Series, I-8 style case, 1.0 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0118-S-SU

U8517185

Immersion Transducer, Standard Series, I-8 style case, 1.0 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
V394-SU

U8423075

Immersion Transducer, 1 MHz, 1.125 in. Element Diameter, Standard Case Style, Straight UHF Connector, includes Test Form Certificate.
1 1.5 39 A392S-SU

U8421057

Immersion Transducer, 1 MHz, 1.50 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
    V392-SU

U8423074

Immersion Transducer, 1 MHz, 1.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
225 0.375 10   I4-0206-P-SU

U8517090

Immersion Transducer, Power Series, I-4 style case, 2.25 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0206-R-SU

U8517091

Immersion Transducer, Resolution Series, I-4 style case, 2.25 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0206-S-SU

U8517092

Immersion Transducer, Standard Series, I-4 style case, 2.25 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 
225 0.5 13   I4-0208-P-SU

U8517094

Immersion Transducer, Power Series, I-4 style case, 2.25 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0208-R-SU

U8517095

Immersion Transducer, Resolution Series, I-4 style case, 2.25 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0208-S-SU

U8517096

Immersion Transducer, Standard Series, I-4 style case, 2.25 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
 
225 0.625 16    I4-0210-R-SU

U8517098

Immersion Transducer, Resolution Series, I-4 style case, 2.25 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0210-S-SU

U8517099

Immersion Transducer, Standard Series, I-4 style case, 2.25 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
 
225 0.75 19 A305S-SU

U8421007

Immersion Transducer, 2.25 MHz, 0.75 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
C305-SU

U8422003

Centrascan Composite Immersion Transducer, 2.25 MHz,0.75 in. element size, Large Case Style, Straight UHF Connector Includes Test Form Certificate
I7-0212-P-SU

U8517155

Immersion Transducer, Power Series, I-7 style case, 2.25 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
I7-0212-R-SU

U8517156

Immersion Transducer, Resolution Series, I-7 style case, 2.25 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
I7-0212-S-SU

U8517157

Immersion Transducer, Standard Series, I-7 style case, 2.25 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
V305-SU

U8423007

Immersion Transducer, 2.25 MHz, 0.75 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
225 1 25 A304S-SU

U8421006

Immersion Transducer, 2.25 MHz, 1.00 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
C304-SU

U8422002

Centrascan Composite Immersion Transducer, 2.25 MHz,1.00 in. Element Diameter, Large Case Style, Straight UHF Connector Includes Test Form Certificate
I8-0216-P-SU

U8517186

Immersion Transducer, Power Series, I-8 style case, 2.25 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0216-R-SU

U8517187

Immersion Transducer, Resolution Series, I-8 style case, 2.25 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0216-S-SU

U8517188

Immersion Transducer, Standard Series, I-8 style case, 2.25 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
V304-SU

U8423006

Immersion Transducer, 2.25 MHz, 1.00 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
225 1.125 29 A397S-SU

U8421060

Immersion Transducer, 2.25 MHz, 1.125 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
 I8-0218-P-SU

U8517190

Immersion Transducer, Power Series, I-8 style case, 2.25 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0218-R-SU

U8517191

Immersion Transducer, Resolution Series, I-8 style case, 2.25 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0218-S-SU

U8517192

Immersion Transducer, Standard I-8 style case, 2.25 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
V397-SU

U8423077

Immersion Transducer, 2.25 MHz, 1.125 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
225 1.5 39 A395S-SU

U8421059

Immersion Transducer, 2.25 MHz, 1.50 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
    V395-SU

U8423076

Immersion Transducer, 2.25 MHz, 1.50 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
35 0.375 10   I4-0306-P-SU

U8517101

Immersion Transducer, Power Series, I-4 style case,3.5 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0306-R-SU

U8517102

Immersion Transducer, Resolution Series, I-4 style case,3.5 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0306-S-SU

U8517103

Immersion Transducer, Standard Series, I-4 style case,3.5 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 
35 0.5 13   I4-0308-P-SU

U8517105

Immersion Transducer, Power Series, I-4 style case,3.5 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0308-R-SU

U8517106

Immersion Transducer, Resolution Series, I-4 style case,3.5 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0308-S-SU

U8517107

Immersion Transducer, Standard Series, I-4 style case,3.5 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
 
35 0.625 16   I4-0310-P-SU

U8517109

Immersion Transducer, Power Series, I-4 style case,3.5 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0310-R-SU

U8517110

Immersion Transducer, Resolution Series, I-4 style case,3.5 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0310-S-SU

U8517111

Immersion Transducer, Standard Series, I-4 style case,3.5 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
 
35 0.75 19 A381S-SU

U8421051

Immersion Transducer, 3.5 MHz, 0.75 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
C381-SU

U8422018

Centrascan Composite Immersion Transducer, 3.50 MHz, 0.75 in. Element Diameter, Large Case Style, Straight UHF Connector Includes Test Form Certificate
I7-0312-P-SU

U8517159

Immersion Transducer, Power Series, I-7 style case,3.5 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
I7-0312-R-SU

U8517160

Immersion Transducer, Resolution Series, I-7 style case,3.5 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
I7-0312-S-SU

U8517161

Immersion Transducer, Standard Series, I-7 style case,3.5 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
V381-SU

U8423063

Immersion Transducer, 3.5 MHz, 0.75 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
35 1 25 A380S-SU

U8421050

A380S-SU IMM: Immersion Transducer 3.5 MHz, 1 in. element diameter, Straight UHF Connector. Includes Test Form Certificate
C380-SU

U8422017

Centrascan Composite Immersion Transducer, 3.50 MHz, 1.00 in. Element Diameter, Large Case Style, Straight UHF Connector Includes Test Form Certificate
   V380-SU

U8423061

Immersion Transducer, 3.5 MHz, 1.00 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 0.375 10   I4-0506-P-SU

U8517113

Immersion Transducer, Power Series, I-4 style case, 5.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0506-R-SU

U8517114

Immersion Transducer, Resolution Series, I-4 style case, 5.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0506-S-SU

U8517115

Immersion Transducer, Standard Series, I-4 style case, 5.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 
5 0.5 13   I4-0508-P-SU

U8517116

Immersion Transducer, Gaging Series, I-4 style case, 5.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0508-R-SU

U8517117

Immersion Transducer, Resolution Series, I-4 style case, 5.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0508-S-SU

U8517118

Immersion Transducer, Standard Series, I-4 style case, 5.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
 
5 0.625 16   I4-0510-P-SU

U8517120

Immersion Transducer, Power Series, I-3 style case, 5.0 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0510-R-SU

U8517121

Immersion Transducer, Resolution Series, I-4 style case, 5.0 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-0510-S-SU

U8517122

Immersion Transducer, Standard Series, I-4 style case, 5.0 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
 
5 0.75 19 A308S-SU

U8421011

Immersion Transducer, 5 MHz, 0.75 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
C308-SU

U8422007

Centrascan Composite Immersion Transducer, 5.0 MHz, 0.75 in. Element Diameter, Large Case Style, Straight UHF Connector Includes Test Form Certificate
I7-0512-P-SU

U8517163

Immersion Transducer, Power Series, I-7 style case, 5.0 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
I7-0512-R-SU

U8517165

Immersion Transducer, Resolution Series, I-7 style case, 5.0 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
I7-0512-S-SU

U8517167

Immersion Transducer, Standard Series, I-7 style case, 5.0 MHz, 0.750 in. element size; Straight UHF Connector Includes Test Form Certificate
V308-SU

U8423012

Immersion Transducer, 5 MHz, 0.75 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 1 25 A307S-SU

U8421010

Immersion Transducer, 5 MHz, 1.00 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
 I8-0516-P-SU

U8517194

Immersion Transducer, Power Series, I-8 style case, 5.0 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0516-R-SU

U8517284

Immersion Transducer, Resolution Series, I-8 style case, 5.0 MHz, 1.00 in. dia; Straight UHF Connector
I8-0516-S-SU

U8517195

Immersion Transducer, Standard Series, I-8 style case, 5.0 MHz, 1.00 in. element size; Straight UHF Connector Includes Test Form Certificate
V307-SU

U8423010

Immersion Transducer, 5 MHz, 1.00 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 1.125 29   I8-0518-P-SU

U8517197

Immersion Transducer, Power Series, I-8 style case, 5.0 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0518-R-SU

U8517198

Immersion Transducer, Resolution Series, I-8 style case, 5.0 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
I8-0518-S-SU

U8517199

Immersion Transducer, Standard Series, I-8 style case, 5.0 MHz, 1.125 in. element size; Straight UHF Connector Includes Test Form Certificate
 
75 0.375 10     I4-0706-S-SU

U8517125

Immersion Transducer, Standard Series, I-4 style case, 7.5 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 
75 0.5 13     I4-0708-S-SU

U8517128

Immersion Transducer, Standard Series, I-4 style case, 7.5 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
 
75 0.625 16     I4-0710-S-SU

U8517131

Immersion Transducer, Standard Series, I-4 style case, 7.5 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
 
75 0.75 19 A321S-SU

U8421036

Immersion Transducer, 7.5 MHz, 0.75 in. Element Diameter, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
    V321-SU

U8423043

Immersion Transducer, 7.5 MHz, 0.75 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
10 0.375 10    I4-1006-R-SU

U8517133

Immersion Transducer, Resolution Series, I-4 style case, 10 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-1006-S-SU

U8517134

Immersion Transducer, Standard Series, I-4 style case, 10 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 
10 0.5 13    I4-1008-R-SU

U8517136

Immersion Transducer, Resolution Series, I-3 style case, 10 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-1008-S-SU

U8517137

Immersion Transducer, Standard Series, I-4 style case, 10 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
 
10 0.625 16    I4-1010-R-SU

U8517139

Immersion Transducer, Resolution Series, I-4 style case, 10 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-1010-S-SU

U8517140

Immersion Transducer, Standard Series, I-4 style case, 10 MHz, 0.625 in. element size; Straight UHF Connector Includes Test Form Certificate
 
10 0.75 19 A315S-SU

U8421030

Immersion Transducer, 10 MHz, 0.75 in. element size, Large Diameter Case Style, Straight UHF Connector Includes Test Form Certificate
    V315-SU

U8423030

Immersion Transducer, 10 MHz, 0.75 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
10 1 25      V322-SU

U8423044

Immersion Transducer, 10 MHz, 1.00 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
15 0.375 10    I4-1506-R-SU

U8517142

Immersion Transducer, Resolution Series, I-4 style case, 15 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-1506-S-SU

U8517143

Immersion Transducer, Standard Series, I-4 style case, 15 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 
15 0.5 13    I4-1508-R-SU

U8517145

Immersion Transducer, Resolution Series, I-4 style case, 15 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-1508-S-SU

U8517146

Immersion Transducer, Standard Series, I-4 style case, 15 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
 
20 0.375 10    I4-2006-R-SU

U8517148

Immersion Transducer, Resolution Series, I-4 style case, 20 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I4-2006-S-SU

U8517149

Immersion Transducer, Standard Series, I-4 style case, 20 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 

Standard Case

  • Knurled case with Straight UHF connect or (SU)
  • Contact us for nonknurled case design and availability of other connector styles
  • Frequencies ranging from 1.0 to 25 Mhz

i-3 Style Housing

0.25 inches (6 mm), 0.375 inches (10 mm) and 0.50 inches (13 mm) element diameters in 0.63 inches (16 mm) housings with straight UHF connectors and 303 stainless steel case housings. If a focus is required, select a focal length between min. and max.

Transducer Configurator

*Please select a specific focus between min max.
**If a focus is required, select a focal length between min max.

To view point target foci, click here.

Frequency (MHZ)
Nominal Element Size (in)
Transducer Type
Frequency
(MHz)
Nominal Element Size ACCUSCAN-S CENTRASCAN Power Series Resolution Series Standard Series VIDEOSCAN
in.mmPart /
Item No.
Part /
Item No.
Part /
Item No.
Part /
Item No.
Part /
Item No.
Part /
Item No.
1 0.5 13 A303S-SU

U8421005

Immersion Transducer, 1 MHz, 0.50 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
 I3-0108-P-SU

U8517027

Immersion Transducer, Power Series, I-3 style case, 1.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
 I3-0108-S-SU

U8517028

Immersion Transducer, Standard Series, I-3 style case, 1.0 MHz, 0.500 in. element size.; Straight UHF Connector Includes Test Form Certificate
V303-SU

U8423005

Immersion Transducer, 1 MHz, 0.50 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
225 0.25 6  C323-SU

U8422014

Centrascan Composite Immersion Transducer, 2.25 MHz, 0.25 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0204-P-SU

U8517030

Immersion Transducer, Power Series, I-3 style case, 2.25 MHz, 0.250 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0204-R-SU

U8517031

Immersion Transducer, Resolution Series, I-3 style case, 2.25 MHz, 0.250 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0204-S-SU

U8517032

Immersion Transducer, Standard Series, I-3 style case, 2.25 MHz, 0.250 in. element size.; Straight UHF Connector Includes Test Form Certificate
V323-SU

U8423048

Immersion Transducer, 2.25 MHz, 0.25 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
225 0.375 10  C325-SU

U8422015

Centrascan Composite Immersion Transducer, 2.25 MHz, 0.375 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0206-P-SU

U8517034

Immersion Transducer, Power Series, I-3 style case, 2.25 MHz, 0.375 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0206-R-SU

U8517035

Immersion Transducer, Resolution Series, I-3 style case, 2.25 MHz, 0.375 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0206-S-SU

U8517036

Immersion Transducer, Gagging Series, I-3 style case, 2.25 MHz, 0.375 in. element size; Straight UHF Connector, includes Test Form Certificate.
V325-SU

U8423053

Immersion Transducer, 2.25 MHz, 0.375 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
225 0.5 13 A306S-SU

U8421009

Immersion Transducer, 2.25 MHz, 0.50 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
C306-SU

U8422004

Centrascan Composite Immersion Transducer, 2.25 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0208-P-SU

U8517038

Immersion Transducer, Power Series, I-3 style case, 2.25 MHz, 0.500 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0208-R-SU

U8517039

Immersion Transducer, Resolution Series, I-3 style case, 2.25 MHz, 0.500 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0208-S-SU

U8517040

Immersion Transducer, Standard Series, I-3 style case, 2.25 MHz, 0.500 in. element size.; Straight UHF Connector Includes Test Form Certificate
V306-SU

U8423009

Immersion Transducer, 2.25 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
35 0.25 6  C384-SU

U8422021

Centrascan Composite Immersion Transducer, 3.50 MHz, 0.25 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0304-P-SU

U8517042

Immersion Transducer, Power Series, I-3 style case,3.5 MHz, 0.250 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0304-R-SU

U8517043

Immersion Transducer, Resolution Series, I-3 style case,3.5 MHz, 0.250 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0304-S-SU

U8517044

Immersion Transducer, Standard Series, I-3 style case,3.5 MHz, 0.250 in. element size.; Straight UHF Connector Includes Test Form Certificate
V384-SU

U8423070

Immersion Transducer, 3.5 MHz, 0.25 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
35 0.375 10  C383-SU

U8422020

Centrascan Composite Immersion Transducer, 3.50 MHz, 0.375 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0306-P-SU

U8517046

Immersion Transducer, Standard Series, I-3 style case,3.5 MHz, 0.375 in. element size.; Straight UHF Connector Includes Test Form Certificate
I3-0306-R-SU

U8517047

Immersion Transducer, Resolution Series, I-3 style case,3.5 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0306-S-SU

U8517048

Immersion Transducer, Standard Series, I-3 style case,3.5 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
V383-SU

U8423066

Immersion Transducer, 3.5 MHz, 0.375 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
35 0.5 13 A382S-SU

U8421053

Immersion Transducer, 3.5 MHz, 0.50 in. Element Diameter, Stanard Case Style, Straight UHF Connector Includes Test Form Certificate
C382-SU

U8422019

Centrascan Composite Immersion Transducer, 3.50 MHz, 0.50 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0308-P-SU

U8517049

Immersion Transducer, Power Series, I-3 style case,3.5 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0308-R-SU

U8517233

Immersion Transducer, Resolution Series, I-3 style case, 3.5MHz, 0.500 in. element size, Straight UHF Connector. Includes Test Form Certificate
I3-0308-S-SU

U8517050

Immersion Transducer, Standard Series, I-3 style case,3.5 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
V382-SU

U8423065

Immersion Transducer, 3.5 MHz, 0.50 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 0.25 6 A310S-SU

U8421018

Immersion Transducer, 5 MHz, 0.25 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
C310-SU

U8422012

Centrascan Composite Immersion Transducer, 5.00 MHz, 0.25 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0504-P-SU

U8517052

Immersion Transducer, Power Series, I-3 style case, 5.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0504-R-SU

U8517053

Immersion Transducer, Resolution Series, I-3 style case, 5.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0504-S-SU

U8517054

Immersion Transducer, Resolution Series, I-3 style case, 5.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
V310-SU

U8423017

Immersion Transducer, 5 MHz, 0.25 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 0.375 10 A326S-SU

U8421038

Immersion Transducer, 5 MHz, 0.375 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
C326-SU

U8422016

Centrascan Composite Immersion Transducer, 5.00 MHz, 0.375 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0506-P-SU

U8517056

Immersion Transducer, Power Series, I-3 style case, 5.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0506-R-SU

U8517057

Immersion Transducer, Resolution Series, I-3 style case, 5.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0506-S-SU

U8517058

Immersion Transducer, Resolution Series, I-3 style case, 5.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
V326-SU

U8423054

Immersion Transducer, 5 MHz, 0.375 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
5 0.5 13 A309S-SU

U8421013

Immersion Transducer, 5 MHz, 0.50 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
C309-SU

U8422008

Centrascan Composite Immersion Transducer, 5.00 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
I3-0508-P-SU

U8517060

Immersion Transducer, Power Series, I-3 style case, 5.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0508-R-SU

U8517061

Immersion Transducer, Resolution Series, I-3 style case, 5.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-0508-S-SU

U8517063

Immersion Transducer, Standard Series, I-3 style case, 5.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
V309-SU

U8423013

Immersion Transducer, 5 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
75 0.5 13 A320S-SU

U8421035

Immersion Transducer, 7.5 MHz, 0.50 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
  I3-0708-R-SU

U8517220

Immersion Transducer, Resolution Series, I-3 style case, 7.5 MHz, 0.500 in. dia; Straight UHF Connector Includes Test Form Certificate
 V320-SU

U8423042

Immersion Transducer, 7.5 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
10 0.25 6 A312S-SU

U8421024

Immersion Transducer, 10 MHz, 0.25 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
  I3-1004-R-SU

U8517066

Immersion Transducer, Resolution Series, I-3 style case, 10.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-1004-S-SU

U8517067

Immersion Transducer, Standard Series, I-3 style case, 10.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
V312-SU

U8423024

Immersion Transducer, 10 MHz, 0.25 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
10 0.375 10 A327S-SU

U8421039

Immersion Transducer, 10 MHz, 0.375 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
  I3-1006-R-SU

U8517069

Immersion Transducer, Resolution Series, I-3 style case, 10.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-1006-S-SU

U8517070

Immersion Transducer, Standard Series, I-3 style case, 10.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
V327-SU

U8423055

Immersion Transducer, 10 MHz, 0.375 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
10 0.5 13 A311S-SU

U8421020

Immersion Transducer, 10 MHz, 0.50 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
  I3-1008-R-SU

U8517073

Immersion Transducer, Resolution Series, I-3 style case, 10.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-1008-S-SU

U8517074

Immersion Transducer, Standard Series, I-3 style case, 10.0 MHz, 0.500 in. element size; Straight UHF Connector Includes Test Form Certificate
V311-SU

U8423019

Immersion Transducer, 10 MHz, 0.50 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
15 0.25 6 A313S-SU

U8421028

Immersion Transducer, 15 MHz, 0.25 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
  I3-1504-R-SU

U8517076

Immersion Transducer, Resolution Series, I-3 style case, 15.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
 V313-SU

U8423028

Immersion Transducer, 15 MHz, 0.25 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
15 0.375 10    I3-1506-R-SU

U8517079

Immersion Transducer, Resolution Series, I-3 style case, 15.0 MHz, 0.375 in. element size; Straight UHF Connector Includes Test Form Certificate
 V328-SU

U8423056

Immersion Transducer, 15 MHz, 0.375 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
15 0.5 13 A319S-SU

U8421032

Immersion Transducer, 15 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
    V319-SU

U8423040

Immersion Transducer, 15 MHz, 0.50 in. Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
20 0.125 3      V316-SU

U8423034

Immersion Transducer, 20 MHz, 0.125 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
20 0.25 6    I3-2004-R-SU

U8517080

Immersion Transducer, Resolution Series, I-3 style case, 20.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
I3-2004-S-SU

U8517081

Immersion Transducer, Standard Series, I-3 style case, 20.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
V317-SU

U8423037

Immersion Transducer, 20 MHz, 0.25 in. element size, Standard Case Style, Straight UHF Connector Includes Test Form Certificate
25 0.25 6    I3-2504-R-SU

U8519002

Immersion Transducer, Resolution Series, I-3 style case, 25.0 MHz, 0.250 in. element size; Straight UHF Connector Includes Test Form Certificate
 V324-SU

U8423052

Immersion Transducer, 25 MHz, 0.25" Element Diameter, Standard Case Style, Straight UHF Connector Includes Test Form Certificate  
25 0.375    I3-2506-R-SU

U8519011

Immersion Transducer, Resolution Series, I-3 style case, 25.0 MHz, 0.375 in. dia; Straight UHF Connector
  

Slim Line Case

  • Stainless steel case is only 0.38" (10 mm) in diameter, ideal for limited access areas
  • Standard configuration is Straight and fits Microdot ® connector style

i-1 and i-2 Style Housings

0.25 inches (6 mm) diameter elements with 0.375 inches (10 mm) housings for difficult to reach fillet or bore areas are available with straight Microdot (I-1) or straight UHF (I-2) connectors and 303 stainless steel housings.

Transducer Configurator

*Please select a specific focus between min max.
**If a focus is required, select a focal length between min max
To view transducer point target focus, click here.

Frequency (MHZ)
Nominal Element Size (in)
Transducer Type
Frequency
(MHz)
Nominal Element Size ACCUSCAN-S Resolution Series Standard Series VIDEOSCAN
in.mmPart /
Item No.
Part /
Item No.
Part /
Item No.
Part /
Item No.
225 0.25 6  
I1-0204-R-SM

U8518002

Immersion Transducer, Resolution Series, I-1 Slim Line style case, 2.25 MHz, 0.25 in. dia; Straight Microdot Connector Includes Test Form Certificate  
I2-0204-R-SU

U8517003

Immersion Transducer, Resolution Series, I-2 style case, 2.25MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
I1-0204-S-SM  

U8518003 

Immersion Transducer, Standard Series, I-1 Slim Line style case, 2.25 MHz, 0.25 in. dia; Straight Microdot Connector Includes Test Form Certificate  
I2-0204-S-SU

U8517004

Immersion Transducer, Standard Series, I-2 style case, 2.25MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
V323-SM

U8423047

Immersion Transducer, 2.25 MHz, 0.25 in. Element Diameter, Slim Line Case Style, Straight Microdot Connector Includes Test Form Certificate
35 0.25 6  
I1-0304-R-SM

U8518006

Immersion Transducer, Resolution Series, I-1 Slim Line style case, 3.5MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate  
I2-0304-R-SU

U8517007 

Immersion Transducer, Resolution Series, I-2 style case, 3.5 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
I1-0304-S-SM 

U8518007

Immersion Transducer, Standard Series, I-1 Slim Line style case, 3.5MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate  
I2-0304-S-SU 

U8517008

Immersion Transducer, Standard Series, I-2 style case, 3.5 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
V384-SM

U8423069

Immersion Transducer, 3.5 MHz, 0.25 in. Element Diameter, Slim Line Case Style, Straight Microdot Connector Includes Test Form Certificate
5 0.25 6 A310S-SM

U8421017

Immersion Transducer, 5 MHz, 0.25 in. Element Diameter, Straight Microdot Connector Includes Test Form Certificate
I1-0504-R-SM

U8518010

Immersion Transducer, Resolution Series, I-1 Slim Line style case, 5.0MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate  
I2-0504-R-SU

U8517011 

Immersion Transducer, Resolution Series, I-2 style case, 5.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate 
I1-0504-S-SM 

U8518011

Immersion Transducer, Standard Series, I-1 Slim Line style case, 5.0MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate
I2-0504-S-SU

U8517012

Immersion Transducer, Standard Series, I-2 style case, 5.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
V310-SM

U8423016

Immersion Transducer, 5 MHz, 0.25 in. Element Diameter, Slim Line Case Style, Straight Microdot Connector Includes Test Form Certificate
10 0.25 6 A312S-SM

U8421023

Immersion Transducer, 10 MHz, 0.25 in. element size, Straight Microdot Connector Includes Test Form Certificate
I1-1004-R-SM

U8518014 

Immersion Transducer, Resolution Series, I-1 Slim Line style case, 10.0 MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate
I2-1004-R-SU

U8517231 

Immersion Transducer, Resolution Series, I-2 style case, 10.0 MHz 0.25 in. diameter; Straight UHF Connector, Includes Test Form Certificate 
I1-1004-S-SM

U8518015 

Immersion Transducer, Standard Series, I-1 Slim Line style case, 10.0 MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate 
I2-1004-S-SU

U8517016

Immersion Transducer, Standard Series, I-2 style case, 10.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
V312-SM

U8423023

Immersion Transducer, 10 MHz, 0.25 in. Element Diameter, Slim Line Case Style, Straight Microdot Connector Includes Test Form Certificate
15 0.25 6 A313S-SM

U8421027

Immersion Transducer, 15 MHz, 0.25 in. Element Diameter, Straight Microdot Connector Includes Test Form Certificate
I1-1504-R-SM 

U8518017  

Immersion Transducer, Resolution Series, I-1 Slim Line style case, 15.0 MHz, 0.250" dia; Straight Microdot Connector Includes Test Form Certificate
I2-1504-R-SU 

U8517018

Immersion Transducer, Resolution Series, I-2 style case, 15.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
I1-1504-S-SM 

U8518018

Immersion Transducer, Standard Series, I-1 Slim Line style case, 15.0 MHz, 0.250" dia; Straight Microdot Connector Includes Test Form Certificate
I2-1504-S-SU

U8517019 

Immersion Transducer, Standard Series, I-2 style case, 15.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
V313-SM

U8423027

Immersion Transducer, 15 MHz, 0.25 in. Element Diameter, Slim Line Case Style, Straight Microdot Connector Includes Test Form Certificate
20 0.125 3    V316-SM

U8423033

Immersion Transducer, 20 MHz, 0.125 in. Element Diameter, Slim Line Case Style, Straight Microdot Connector Includes Test Form Certificate
20 0.25 6  
I1-2004-R-SM

U8518020

Immersion Transducer, Resolution Series, I-1 Slim Line style case, 20.0 MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate  
I2-2004-R-SU

U8517022

Immersion Transducer, Resolution Series, I-2 style case, 20.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
I1-2004-S-SM

U8518021

Immersion Transducer, Standard Series, I-1 Slim Line style case, 20.0 MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate  
I2-2004-S-SU

U8517023

Immersion Transducer, Standard Series, I-2 style case, 20.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate
V317-SM

U8423036

Immersion Transducer, 20 MHz, 0.25 in. element size, Slim Line Case Style, Straight Microdot Connector Includes Test Form Certificate
25 0.25 6  
I1-2504-R-SM

U8517204 

Immersion Transducer, Resolution Series, I-1 Slim Line style case, 25.0 MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate
I2-2504-R-SU

U8517207

Immersion Transducer, Resolution Series, I-2 style case, 25.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate  
I1-2504-S-SM

U8517205

Immersion Transducer, Standard Series, I-1 Slim Line style case, 25.0 MHz, 0.25" dia; Straight Microdot Connector Includes Test Form Certificate
I2-2504-S-SU

U8517209 

Immersion Transducer, Standard Series, I-2 style case, 25.0 MHz, 0.25" dia; Straight UHF Connector Includes Test Form Certificate 
V324-SM

U8423051

Immersion Transducer, 25 MHz, 0.25 in. Element Diameter, Standard Case Style, Straight Microdot Connector Includes Test Form Certificate

Pencil Case

  • Small diameter, 2" (51 mm) long barrel improves access to difficult-to-reach areas
  • Standard connector style is Straight UHF (SU)

Transducer Configurator

*Please select a specific focus between min max.
**If a focus is required, select a focal length between min max
To view point target foci, click here.

Frequency (MHZ)
Nominal Element Size (in)
Transducer Type
Frequency
(MHz)
Nominal Element Size ACCUSCAN-S VIDEOSCAN
in.mmPart /
Item No.
Part /
Item No.
225 0.25 6  V323-N-SU

U8423045

Immersion Transducer, 2.25 MHz, 0.25 in. element size, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate
35 0.25 6  V384-N-SU

U8423067

Immersion Transducer, 3.5 MHz, 0.25 in. element size, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate
5 0.25 6 A310S-N-SU

U8421014

Immersion Transducer, 5 MHz, 0.25 in. element size, Straight UHF Connector Includes Test Form Certificate
V310-N-SU

U8423014

Immersion Transducer, 5 MHz, 0.25 in. Element Diameter, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate
10 0.25 6 A312S-N-SU

U8421021

Immersion Transducer, 10 MHz, 0.25 in. Element Diameter, Straight UHF Connector Includes Test Form Certificate
V312-N-SU

U8423021

Immersion Transducer, 10 MHz, 0.25 in. element size, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate
15 0.25 6 A313S-N-SU

U8421025

Immersion Transducer, 15 MHz, 0.25 in. element size, Straight UHF Connector Includes Test Form Certificate
V313-N-SU

U8423025

Immersion Transducer, 15 MHz, 0.25 in. Element Diameter, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate
20 0.125 3  V316-N-SU

U8423032

Immersion Transducer, 20 MHz, 0.125 in. Element Diameter, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate
20 0.25 6  V317-N-SU

U8423035

Immersion Transducer, 20 MHz, 0.25 in. Element Diameter, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate
25 0.25 6  V324-N-SU

U8423049

Immersion Transducer, 25 MHz, 0.25 in. Element Diameter, Pencil Case Style, Straight UHF Connector Includes Test Form Certificate

Loading...

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어