2019년도 Minex Europe 2019 요약-현장에서의 Vanta XRF

Olympus’ Todd Houlahan, Director, International Mining, gave a presentation at Minex Europe in Sofia, Bulgaria in June 2019. This year’s conference topic was the future of sustainable mining in the Balkans and beyond.

The conference hosted over 190 delegates from 130 companies and 26 countries. The event featured keynote and technical sessions where attendees reviewed global mining progress and the development of sustainable, efficient, and responsible mining in Europe.

A popular topic at Minex Europe was the increasing demand from a variety of industries focused on extracting lithium, nickel, copper, and rare earth elements (REEs) and how this demand will influence the energy and automotive sectors. The role of the European Union for mineral imports and infrastructure for processing materials was also discussed.

Other hot topics for event attendees included:

  • Emerging exploration technologies
  • Challenges of new exploration companies
  • Mineral resource and grade control information
Olympus’ Todd Houlahan at Minex Europe

While at the conference, Todd presented case studies demonstrating the innovative use of pXRF in Southern and Eastern Europe. Case studies presented from customers in Serbia, Greece, Bosnia, and Turkey demonstrated:

  • In Serbia, XRF as a cost-effective analytical tool for early stage exploration through:
    • Identification of soil anomalies
    • pXRF results supplied to directors in daily drill reports to allow for immediate prioritization of subsequent drillholes without waiting for lab assays
    • Assisting geologists with logging and discrimination of lithologies
  • In Greece, use of XRF to extract multielement data from historic samples previously assayed only for copper (Cu) and gold (Au)
  • In Bosnia, use of XRF in processing operations and metallurgical accounting during plant commissioning
  • In Turkey, use of pXRF for pathfinder geochemistry, lithogeochemistry, and understanding different textures within drillcore, which led to greater understanding in a mineralization event environment

Read Todd's Presentation

Related Content

Olympus Geochem Technical Tutorial Series

XRF FAQs

Miss Us at PDAC? Here’s the Latest for Our Mining Customers

Identifying Rock Types and Mineralization with XRF at the Mount Pleasant Mine


Get In Touch
마케팅 전문가, 분석 장비

Michelle은 마케팅 커뮤니케이션에 9년 이상의 경력을 가지고 있으며, Olympus의 분석 장비 사업에서 X선 형광 및 X선 회절 분석기를 담당하고 있습니다. 그녀는 신제품 출시를 위해 제품, 엔지니어링 및 학술 지원 그룹과 협력하여 웨비나를 제작하고 애플리케이션 노트를 작성합니다.

9월 18, 2019
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
InSight 블로그 가입하기
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
아래 양식을 작성하여 원하는 내용을 알려주십시오.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.