Nondestructive Precious Metals Assay and Karat ID


Get fast, accurate analysis results with the GoldXpert Portable Benchtop XRF Analyzer

The GoldXpert XRF analyzer is an easy-to‑use, cost-effective method to obtain alloy chemistry and karat classification with one nondestructive and non-intrusive test. And, in an economic environment where fast and accurate results are more important than ever, the GoldXpert XRF analyzer provides outstanding precision and accuracy. Whether you buy gold, sell or produce jewelry, fabricate metal, or recycle scrap metal, you need a fast, highly accurate method to determine karatage (gold content) for quality control and pricing.

GoldXpert screen
XRF is a widely used, proven, and accepted method of chemistry analysis and karating of precious metals samples, including purity and fineness. XRF analysis provides a less expensive, quicker testing alternative to fire assay and chemical tests, and on-the-spot analysis of your silver, platinum, or other materials, making it an easy way to boost customer confidence and ensure dealer reliability.

GoldXpert

gold jewelry
On-the-spot gold karat classification, 0-24kt
diamond ring
Accurate compositional analysis of platinum, silver, and other precious metals
silver coin
Determination of Gold and Silver content in coinage
silver bracelet
Identify and analyze unknown metals for pricing, and even lead screening

Our analyzers give you the benefit and convenience of easy, on-the-spot analysis, so you can feel confident about the results for your gold and precious metal assets. The followed accuracy and precision data was generated using a GoldXpert with a Si PIN detector system, and is representative of typical performance expected from a Si PIN base system:

gold graph from GoldXpert
Results Graph from GoldXpert
Silver Results Graph from GoldXpert

GoldXpert Portable Benchtop XRF

The Compact Professional Precious Metals Testing Solution

The GoldXpert offers the best of both worlds. A handsome countertop analyzer fit for the consumer showroom environment, it can also be networked for high productivity QA/QC jobs. The large chamber door opens quickly, with a push of the large front trigger. The GoldXpert can also function as a portable analyzer, running off of a rechargeable Li ION battery pack. Compact and lightweight, weighing only 22 lbs (10 kg), the GoldXpert can be transported easily to wherever testing is needed.

Leaded glass viewing window - easily see sample in chamber

Integrated camera indicating sample analysis points

Safe-closed beam XRF system

Small spot collimation for analysis; ability to switch between 3-mm and 10-mm diameter spots with one push of a button

4 W X-Ray tube, 200 µA current (max) plus optimized beam settings for accurate analysis

Small desktop footprint: 267 mm x 310 mm x 340 mm (10.5 in. x 12.2 in. x 13.4 in.) (with door closed)

GoldXpert

LED-lit sample chamber: 125 mm x 210 mm x 180 mm (4.9 in. x 8.2 in. x 7.0 in.)

Analysis indicator light with 360° visibility

Portable - optional battery operation for mobile off-site use

USB interface for high-speed data export and printing

Responsive, bright, color touch screen display

Silicon PIN detector system standard. Silicon Drift Detector system available for optimized precision and sensitivity.

Olympus IMS
应用所使用的产品

DELTA Element是一款性价比极高的手持式X射线荧光(XRF)分析仪,这是一款经过优化的分析仪,可以进行废料金属的分拣、材料成份的辨别(PMI)、合金的质量保证和质量控制,以及贵金属的分析。
DELTA Professional将硅漂移探测器(SDD)和一个4W优化X射线管结合在一起使用,可在检测速度、检出限及可检元素的范围方面提供极为优质的性能。它可以分析合金和矿石中镁(Mg)及原子数更高的元素。DELTA Professional是Olympus所生产的最具问题解决价值的手持式XRF分析仪。
GoldXpert是一款适用于摆放在陈列室环境的时尚台式分析仪。GoldXpert机体紧凑、轻便,重量仅有10公斤(22磅),可被方便地运送到任何地方完成检测任务。GoldXpert在数秒中之内即可提供材料精确的化学成份信息及克拉级别。
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK