The DELTA Takes Phosphorus (P) in Steel Detection Limits to an All Time Low!

The right amount of P content can increase yield and tensile strength of low carbon steel improving its processing, matching and corrosion resistance characteristics. However, too much P can cause brittleness which reduces the steel's strength and ductility, and ultimately its value. Ultra-low carbon steels and line pipe steels are among the most demanding for low P content - less than 0.01%. Hence, highly accurate measurements of low levels of P in ferrous alloys are critical for predicting quality for end use and ultimately the selling point of the piping and components. The DELTA Premium, the latest Olympus development in HHXRF goes to an all time high in accuracy and an all time low in detection limits for P in steel. It detects trace levels of P as low as 0.014% in carbon steel without vacuum or helium purge attachments.

Oil Jetty
Oil Jetty Photo by DH Wright, 2009

Accurate Low Limits of Detection of Phosphorus (P) is Critical for Line Pipe Steels
Standard wt % P, Assay wt % P, DELTA Measured
FXS313 0.014 0.012
FXS314 0.037 0.036
FXS315 0.056 0.053
FXS316 0.077 0.079
FXS317 0.109 0.114
FXS318 0.321 0.319
Table X. Analysis results of six certified reference standards with varying P content
HHXRF Measurements taken with DELTA Premium for 5 sec Beam 1; 120 sec Beam 2

Analysis data

Assay results

The DELTA Premium detects P in Steel with a correlation coefficient (R2) of 0.9993 in the range or 0.014 to 0.321!

In addition to testing for P in steel, the scrap processing recycling industry depends on HHXRF analyzers for metal sorting, buying and selling. Managers cannot afford to depend on out-of-date and unreliable equipment, or untimely support of equipment. They also cannot afford to fall behind the technology curve. The analytical capabilities of HHXRF continue expanding, and new features continually continually enable operators to be more effective and efficient. Upgrade your HHXRF to the DELTA - the latest HHXRF loaded with innovative features and backed by the industry's best service and support.

Handheld XRF for Metals & Alloys Industries

Iron & Steel Non-ferrous Scrap & Secondary

Iron and steel are the most widely used of metals and alloys. Lighter metals, non-ferrous, newly developed and exotic alloys are also utilized extensively, but iron and steel are considered the basic raw materials for the majority of industrial goods and construction. Although produced from ores mined around the globe, steel is one of the most recycled materials in the world. From base form to recycled materials to finished products, metals and alloys are integral to the fabric of society, the consumption of which is often considered a primary indicator of development and economic progress.

Metals Alloys is a serious, dynamic business.

The DELTA XRF analyzer is an essential tool for all businesses involved in the trade or use of metals alloys. In seconds, you can nondestructively measure 25+ elements. Turnings, shavings, rods, wires, small parts, components, sizeable materials and large structures can all be analyzed directly, non-destructively. How you get them, how you make them, how you use them, how you sell them is how you measure them. Whether you check purity, chemistry, or grade ID for highest value, maximum recovery, quality, conformance, or maintenance and safety, our DELTA XRF analyzer will give you immediate answers to take action on now.

Delta Handheld XRF testing alloys
Olympus IMS

Productos para la aplicación
Los analizadores XRF portátiles DELTA, dedicados a la identificación positiva del material (PMI), permiten analizar aleaciones de forma no destructiva para identificar con rapidez y precisión los grados de las aleaciones y medir la composición de los metales. Efectúe inspecciones PMI y ensayos de control/aseguramiento de calidad, que cubren desde una identificación simple de grados, en conformidad con las especificaciones del control de calidad, hasta inspecciones de materiales entrantes y verificaciones de productos finales.
Este modelo de analizador portátil DELTA proporciona la identificación de elementos en 1 o 2 segundos en la mayoría de los grados de aleación y metales puros. Su diseño, pensado para ofrecer durabilidad, soporta los ambientes de procesamiento más extremos. Clasifique y analice aleaciones con rapidez y fiabilidad en una amplia variedad de materiales ferrosos y no ferrosos en tan solo segundos.
El DELTA Element es un analizador de fluorescencia de rayos X (XRF) económico y de alto rendimiento que ha sido optimizado para las aplicaciones de clasificación de chatarra, identificación positiva de los materiales (PMI), control y aseguramiento de calidad de aleaciones (QA/QC), y análisis de metales preciosos.
El DELTA Professional, dotado de un detector de deriva de silicio (SDD) de gran superficie y tubo de rayos X avanzado de 4W, proporciona un rendimiento superior en términos de velocidad, límites de detección y escala de elementos. Analiza elementos que van desde el magnesio (Mg) hasta elementos superiores en aleaciones y minerales. Este analizador representa la mejor solución de la serie de analizadores DELTA de Olympus.
Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.