Uranium Exploration, Pathfinders & Light Elements


Olympus' DELTA range of Portable X-Ray Fluorescence (XRF) Analyzers continue to lead the way in real time, in-field geochemical analysis. Custom built for exploration and mining specific applications, the DELTA hosts a powerful 4W X-ray Tube coupled with an application optimized anode and silicon drift detector providing the lowest possible Limits of Detection (LOD's) in the shortest possible analysis times. With a workable LOD of 2-4 ppm for both Uranium Thorium, the DELTA provides unparalleled performance for the Uranium Explorer with quantification at or below the same level as the average crustal abundance for Uranium (typically around 2-4 ppm U)

The DELTA's 3-Beam Soil Mode provides both the power and flexibility to tailor your analytical requirements in line with the geochemical signatures of the deposit style you are searching for, with access to a range of over 30 analytes. Whether you are exploring for Calcretes, Phosphorites or Unconformity-related style Uranium mineralization, the DELTA arrives configured with an effective pathfinder element suite which includes P, V, Ni, As, Mo Base Metals plus the ability to analyze Light Elements with the addition of 2-Beam Mining Mode. This added versatility enables analysis of Whole Rock Litho-Geochemistry and Alteration assemblages and can include Mg, Al, Si, P, S, K, Ca in addition to standard Mining Mode elements.

Delta Handheld XRF Analyzer testing a rock outside

Summary Geochemical Signatures
Deposit Type Geochemical Signatures
Unconformity-related Nl, Pb, Co, As, B, Mo
Sandstone Mo, Se, Ti, S, Fe
Breccia Complex (IOCG) Fe, Cu, Au, Ag, Ba, F & REE
Quartz-Pebble Conglomerate Ti, Au, Ag, REE, Fe, S, PGE, Ni, Co
Calcretes (Surficial) V
Phosphorite P, F
Other Uranium Deposit Types Include:Vein, Intrusive, Volcanic & Caldera-related, Metasomatic, Collapsed Breccia Pipe, Lignite & Black Shales
Table Source: ioGlobal Geochemistry Workshop - Oct 2008

Data sample result graphs

Olympus IMS

应用所使用的产品
DELTA Professional分析仪将硅漂移探测器(SDD)和一个4W优化X射线管结合在一起使用,可在检测速度、检出限及可检元素的范围方面提供非常高的性能。这款分析仪可以分析合金和矿石中镁(Mg)及原子数更高的元素。奥林巴斯所生产的DELTA Professional分析仪是一款性价比很高的手持式XRF分析仪。
在包含勘探、矿石品位/过程控制和保证环境可持续发展环节在内的整个矿产开发过程中,用于采矿和地球化学领域的DELTA手持式XRF分析仪可以即时得出检测结果,从而有助于决定所要采取的下一步措施。可在现场对金属、矿物及污染物进行探测。GPS-GIS-XRF用于即时绘制金属分布映射图,既节省时间又节省成本。