1 00:00:06,709 --> 00:00:10,606 Building on an already strong selection of pipeline products, 2 00:00:10,608 --> 00:00:14,898 Olympus NDT now offers a Guided Wave inspection system 3 00:00:14,899 --> 00:00:17,758 for the detection of corrosion and metal loss 4 00:00:17,759 --> 00:00:19,864 in piping and pipeline. 5 00:00:19,866 --> 00:00:23,358 Used as a screening tool, the UltraWave LRT 6 00:00:23,359 --> 00:00:27,603 significantly increases the efficiency and productivity 7 00:00:27,605 --> 00:00:30,258 of corrosion management projects. 8 00:00:30,260 --> 00:00:33,659 Guided wave technology is a nondestructive testing method 9 00:00:33,661 --> 00:00:37,816 that is widely applied to structural- integrity monitoring programs 10 00:00:37,818 --> 00:00:41,504 in the oil, gas, and chemical industries. 11 00:00:41,506 --> 00:00:44,954 With an inspection-range potential of hundreds of meters, 12 00:00:44,956 --> 00:00:48,268 and 100% pipe-wall coverage, 13 00:00:48,270 --> 00:00:51,550 this technique increases inspection productivity 14 00:00:51,551 --> 00:00:53,994 for conventional above ground pipe, 15 00:00:53,996 --> 00:00:56,414 and is also very useful for the inspection 16 00:00:56,416 --> 00:00:59,418 of pipes with limited access. 17 00:00:59,419 --> 00:01:01,821 Combined with other NDT techniques, 18 00:01:01,823 --> 00:01:04,438 a guided wave system will help to maximize 19 00:01:04,439 --> 00:01:06,625 the efficiency of inspection projects, 20 00:01:06,626 --> 00:01:11,246 without compromising data quality. 21 00:01:11,248 --> 00:01:13,081 The Olympus UltraWave LRT system 22 00:01:13,083 --> 00:01:14,966 is a turnkey solution, 23 00:01:14,968 --> 00:01:17,291 which includes all the tools and accessories 24 00:01:17,293 --> 00:01:20,914 that the user will need to perform inspections. 25 00:01:20,916 --> 00:01:23,118 A complete standard kit comes packed 26 00:01:23,119 --> 00:01:26,145 in three rolling cases to allow for easy shipping 27 00:01:26,146 --> 00:01:28,976 and transportation on-site. 28 00:01:28,978 --> 00:01:31,531 The low profile collar allows for inspection 29 00:01:31,533 --> 00:01:33,620 in limited access areas 30 00:01:33,621 --> 00:01:35,959 and ensures a constant contact of the probe 31 00:01:35,961 --> 00:01:39,283 on the pipe during the inspection. 32 00:01:39,285 --> 00:01:42,261 The UltraWave LRT user-friendly software 33 00:01:42,263 --> 00:01:45,301 provides the operator with a step-by-step wizard 34 00:01:45,303 --> 00:01:47,779 for entering the inspection parameters, 35 00:01:47,781 --> 00:01:50,791 including the identification of each inspected line 36 00:01:50,793 --> 00:01:53,969 and its location, as well as the pipe size, 37 00:01:53,971 --> 00:01:57,438 material, configuration, and more. 38 00:01:57,439 --> 00:02:00,666 During acquisition, the probes propagate 39 00:02:00,668 --> 00:02:04,518 low frequency ultrasonic guided waves along the structure, 40 00:02:04,520 --> 00:02:08,118 ranging from 15 to 85 kHz. 41 00:02:08,119 --> 00:02:10,083 The UltraWave LRT software 42 00:02:10,084 --> 00:02:12,796 is equipped with a unique F-scan color map 43 00:02:12,798 --> 00:02:15,171 that displays the entire frequency range 44 00:02:15,173 --> 00:02:17,979 acquired over the inspected pipe length. 45 00:02:17,981 --> 00:02:20,504 The operator can perform active focusing 46 00:02:20,506 --> 00:02:22,931 on the suspected indication. 47 00:02:22,933 --> 00:02:25,308 Synthetic focusing is used to generate 48 00:02:25,310 --> 00:02:27,171 an unrolled pipe view. 49 00:02:27,173 --> 00:02:29,913 It is performed at one selected frequency 50 00:02:29,914 --> 00:02:32,864 and shows the amplitude data of each channel 51 00:02:32,866 --> 00:02:35,766 over the entire inspected zone. 52 00:02:35,768 --> 00:02:37,973 Information about the axial position 53 00:02:37,974 --> 00:02:42,798 and circumferential extent of all defects is provided. 54 00:02:42,799 --> 00:02:45,484 Always keep in mind that a guided wave system 55 00:02:45,486 --> 00:02:47,188 is a screening tool. 56 00:02:47,189 --> 00:02:50,006 Once an area of concern has been identified, 57 00:02:50,008 --> 00:02:52,575 prove-up testing should always be performed 58 00:02:52,576 --> 00:02:56,726 on the indication using other NDT methods. 59 00:02:56,728 --> 00:02:58,786 A UT thickness gage 60 00:02:58,788 --> 00:03:00,651 or a Phased-Array flaw detector 61 00:03:00,653 --> 00:03:03,618 can be used to confirm the exact remaining wall thickness 62 00:03:03,620 --> 00:03:08,293 of the pipe at the location specified by the UltraWave LRT. 63 00:03:08,295 --> 00:03:12,563 Olympus NDT offers training on the guided wave technique 64 00:03:12,565 --> 00:03:16,224 and inspection with the UltraWave LRT system. 65 00:03:16,226 --> 00:03:18,075 On-site technical support 66 00:03:18,076 --> 00:03:20,636 is also offered around the globe. 67 00:03:20,638 --> 00:03:23,451 Olympus NDT is firmly committed to providing 68 00:03:23,453 --> 00:03:25,838 the highest level of service to its customer, 69 00:03:25,839 --> 00:03:28,358 no matter where they are in the world. 70 00:03:28,359 --> 00:03:31,791 For more information on the UltraWave LRT system, 71 00:03:31,793 --> 00:03:34,213 contact your local sales representative 72 00:03:34,214 --> 00:03:42,701 or visit our website at www.olympus-ims.com.