Item NumberPart CodeNominal Element Size (mm)Nominal Element Size (in)Angle (°)SeriesTemperature Range °FTemperature Range °CEstimated ship*
U8700011
ABWHT-2-45
13 x 250.50 x 1.0045°高温5002606 weeks
U8700012
ABWHT-2-60
13 x 250.50 x 1.0060°高温5002606 weeks
U8700013
ABWHT-2-70
13 x 250.50 x 1.0070°高温5002606 weeks
U8700007
ABWHT-1-45
130.545°高温5002606 weeks
U8700008
ABWHT-1-60
130.560°高温5002606 weeks
U8700009
ABWHT-1-70
130.570°高温5002606 weeks
U8700015
ABWHT-3-45
25145°高温5002605 weeks
U8700016
ABWHT-3-60
25160°高温5002605 weeks
U8700017
ABWHT-3-70
25170°高温5002605 weeks

* Product lead times vary. You will receive shipping confirmation 1-2 business days after placing your order.
If you need a product sooner, please contact a sales representative for more details.

Web Store not Available

The Olympus web store is currently not available in your country. Please contact your local sales representative for further product information and purchases.