Turbine Dovetail Inspection Using Eddy Current Arrays
General description of the application
Dovetail inspection can be extremely time consuming and demanding. One of the alternatives is to use a complex robot, but it is still slow and very costly.
The system we are proposing completely covers the part to be inspected in one single pass. It uses an array of elements laid out in a probe design perfectly adapted to the part profile.
Typical inspection requirement
• Complete part coverage
• Defect sizing and positioning
Defects detected
• 0.8 mm x 0.4 mm x 0.1 mm (30 mils x 15 mils x 4 mils)
• Generally parallel to the inspection displacement
Description of the solution
• Multichannel probe
• Real-time C-scan display with pseudo-isometric view
• 24-channel probe
• Probe shaped to fit the part profile
Description of the inspection system
• MultiScan MS-5800™ with MultiView™ software running on a laptop or desktop PC
• Probe with external multiplexer unit
• Optional encoder
Parts to inspect
Engine disk dovetail
Defects to be detected
Fatigue cracks
Method of inspection
The probe is balanced on the defect-free dovetail like any other ET system. After calibration on a long calibration defect, the probe is pushed inside each dovetail. The data appears in real-time on the computer screen as a C-scan.
The preferred display is the C-scan. It makes an excellent cartography of the part, especially if an encoder is used.
It is also possible to have access to the impedance plane and strip charts of each channel to make an independent analysis of each signal. This is possible because all the channels are saved individually and integrally.
Le logiciel d’acquisition et d’analyse MultiView pour l’inspection de tubes permet l’analyse du plan de tension, le traçage des courbes théoriques du plan de tension, la superposition de mesures circonférentielles, l’étalonnage de trois courbes de profondeur à partir d’un seul point de référence, l’étalonnage de plan de tension sans signal provenant de la plaque de support et la commande logicielle à double pilote. De plus, ce logiciel offre une vue cylindrique hors ligne, des curseurs de mesure en profondeur, l’affichage de la perte de paroi (%), et l’acquisition du C-scan en temps réel.
Sorry, this page is not available in your country
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.