1 00:00:04,500 --> 00:00:06,100 Olympus is proud to present 2 00:00:06,100 --> 00:00:07,700 the next generation of dedicated 3 00:00:07,700 --> 00:00:09,100 phased array probes and wedges 4 00:00:09,100 --> 00:00:14,366 for weld inspection using the Omniscan® SX. 5 00:00:14,366 --> 00:00:16,233 The new probe and wedge designs 6 00:00:16,233 --> 00:00:17,533 offer many improvements 7 00:00:17,533 --> 00:00:20,000 over the previous generation. 8 00:00:20,000 --> 00:00:23,766 two housings and three configurations are possible. 9 00:00:23,766 --> 00:00:26,400 a 32-element A31 probe 10 00:00:26,400 --> 00:00:28,833 and 32- and 64- element versions 11 00:00:28,833 --> 00:00:30,900 of the A32 probe. 12 00:00:30,900 --> 00:00:32,933 The new IHC wedges are made 13 00:00:32,933 --> 00:00:34,800 entirely out of Rexolite®. 14 00:00:34,800 --> 00:00:36,433 When compared with previous 15 00:00:36,433 --> 00:00:38,400 aluminum-ring wedges, they are: 16 00:00:38,400 --> 00:00:40,800 Lighter for greater stability on scanners, 17 00:00:40,800 --> 00:00:43,100 More ergonomic during manual scanning 18 00:00:43,100 --> 00:00:44,766 and more efficient when providing 19 00:00:44,766 --> 00:00:47,133 irrigation for optimal coupling. 20 00:00:47,133 --> 00:00:49,200 All wedges feature mounting holes 21 00:00:49,200 --> 00:00:51,766 for the Mini-Wheel™ encoder. 22 00:00:51,766 --> 00:00:54,400 The cable exit is designed for easy integration 23 00:00:54,400 --> 00:00:57,833 of the probes with Olympus scanners. 24 00:00:57,833 --> 00:00:59,633 There is a new wear protection system 25 00:00:59,633 --> 00:01:01,566 that consists of two metal strips 26 00:01:01,566 --> 00:01:03,566 delivering reliable wear protection 27 00:01:03,566 --> 00:01:05,733 and consistent data acquisition. 28 00:01:05,733 --> 00:01:07,800 These probes and wedges also have 29 00:01:07,800 --> 00:01:09,866 an improved signal-to-noise ratio. 30 00:01:09,866 --> 00:01:12,700 The sound path is shorter for better sound transmission, 31 00:01:12,700 --> 00:01:14,833 and there are multiple design improvements 32 00:01:14,833 --> 00:01:16,833 to the probe and wedge for optimized acoustics 33 00:01:16,833 --> 00:01:19,300 and reduced adverse echoes. 34 00:01:19,300 --> 00:01:21,533 A line of high-temperature wedges 35 00:01:21,533 --> 00:01:22,966 compliment the A31 36 00:01:22,966 --> 00:01:25,000 and A32 weld series probes. 37 00:01:25,000 --> 00:01:27,100 These wedges are made of Ultem™ resin 38 00:01:27,100 --> 00:01:30,866 and can withstand temperatures up to 150 °C 39 00:01:30,866 --> 00:01:33,000 or 300 °F 40 00:01:33,000 --> 00:01:34,700 These wedges are available in 41 00:01:34,700 --> 00:01:36,700 the standard 0° delay line 42 00:01:36,700 --> 00:01:39,866 and 55° for shear wave inspection. 43 00:01:39,866 --> 00:01:41,333 The wedges are capable of 44 00:01:41,333 --> 00:01:46,366 manual-encoded inspection using the Mini-Wheel encoder. 45 00:01:46,366 --> 00:01:48,133 The wedge comes with a protective sleeve 46 00:01:48,133 --> 00:01:49,966 to protect the rubber probe cable 47 00:01:49,966 --> 00:01:52,933 in case of accidental contact with the hot part. 48 00:01:52,933 --> 00:01:54,466 This high-temperature solution 49 00:01:54,466 --> 00:01:55,733 is designed to be used with an 50 00:01:55,733 --> 00:01:58,166 ON and OFF duty cycle. 51 00:01:58,166 --> 00:01:59,600 Software improvements also 52 00:01:59,600 --> 00:02:01,600 help speed up weld inspection. 53 00:02:01,600 --> 00:02:04,366 MXU software adds the compound scan 54 00:02:04,366 --> 00:02:05,633 as an additional selection 55 00:02:05,633 --> 00:02:07,400 within the OmniScan Setup wizard 56 00:02:07,400 --> 00:02:11,333 making it is just as easy to set up as a sectorial scan. 57 00:02:11,333 --> 00:02:12,766 The compound scan is an improved 58 00:02:12,766 --> 00:02:15,633 focal law strategy to increase the volumetric coverage 59 00:02:15,633 --> 00:02:17,533 of welds and other applications 60 00:02:17,533 --> 00:02:19,600 while reducing the number of required groups 61 00:02:19,600 --> 00:02:22,000 and scans during inspections. 62 00:02:22,000 --> 00:02:23,466 The HST-Lite scanner 63 00:02:23,466 --> 00:02:25,500 is the perfect choice for cost-effective, 64 00:02:25,500 --> 00:02:27,233 one-channel TOFD inspections 65 00:02:27,233 --> 00:02:29,666 when signal quality is important. 66 00:02:29,666 --> 00:02:31,500 The combination of magnetic wheels 67 00:02:31,500 --> 00:02:33,466 and spring-loaded probe holders 68 00:02:33,466 --> 00:02:35,233 offer the stability required to perform 69 00:02:35,233 --> 00:02:39,033 high-quality, one-line inspections. 70 00:02:39,033 --> 00:02:40,566 The scanner can be operated 71 00:02:40,566 --> 00:02:42,900 using only one hand and will attach 72 00:02:42,900 --> 00:02:44,633 to ferromagnetic surfaces 73 00:02:44,633 --> 00:02:47,566 even when in an upside-down position. 74 00:02:47,566 --> 00:02:49,366 The HST-Lite scanner, 75 00:02:49,366 --> 00:02:50,833 when purchased as a kit, 76 00:02:50,833 --> 00:02:53,266 comes standard with stainless steel TOFD wedges. 77 00:02:53,266 --> 00:02:57,433 Stainless steel wedges offer several advantages, including: 78 00:02:57,433 --> 00:02:59,066 Better wear resistance 79 00:02:59,066 --> 00:03:00,066 Better coupling 80 00:03:00,066 --> 00:03:01,200 A shorter approach 81 00:03:01,200 --> 00:03:04,733 and more ruggedness for a longer life. 82 00:03:04,733 --> 00:03:07,433 Designed specifically for use with the COBRA® scanner, 83 00:03:07,433 --> 00:03:09,500 an additional line of TOFD wedges 84 00:03:09,500 --> 00:03:12,066 are available for low profile inspections. 85 00:03:12,066 --> 00:03:15,300 These wedges can be fitted with 3 mm element diameter 86 00:03:15,300 --> 00:03:19,966 ST1 probes to inspect 1-inch to 4.5-inch pipes. 87 00:03:19,966 --> 00:03:21,466 These wedges are available 88 00:03:21,466 --> 00:03:23,966 in various longitudinal refracted angles. 89 00:03:23,966 --> 00:03:26,500 They can be ordered for specific diameters, 90 00:03:26,500 --> 00:03:28,066 or customers can purchase a kit 91 00:03:28,066 --> 00:03:30,900 covering the complete diameter range. 92 00:03:30,900 --> 00:03:34,233 For more information on weld solutions with the Omniscan SX 93 00:03:34,233 --> 00:03:36,666 contact your local Olympus representative, 94 00:03:36,666 --> 00:03:40,133 or visit our website.