Portable X-Ray Fluorescence (XRF) for Non-Chromate Conversion Coatings

Olympus portable XRF analyzers provide a rapid, nondestructive method for accurately determining the thickness of non-chromate conversion coatings. These measurements must fall within a target thickness range to ensure that subsequent paint coatings adhere properly and that the component is protected against corrosion.

Non-Chromate Conversion Coatings

Aluminum alloys are used for a range of commercial and residential construction materials. After the alloy is extruded, a conversion coating is applied to protect it against corrosion and ensure the proper adhesion of subsequent paint coatings.

Chromite conversion coatings have historically been popular, but hexavalent chromium poses environmental and health risks. Consequently, the European Union banned the coatings, leading to the rise of non-chromate conversion coatings as an alternative. Even in countries where hexavalent chromium is still allowed, many architects will only purchase material coated with non-chromate conversion coatings since they are safer and more environmentally friendly.

Titanium-zirconium (Ti-Zr) conversion coatings are popular non-chrome alternatives. Although they are safer, they are also colorless, making it impossible for an operator to visually determine if the coating has been applied evenly and in the right thickness. If the coating is too thick, there is the potential for adhesion failure while, if the coating is too thin, the aluminum alloy is more likely to corrode.

Vanta Portable XRF Analyzers

Vanta portable XRF analyzers provide a rapid, nondestructive method to ensure Ti-Zr-based conversion coatings have been applied and that the coatings are within the required thickness range. Data provided in Figure 1 illustrates the accurate coating thickness capabilities of the Vanta portable XRF.

Excellent correlation between results obtained using an Olympus Vanta XRF analyzer and coating thickness reference materials.
Figure 1. Excellent correlation between results obtained using an Olympus Vanta XRF analyzer and coating thickness reference materials.

Benefits of Vanta XRF Analyzers

The Olympus Vanta XRF instrument enables operators to analyze a range of coated materials in the warehouse or yard quickly and nondestructively. Features include:

  • Continuous operation at temperatures up to 50 °C (122 °F).
  • IP55/IP54 rated to withstand dirt, dust, and rain.
  • Rugged and built to pass a 4-foot drop test (MIL‑STD-810G) to help prevent breakages.
  • Connect to the Cloud to access and share data across multiple platforms from any location.*


 

*Requires optional wireless dongle.

Vanta XRF instrument

Olympus IMS

이 애플리케이션에 사용되는 제품
Vanta™ 휴대용 XRF 분석기 시리즈는 최신의 가장 강력한 휴대용 XRF 장치로서 현장에서 실험실 품질의 결과를 요구하는 고객을 위해 신속하고 정확한 요소 분석을 제공합니다. 분석기는 IP55 또는 IP54 등급으로 견고하게 제작됐으며, 가동 시간 향상과 소유 비용 절감을 위해 낙하 시험을 거쳤습니다.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
아래 양식을 작성하여 원하는 내용을 알려주십시오.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.