1 00:00:04,933 --> 00:00:06,833 The HVAC and Heat Exchanger Tubing Kit using the NORTEC 600D 2 00:00:06,833 --> 00:00:08,433 Inspect more with less 3 00:00:08,433 --> 00:00:12,100 Eddy Current Testing Demonstration 4 00:00:12,100 --> 00:00:20,900 In the case 5 00:00:20,900 --> 00:00:30,033 Differential Demonstration Single Frequency 6 00:00:30,033 --> 00:00:32,900 Null 7 00:00:32,900 --> 00:00:36,200 Scan hole 8 00:00:36,200 --> 00:00:38,633 Freeze 9 00:00:38,633 --> 00:00:41,733 Hole set at 40 degrees 10 00:00:41,733 --> 00:00:47,133 Gain adjusted to 6 divisions peak to peak 11 00:00:47,133 --> 00:01:04,366 Calibration complete 12 00:01:04,366 --> 00:01:09,066 Differential Demonstration Dual Frequency with AUTO MIX 13 00:01:09,066 --> 00:01:40,933 Use AUTO MIX to detect defects under supports 14 00:01:40,933 --> 00:01:46,666 Absolute Demonstration Single Frequency 15 00:01:46,666 --> 00:01:49,066 Null 16 00:01:49,066 --> 00:01:54,300 Scan grooves 17 00:01:54,300 --> 00:01:56,566 Freeze 18 00:01:56,566 --> 00:02:01,866 Largest groove's amplitude set to 80% screen height 19 00:02:01,866 --> 00:02:05,266 Largest groove's angle set vertically 20 00:02:05,266 --> 00:02:22,266 Calibration complete 21 00:02:22,266 --> 00:02:25,500 Best Practice Tips 22 00:02:25,500 --> 00:02:29,166 Proper Pulling Technique/Method 23 00:02:29,166 --> 00:02:35,033 Good Pulling Technique/Method Bad Pulling Technique/Method 24 00:02:35,033 --> 00:02:42,633 Proper Null and Erase Good Bad