Headlamp Lens Waviness Measurement Using a Laser Microscope


Headlamp
Headlamp

Application

The laws of individual countries define the areas that automotive headlamps can and cannot illuminate. For this reason, headlamp lenses must provide a high level of accuracy in the distribution of light.
Accurate measurement of the waviness of the inside lens surface can verify if the proper light distribution has been achieved.

The Olympus solution

Measurement using the Olympus LEXT OLS5000 3D laser scanning confocal microscope

Features of the product

(1) The OLS5000 microscope measures the state of waviness by using a plane. Color images, laser images, and 3D profile data can all be obtained at the same time, expanding the range of analysis.

(2) Using the stitching mode, wide-area data can be easily obtained.

Images

Waviness measurement for an area of 2,120 × 1,196 µm
Waviness measurement for an area of 2,120 × 1,196 µm

Profile measurement for an area of 2,120 × 1,196 µm
Profile measurement for an area of 2,120 × 1,196 µm

Olympus IMS

应用所使用的产品

具有出色精度和光学性能的LEXT™OLS5100激光扫描显微镜配备了让系统更加易于使用的智能工具。其能够快速高效完成亚微米级形貌和表面粗糙度的精确测量任务,既简化了工作流程又能让您获得可信赖的高质量数据。

Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country