Wanddickenmessung Mehrschichtkunstsoffen


Application: Measurement of individual layers and total thickness in coextruded plastic, both raw sheet stock and molded products.

Background: Sheet stock of engineering thermoplastics such as acrylonitrile butadiene styrene (ABS) and acrylic, used to form a wide variety of molded consumer products such as automotive interior parts, refrigerator shelves, and plastic window frames, is sometimes produced as two coextruded layers, an outer cap layer that provides cosmetic properties such as a glossy surface, and a base layer that optimizes structural properties. Manufacturers and fabricators need to measure the thickness of the cap layer as well as total product thickness to insure compliance with specifications.
Equipment: It is often possible to measure cap layer, base layer, and total thickness both in the sheet stock and in the final molded product using a Model 38DL PLUS thickness gage with the optional Multi-Measurement software and a common delay line transducer such as an M208-RM (20 MHz) or an M202-RM (10 MHz). Cap layers may often be measured down to a minimum thickness of 0.008" (0.20 mm) or less. The primary limitation on ultrasonic testing of this class of products is that occasionally the cap layer and base layer are both made materials with very similar acoustic properties, in which case there can be insufficient reflection from the boundary between them to measure the layers separately. For this reason, performance should be evaluated on samples of the actual product to be measured. Total product thickness can be measured in all cases.

Typical Procedure: The waveforms below show simultaneous measurement of cap layer and base layer in a typical coextruded ABS plastic part, using an M208 transducer. The echoes seen on the screen represent the outer surface of the part, the boundary between the cap layer and the base layer, and the inner surface of the part.


cap layer measurement



base layer measurement

As with any ultrasonic thickness measurement, accuracy is dependent on proper sound velocity calibration. Velocity calibration must be performed for each material being measured, on samples of known thickness.

Olympus IMS
ProductsUsedApplications

Das 45MG ist ein Ultraschalldickenmesser mit Standardmessfunktionen und optionalen Softwarefunktionen. Dieses einzigartige Gerät ist mit der gesamten Palette von Olympus Einzelschwinger- und Sender-Empfängermessköpfen kompatibel, was dieses innovative Gerät zu einer Universallösung für nahezu jeden Anwendungsbereich in der Dickenmessung macht.
Das 38DL PLUS ist ein hochentwickelter Ultraschalldickenmesser. Es misst mit Sender-Empfängerschallkopf Korrosionen im Inneren von z. B. Rohren und besitzt eine THRU-COAT und Echo-Echo-Funktion. Es misst mit Einschwingermessköpfen dünne, sehr dicke oder mehrschichtige Werkstoffe sehr genau.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

Diese Seite verwendet Cookies, um die Leistung zu verbessern, Datenverkehr zu analysieren und Werbeanzeigen zu personalisieren. Wenn Sie Ihre Browser-Einstellungen nicht ändern, werden weiterhin Cookies auf dieser Webseite verwendet. Um zu erfahren wie Cookies auf dieser Webseite verwendet werden und wie Sie unsere Verwendung von Cookies beschränken, lesen Sie unsere Cookie-Richtlinie.

OK