Inspection & Measurement Systems

Detectores de Defeitos

Integrated Wedge and Code Compliant Probes

Integrated wedge and code compliant probes combine the probe and the wedge in the same housing, offering the lowest-profile probe-and-wedge combination for contact angle beam inspection. Coupling is always good between probe and wedge interfaces, as there is no need for couplant between the probe and wedge.

These probes are used for manual weld inspection using 40° to 70° simultaneously in addition to manual inspection of stress-corrosion cracking and AWS and DGS code compliant applications.

Advantages

  • Probe and wedge in the same housing
  • The lowest-profile probe-and-wedge combination for contact angle beam inspection
  • Coupling always good between probe and wedge interfaces, no need for couplant between the probe and wedge
  • Very small assembly for easy access in restricted areas
  • Inspections of 30° to 70° in steel, SW or LW
  • Easy to handle
  • Probes with an internal wedge can be specially ordered to fit a specific curvature radius.

Typical Applications

  • Manual weld inspection of 6.35 mm to 19 mm (0.25 in. to 0.75 in.) thick surfaces (butt joints, corner joints, tee joints), using 40° to 70° simultaneously
  • Manual inspection of stress-corrosion cracking
  • AWS and DGS code compliant applications

Probe Specifications and Dimensions

Part Number Item Number Frequency
(MHz)
Number of Elements Pitch
(mm)
Active Aperture
(mm)
Elevation
(mm)
Nominal Refracted Beam Angle in Steel Integrated Wedge External Dimensions
mm (in.)
L W H
2L8-DGS1 U8330598 2.0 8 1.0 8.0 9.0 58° SW Yes 27 (1.06) 17 (0.67) 22 (0.87)
4L16-DGS1 U8330597 4.0 16 0.5 8.0 9.0 58° SW Yes 27 (1.06) 17 (0.67) 22 (0.87)
2.25L16-45SW1 U8330014 2.25 16 0.75 12.0 12.0 45° SW Yes 30 (1.18) 15 (0.59) 31 (1.22)
2.25L16-45LW1 U8330495 2.25 16 0.75 12.0 12.0 45° LW Yes 30 (1.18) 15 (0.59) 31 (1.22)
5L16-45SW1 U8330496 5.0 16 0.60 9.6 10.0 45° SW Yes 30 (1.18) 15 (0.59) 31 (1.22)
5L16-45LW1 U8330497 5.0 16 0.60 9.6 10.0 45° LW Yes 30 (1.18) 15 (0.59) 31 (1.22)
2.25L16-AWS1 U8330660 2.25 16 1.0 16.0 16.0 N/A No 25 (0.98) 38 (1.50) 18 (0.71)
These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths