1 00:00:06,382 --> 00:00:09,343 Friction Stir Weld Inspection Solution 2 00:00:10,428 --> 00:00:17,643 Friction stir welding is a method that uses frictional heat created by a rotating tool to join two parts. 3 00:00:17,643 --> 00:00:20,855 This process can introduce various flaws at different locations in the weld. 4 00:00:20,855 --> 00:00:27,278 Voids, tunnels, lack of penatration, kissing bonds. 5 00:00:30,365 --> 00:00:35,703 Olympus gas developed a complete solution to inspect friction stir welds in fuel tanks used by the aerospace industry. 6 00:00:35,703 --> 00:00:41,333 The system is automatically calibrated on a reference standard 7 00:00:41,333 --> 00:00:48,842 by moving the inspection head over a series of manufactured flaws. 8 00:00:53,472 --> 00:00:58,435 Once calibrated, the inspection head moves to the inspection position. 9 00:00:58,435 --> 00:01:02,813 Inspection can then be performed without leaving traces of water on the surface. 10 00:01:02,813 --> 00:01:07,985 The inspection head design provides optimal positioning of the phased array probes and wedges. 11 00:01:07,985 --> 00:01:11,530 PA probes can be positioned at forward, backward, clockwise, 12 00:01:11,530 --> 00:01:15,075 counterclockwies or oblique orientation to inspect the full volume of the weld. 13 00:01:18,328 --> 00:01:22,292 Once the inspection is complete, the inspection head retracts from the surface, ready to inspect the next weld. 14 00:01:25,587 --> 00:01:29,757 www.olympus-ims.com