Immersion Flat with Radius (IFWR) Phased Array Probes

Overview

Olympus manufactures custom immersion flat with radius (IFWR) phased array probes to increase coverage, improve detectability, and simplify data analysis. Mistras Group Inc. has increased productivity by using a single custom Olympus 3.5MHz 64 element IFWR probe; replacing two probes in their composite inspection setup. Mistras Group Inc. provided the following details and graphics outlining their success.

Old Technique

Mistras previously used 1 linear 64 element, 1 concave 32 element probe, and the OmniScan MX to inspect 8 zones across a composite part. The inspection with two probes took approximately 2.5 hours.

Figure 1: 8 zones to cover the entire composite piece
Figure 1: 8 zones to cover the entire composite piece

Firgure 2: Two setups required to cover the entire partFirgure 2: Two setups required to cover the entire part


Firgure 2: Two setups required to cover the entire part

The C-scan data recored from multiple probes and passes becomes more difficult to record and analyze. Each scan must be properly identified to ensure acurrate analysis.

Figure 3: C-scan data is recored for each zone
Figure 3: C-scan data is recored for each zone

New Technique

Using the Olympus custom IFWR probe, inspection of all 8 zones can be completed with one probe in two passes; reducinig inspection time by approximately 50%.

Figure 4: Custom Immersion Flat With Radius (IFWR) probe setup
Figure 4: Custom Immersion Flat With Radius (IFWR) probe setup

Reducing quantity of probes while increasing coverage has proven to simplify recording and analyzing data. Each part now has only two C-scan’s to analyze.

Figure 5: Data captured from one pass covers 4 zones
Figure 5: Data captured from one pass covers 4 zones

Conclusion

Olympus has worked with Mistras Group Inc. to provide a custom probe which has proven to reduce inspection time, improve detectability, and simplify data analysis. Olympus has the capability to manufacture IFWR probes to customer specifications and specific part requirements.

To inquire for custom probe possibilities specific to your application please contact SCE.PM@olympusndt.com or submit details via our online custom probe form.

Olympus IMS

이 애플리케이션에 사용되는 제품
OmniScan ™ X3 시리즈의 모든 결함 탐상기는 완전한 위상 배열 툴박스입니다. 혁신적인 TFM 및 고급 PA 기능은 강력한 소프트웨어 도구와 간단한 워크 플로우로 생산성을 향상시키는 동시에 결함을 확실하게 식별하는 데 도움이됩니다.
단일 그룹인 경량 옴니스캔 SX는 읽기 쉬운 8.4인치(21.3cm) 터치 스크린을 갖추고 있으며, 비용 효율적인 솔루션을 제공합니다. 옴니스캔 SX는 SX PA와 SX UT의 두 가지 모델로 제공됩니다. SX PA는 UT 전용 SX UT와 마찬가지로 P/E, P-C 또는 TOFD 검사를 위한 재래식 UT 채널을 장착한 16:64PR 장치입니다.
옴니스캔 MX2는 이제 UT 채널이 있는 새로운 위상 배열 모듈(PA2), TOFD(회절 비행 시간)에 사용할 수 있는 새로운 2채널 재래식 초음파 모듈(UT2) 및 성공적인 옴니스캔 MX2 플랫폼의 기능을 확장하는 새로운 소프트웨어 프로그램을 제공합니다.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
아래 양식을 작성하여 원하는 내용을 알려주십시오.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.