High-Sensitivity Probes for HTHA |
Earlier and More Reliable Detection of High-Temperature Hydrogen Attack |
Specifications |
Wedges for A38 and A28 ProbesThe A38 and A28 DLA probes’ dedicated angle-beam wedge series are optimized for weld volume and heat-affected zone inspection. The angle of these wedges is set to generate L-waves at a 65-degree nominal incident angle in steel. They feature a roof angle calculated for each AOD diameter from 4 in. to 48 in. (101.6 mm to 1220 mm). SA38 and SA28 wedges are available in two focus depths (FD) to cover a wide range of thicknesses, from 4 mm to 95 mm (0.16 in. to 3.74 in.). These wedges enable you to fully exploit the A38 probe’s extended focusing capabilities. |