Industrial Testing Instruments

EPOCH 4B

Prodotti obsoleti

The Panametrics-NDT™ EPOCH 4B is a general purpose digital ultrasonic flaw detector that combines many practical features for flaw detection and thickness measurements, a rugged and splash proof housing, and a numeric datalogger. An intuitive direct-access keypad with fewer keys, easy thumb control of critical parameter settings, and convenient portability make the EPOCH 4B an excellent choice for inspectors who need an affordable and easy-to-use flaw detector.
Standard measurement features include DAC and TVG software, a 25 MHz bandwidth for thin material testing, a fast 60 Hz display update rate, a tunable square wave pulser for attenuating materials, and many other benefits for weld inspection, thickness monitoring, bond inspection, and crack detection and sizing.
The EPOCH 4B offers several software options. The narrowband filter option improves signal-to-noise ratio in high gain applications. AWS D1.1/D1.5 provides a "dynamic reflector" indication rating for various weld inspection classifications. The API 5UE software uses the Amplitude Distance Differential technique from API's Recommended Practice 5UE to size cracking in OCTG pipe during prove-up. Echo-to-Echo provides true metal thickness measurements with no need to remove paint or coating. Other options include Low PRF, Expanded Memory, and Extended Range.

Features

• Selectable, tunable square wave or negative spike excitation pulser
• Light, ergonomically designed (5.7 lbs./2.6 Kg)
• Fast, minimum 60 Hz display update rate
• High-power NiMH battery
• Large, bright, high-resolution ELD with full/split screen views
• Automated transducer calibration
• Display Freeze holds waveform and soundpath data
• Soundpath data viewable in inches, millimeters, or microseconds
• Basic DAC/TVG standard
• Peak Memory
• RF display mode
• Alarms, threshold positive/negative, or minimum depth
• Numeric datalogger
• Security Key enables remote upgrade of software options

Instrument software options

• Advanced DAC/TVG
• Expanded Memory
• Low PRF
• Echo-to-Echo thickness measurement
• Extended range
• Narrowband filters
• AWS D1.1/D1.5
• API 5UE

EPOCH 4B Specifications*

MEASUREMENTS
Sensitivity: 110 dB Max and Reference level sensitivity feature with 6 dB or 0.1 dB selectable resolution.
Auto Transducer Calibration: Automated calibration of transducer Zero Offset and/or Velocity.
Reject: 0% to 80% of full scale in 1% increments
Units: English, Metric, or Microseconds
Material Velocity: 0.025 to 0.6000 in/µsec (635 to 15240 m/S)
Range:
- Standard 0.16 inch to 200 inch (4 mm to 5,000 mm)
- Optional 0.038 inch to 400 inch (1 mm to 10,000 mm)
Refracted Angle: Fixed settings of 0°, 30°, 45°, 60°, 70°, or variable from 10° to 85° in 0.1° resolution
Peak Memory: Simultaneous display of live A-scan at 60 Hz update rate and peak envelope of A-scan display
Pulser Type: User selectable, tunable square wave, negative spike excitation
Pulse Energy: Low (100 V), Medium
(200 V), High (300 V), and Max (400 V)
Damping: 50, 63, 150, and 400 Ohms
Rectification: Full Wave, Half Wave Positive or Negative, and unrectified RF settings
Analog Bandwidth: 0.3 MHz to
25 MHz at -3 dB
Filters: Broadband; Optional narrowband filters
Test Modes: Pulse Echo, Dual, or Thru-Transmission
Alarms: Selectable threshold positive/negative or minimum depth modes

DISPLAY
Display: 320 pixels (W) X 240 pixels (H), ELD screen
Display Update Rate: Minimum 60 Hz

POWER SUPPLY
Power Requirements: AC Mains: 100-120 VAC, 200-240 VAC, 50-60 Hz
Battery: Internal Rechargeable NiMH battery pack rated at 12 V at 4000 mAH
BatteryOperating Time: 7 hours nominal. 2 hours typical recharge time
OUTPUTS
HighSpeed Parallel Port: Allows output of alarm conditions
Analog Output: Keypad selectable voltage output of depth or amplitude data
VGAOutput Port: Connects to standard VGA monitor or A/V projector
RS-232 Communications Port: Allows interfacing with PCs and printers. Max Baud Rate, 38.4.

GENERAL
Keypad: English or International symbols
Languages: Available in keypad selectable languages: English, French, German, Spanish, Italian, Russian, Japanese, and user-defined custom languages
Transducer Cable Connectors: Fits BNC or Number 1 Lemo®
Dimensions: 11.15" H x 6.55" W x 2.6" T
Weight: 5.7 lbs. (2.6 Kg) with battery
Operating Temperature: -20° C to 50° C (-4° F to 122° F)
Storage Temperature: -40° C to 70° C (-40° F to 158° F) depending on battery and display
PC Requirements: Compatible with Microsoft® Windows® XP®, Microsoft Windows 2000®
Warranty: One year warranty, battery not included. Optional second year warranty available.

STANDARD INCLUSIONS
EPOCH 4B Microprocessor-Based Ultrasonic Flaw Detector includes:
• EP4/MCA Mini Charger Adapter
• EP4/BAT Nickel Metal Hydride Rechargeable Battery
• EP4/CAL-NIST NIST Calibration Certificate
• EP4B/MAN Instruction Manual
• EP4/TC Transport Case
• EP4/PS Stainless Steel Pipe Stand
• EP4/HS Hand Strap

Optional Accessories
EP4/SCShipping Hard Shell Case
EP4/BAT-AAAlkaline Battery Pack
EP4/ECExternal Stand-Alone Charger
EP4/RPCRubber Protective Carrying Case
EP4/PRPrinter: 110-120 V
EP4/PREPrinter: 230-240 V
EP4/DP-EDisplay Protectors (ELD)
EP4/DP-LDisplay Protectors (LCD)
EP4/C-15VGA-6VGA Cable
EP4/C-25PRL-6Parallel Port Cable
EP4/C-9FAT-6Serial Port Cable
GAGEVIEWPRO-KIT-SERIALInterface Program including Serial Port Cable

*All specifications are subject to change without notice.

Some Epoch 4B Applications

Measurement of wall thickness of steam boiler tubes with EMAT transducers
Ringdown Test for Bond Integrity
Measuring Internal Oxide Scale in Boiler Tubes
Ultrasonic Preamplifiers
An Introduction to Angle Beam Assemblies
High Temperature Ultrasonic Testing
Ultrasonic Couplants
Phase Shift Test for Bond Integrity
Ultrasonic Measurements of Liquids
Thickness Testing of Reinforced Rubber Conveyor Belts
Measuring Nodularity in Cast Iron
Ultrasonic Testing in the Foundry Industry
English | 日本語 | français | 中文 | Deutsch | italiano | čeština | magyar | Español | русский | Tiểng Việt | polski | português