Bond Testing in Composite Power Line Insulators


Bond Testing in Composite Power Line Insulators

Application

Verifying the integrity of bonding between the silicone skirts and the composite core of composite high-voltage power line insulators.

Background

The high-voltage pylon insulators used for power transmission lines and railroad traction power wires have traditionally been made of glass or ceramic, but many users are now switching to composite insulators because of their advantages with respect to weight, durability, and environmental performance. These insulators consist of a fiber-reinforced polymer (FRP) composite core coated with a layer of silicone rubber and bracketed with metal end fittings. Good bonding between the silicone and the FRP is essential for proper electrical performance, since bond failures may result in flashovers. Ultrasonic flaw detectors can be used to quickly and nondestructively check the integrity of these bonds, both at the manufacturing stage and in service.

Bond Testing in Composite Power Line Insulators
Bond Testing in Composite Power Line Insulators

Equipment

Any of the Olympus EPOCH® series instruments, including the EPOCH 650 and EPOCH 6LT flaw detectors, can be used for this test, along with a small diameter contact transducer, such as a V112-RM (10 MHz, 0.25 in./6.25 mm diameter), that fits in the space between the flared skirts.

Procedure

The phase or polarity of an echo reflected from the boundary between two materials depends on the relative acoustic impedances (density × sound velocity) of the materials. When the first material has an acoustic impedance higher than the second, the echo polarity is negative. When the first material has an acoustic impedance lower than the second, the echo polarity is positive. Silicone has an impedance lower than fiberglass but higher than air. Thus a bonded silicone/FRP joint returns a positive echo, and a disbonded silicone/air boundary returns a negative echo. In this test, the flaw detector is set to RF display mode. The operator identifies the echo from the silicone/FRP boundary, sets it in the center of the screen, and sets gain to approximately 80% screen height. The display patterns should then be as follows:

Bonded Joint PositivePeak

Bond Testing in Composite Power Line Insulators

Disbonded Joint Negative Peak

Bond Testing in Composite Power Line Insulators

If the thickness and/or concentricity of the silicone coating are of interest, they can be measured at the same time by calibrating the instrument to the velocity of silicone (typically about 1.48 mm/uS or .058 in/uS) and placing a measurement gate on the echo.

Olympus IMS
ProductsUsedApplications

The EPOCH 6LT portable ultrasonic flaw detector is optimized for one-handed operation and delivers excellent performance in rope access and high-portability applications. Lightweight with an ergonomic design, the instrument fits securely in a user’s hand or can be strapped to the leg for rope access applications.
Ultrasonic transducers are used for applications as diverse as flaw detection, thickness gaging, materials research and medical diagnostics. More than 5000 ultrasonic transducer types come in many styles, element diameters, frequencies, and connector styles.
The EPOCH 650 is a conventional ultrasonic flaw detector with excellent inspection performance and usability for a wide variety of applications. This intuitive, rugged instrument is a continuation of the popular EPOCH 600 flaw detector with additional capabilities.
Performs eddy current array testing inspections. The test configuration supports 32 sensor coils (up to 64 with an external multiplexer) working in bridge or transmit-receive mode. The operating frequency ranges from 20 Hz to 6 MHz with the option of using multiple frequencies in the same acquisition.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK