Embossing on the surface of dashboards, seats, door trim, and other interior components of automobiles contribute to the product’s aesthetic value and influence the satisfaction of car buyers.

Door switch buttons are one of these aesthetic components, and the material, texture, and color of the buttons in proportion to the surrounding door trim has a significant influence on the value of the overall product. Although the emotional impression derived from perceived differences is important, automobile manufacturers require a quantitative evaluation.

(2) Olympus' solution

The texture of the embossing on door swtiches can be evaluated using Olympus' LEXT OLS5000 3D scanning laser microscope, which is capable of high-resolution and high-precision 3D data display and surface roughness analysis. The LEXT OLS5000 microscope’s laser optical system is a noncontact type, yet it provides the same roughness (two-dimensional) parameters as contact-type microscopes and produces compatible results. The OLS5000 microscope also provides three-dimensional roughness parameters that comply with ISO25178, enabling you to obtain more information than mere line roughness through surface-area evaluation using 3D images and numerical data. High resolution data can be acquired for multiple points on the surface by saving measurement coordinates in Stitching mode, increasing the field of view exponentially.

Images

(1) Sample A (20X objective, 3×3 stitching of 640 µm2 points for an effective field of vision: 1800 µm2)

Measurement point 1

Measurement point 1

Measurement point 2

Measurement point 2

Measurement point 3

Measurement point 3

Parameter Sq [µm] Sa [µm] Sz [µm]
Point 1 3.402 2.536 27.709
Point 2 4.655 3.438 36.533
Point 3 4.616 3.541 37.549
Average 4.367 3.299 33.438
Standard deviation 0.647 0.519 4.527


(2) Sample B (20X objective, 3 ×3 stitching of 640 µm2 points for an effective field of vision: 1800 µm2)

Measurement point 1

Measurement point 1

Measurement point 2

Measurement point 2

Measurement point 3

Measurement point 3

Parameter Sq [µm] Sa [µm] Sz [µm]
Point 1 8.467 6.927 57.411
Point 2 9.235 7.576 57.320
Point 3 9.190 7.488 63.444
Average 8.983 7.340 59.441
Standard deviation 0.354 0.288 2.867
Olympus IMS
Verwendete Produkte

Mit dem konfokalen LEXT OLS5000 Laser-Scanning-Mikroskop können Sie auf einfachste Weise berührungslose und zerstörungsfreie 3D-Prüfungen und Messungen vornehmen. Durch einfaches Anklicken der Startschaltfläche lassen sich feinste Formen im Submikrometerbereich messen. Die Kombination aus Bedienerfreundlichkeit und zukunftsweisenden Funktionen sorgt für eine viermal schnellere Prüfgeschwindigkeit als bei unserem Vorgängermodell. LEXT Objektive mit langem Arbeitsabstand und Erweiterungsstativ-Option erlauben die Prüfung von bis zu 210 mm großen Objekten.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

Diese Seite verwendet Cookies, um die Leistung zu verbessern, Datenverkehr zu analysieren und Werbeanzeigen zu personalisieren. Wenn Sie Ihre Browser-Einstellungen nicht ändern, werden weiterhin Cookies auf dieser Webseite verwendet. Um zu erfahren wie Cookies auf dieser Webseite verwendet werden und wie Sie unsere Verwendung von Cookies beschränken, lesen Sie unsere Cookie-Richtlinie.

OK