Multimedia
Anwendungsbeispiele
Zurück zur Datenbank

Height Measurement of Microscopic Bumps on an Integrated Circuit


Image of microscopic bumps on an integrated chip.
Image of microscopic bumps on an integrated chip.

Measuring the Height of Microscopic Bumps for Flip Chip Bonding

Mounting integrated circuit (IC) chips on a printed circuit board (PCB) using a grid of microbump solders is a technique called flip chip bonding. To ensure a proper connection between the IC and PCB, the height of the bumps must be uniform. For this reason, the bump height must be measured quickly and accurately during production.

Measuring the Height of Microscopic Bumps for Flip Chip Bonding

Measuring the Height of Microscopic Bumps for Flip Chip Bonding

Olympus' Solution: Height Measurement Using the OLS5000 Industrial Microscope

The LEXT OLS5000 3D laser scanning microscope can provide precise and fast height measurement at the microscopic level thanks to a range of innovative features:

(1) With the microscope’s unique PEAK algorithm, it takes only about 10 seconds to acquire data in a 649 µm × 640 µm area of bumps 20 µm high.

(2) The system has a multiple-area data acquisition function, which enables you to specify multiple areas and obtain the data of those areas simultaneously.

Olympus' Solution: Height Measurement Using the OLS5000 Industrial Microscope
 

(3) By setting the height reference plane for the image to be acquired, you can measure the heights of all the bumps within the field of view at one time.

Setting the reference plane for height measurement.

Setting the reference plane for height measurement.

All the bump heights within the field of view can be automatically measured.

All the bump heights within the field of view can be automatically measured.
 

(4) All the details and steps of an operation you have performed can be stored as a template when producing a report. When repeating a measurement, you can reload the template to obtain a report analyzed using the same procedure parameters.

(5) Typical bump measuring systems inspect bumps at high speed, but they do not work well for very fine microscopic bumps. The OLS5000 microscope helps ensure accuracy and reproducibility suitable for the height measurement of microscopic bumps.

Olympus IMS
Verwendete Produkte

Mit dem konfokalen LEXT OLS5000 Laser-Scanning-Mikroskop können Sie auf einfachste Weise berührungslose und zerstörungsfreie 3D-Prüfungen und Messungen vornehmen. Durch einfaches Anklicken der Startschaltfläche lassen sich feinste Formen im Submikrometerbereich messen. Die Kombination aus Bedienerfreundlichkeit und zukunftsweisenden Funktionen sorgt für eine viermal schnellere Prüfgeschwindigkeit als bei unserem Vorgängermodell. LEXT Objektive mit langem Arbeitsabstand und Erweiterungsstativ-Option erlauben die Prüfung von bis zu 210 mm großen Objekten.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

Diese Seite verwendet Cookies, um die Leistung zu verbessern, Datenverkehr zu analysieren und Werbeanzeigen zu personalisieren. Wenn Sie Ihre Browser-Einstellungen nicht ändern, werden weiterhin Cookies auf dieser Webseite verwendet. Um zu erfahren wie Cookies auf dieser Webseite verwendet werden und wie Sie unsere Verwendung von Cookies beschränken, lesen Sie unsere Cookie-Richtlinie.

OK