Evident LogoOlympus Logo
자료실
Application Notes
자료로 돌아가기

항공 우주 고정구 구멍의 위상 배열 검사


Phased Array Inspection of Aerospace Fastener Holes

Military forces around the world are extending the life of aging aircraft by using phased array ultrasound testing to detect cracks and other flaws to help prevent catastrophic failures.

One time-consuming challenge is inspecting aircraft fastener holes to detect faying (back wall) surface cracks.

Minimizing Aircraft Downtime

Reducing the downtime associated with inspecting aircraft is critical. Current inspection methods require a lengthy mechanical breakdown to allow inspectors access to all the critical fastener holes. During this time-consuming process, hundreds of overhead fasteners must be inspected.

The inspection area showing hundreds of overhead fasteners

The inspection area showing hundreds of overhead fasteners

Fast Fastener Inspection

To help inspectors complete their fastener inspections more quickly, Olympus created a small-access spinner probe with two shear wave linear arrays packaged in a cylindrical case. The case magnetically couples the probe around each raised fastener head, easing the inspection process.

inspection results displaying three phased array groups

The inspection results displaying three phased array groups—two groups of sectorial scan data for detecting cracks and a third group to check the quality of the coupling. The easy-to-interpret data is recorded in real time to visually display cracks detected in the C-scan and the couplant channel as a thin red line.

First, an inspector applies a light mist or couplant to the fastener. The probe then magnetically attaches to the fastener head, and the inspector turns the probe 180 degrees to achieve a full 360-degree inspection. The solution saves time and avoids the need for mechanical dissasembly.

Inspecting a fastner under an airplane

Inspecting a fastner under an airplane

The results of inspecting a fastener using the probe

The results of inspecting a fastener using the probe

Conclusion

The Olympus small-access spinner probe improves coupling, detection, inspection time, and provides easy-to-interpret phased array ultrasound data. Please contact SCE.PM@olympus-ossa.com if you would like more information about this application, support for solving your own application, or need customized ultrasound transducers.

Images supplied by the US Naval F-5 Adversary Program.

Olympus IMS

이 애플리케이션에 사용되는 제품
위상 배열 응용 분야별 프로브의 범위는 0.5MHz에서 18MHz이며, 16, 32, 64 또는 128개의 소자가 있을 수 있습니다. 특수 프로브는 최대 수백 개의 소자를 가지고 있을 수 있습니다.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
아래 양식을 작성하여 원하는 내용을 알려주십시오.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.