Handheld XRF for Light Elements Phosphorus (P) in Steel


Think you have the fastest and most reliable HHXRF? Think again.

The DELTA Takes Phosphorus (P) in Steel Detection Limits to an All Time Low!

The right amount of P content can increase yield and tensile strength of low carbon steel improving its processing, matching and corrosion resistance characteristics. However, too much P can cause brittleness which reduces the steel's strength and ductility, and ultimately its value. Ultra-low carbon steels and line pipe steels are among the most demanding for low P content - less than 0.01%. Hence, highly accurate measurements of low levels of P in ferrous alloys are critical for predicting quality for end use and ultimately the selling point of the piping and components. The DELTA Premium, the latest Olympus development in HHXRF goes to an all time high in accuracy and an all time low in detection limits for P in steel. It detects trace levels of P as low as 0.014% in carbon steel without vacuum or helium purge attachments.

Oil Jetty
Oil Jetty Photo by DH Wright, 2009

Accurate Low Limits of Detection of Phosphorus (P) is Critical for Line Pipe Steels
Standard wt % P, Assay wt % P, DELTA Measured
FXS313 0.014 0.012
FXS314 0.037 0.036
FXS315 0.056 0.053
FXS316 0.077 0.079
FXS317 0.109 0.114
FXS318 0.321 0.319
Table X. Analysis results of six certified reference standards with varying P content
HHXRF Measurements taken with DELTA Premium for 5 sec Beam 1; 120 sec Beam 2

Analysis data

Assay results

The DELTA Premium detects P in Steel with a correlation coefficient (R2) of 0.9993 in the range or 0.014 to 0.321!

In addition to testing for P in steel, the scrap processing recycling industry depends on HHXRF analyzers for metal sorting, buying and selling. Managers cannot afford to depend on out-of-date and unreliable equipment, or untimely support of equipment. They also cannot afford to fall behind the technology curve. The analytical capabilities of HHXRF continue expanding, and new features continually continually enable operators to be more effective and efficient. Upgrade your HHXRF to the DELTA - the latest HHXRF loaded with innovative features and backed by the industry's best service and support.

Handheld XRF for Metals & Alloys Industries

Iron & Steel Non-ferrous Scrap & Secondary

Iron and steel are the most widely used of metals and alloys. Lighter metals, non-ferrous, newly developed and exotic alloys are also utilized extensively, but iron and steel are considered the basic raw materials for the majority of industrial goods and construction. Although produced from ores mined around the globe, steel is one of the most recycled materials in the world. From base form to recycled materials to finished products, metals and alloys are integral to the fabric of society, the consumption of which is often considered a primary indicator of development and economic progress.

Metals Alloys is a serious, dynamic business.

The DELTA XRF analyzer is an essential tool for all businesses involved in the trade or use of metals alloys. In seconds, you can nondestructively measure 25+ elements. Turnings, shavings, rods, wires, small parts, components, sizeable materials and large structures can all be analyzed directly, non-destructively. How you get them, how you make them, how you use them, how you sell them is how you measure them. Whether you check purity, chemistry, or grade ID for highest value, maximum recovery, quality, conformance, or maintenance and safety, our DELTA XRF analyzer will give you immediate answers to take action on now.

Delta Handheld XRF testing alloys
Olympus IMS
应用所使用的产品

DELTA合金与金属手持式X射线荧光分析仪可以进行专业性极强的材料化学分析,可快速精确地辨别合金级别和纯金属。这款分析仪在数秒钟之内就可做出合金化学成分的辨别及定级。从简单的分拣到复杂的级别划分,从来料检测到最后产品的核查,都可用到这款分析仪。
DELTA废料手持式XRF分析仪在半秒钟内可对大多数合金的级别和纯金属进行可靠的辨别。这些分析仪坚固结实,可以用于最恶劣的处理环境中。在数秒钟内可对大量的铁性和非铁性材料进行快速、可靠的合金分拣和分析。
DELTA Element是一款性价比极高的手持式X射线荧光(XRF)分析仪,这是一款经过优化的分析仪,可以进行废料金属的分拣、材料成份的辨别(PMI)、合金的质量保证和质量控制,以及贵金属的分析。
DELTA Professional将硅漂移探测器(SDD)和一个4W优化X射线管结合在一起使用,可在检测速度、检出限及可检元素的范围方面提供极为优质的性能。它可以分析合金和矿石中镁(Mg)及原子数更高的元素。DELTA Professional是Olympus所生产的最具问题解决价值的手持式XRF分析仪。
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK