1 00:00:10,633 --> 00:00:13,466 The FOX-IQ® in-line XRF analyzer 2 00:00:13,466 --> 00:00:15,633 performs fully automated analysis 3 00:00:15,633 --> 00:00:18,033 for high-volume process control. 4 00:00:18,033 --> 00:00:20,800 X-ray fluorescence (XRF) 5 00:00:20,800 --> 00:00:22,600 is a proven technique used to quickly 6 00:00:22,600 --> 00:00:24,233 and nondestructively 7 00:00:24,233 --> 00:00:27,100 verify alloy grade and chemistry. 8 00:00:27,100 --> 00:00:28,633 The FOX-IQ analyzer 9 00:00:28,633 --> 00:00:31,366 provides customizable, continuous measurements 10 00:00:31,366 --> 00:00:33,266 of titanium to uranium 11 00:00:33,266 --> 00:00:35,800 on any surface and can deliver results 12 00:00:35,800 --> 00:00:38,200 in the form of material chemistry, 13 00:00:38,200 --> 00:00:40,300 accurate grade identifications, 14 00:00:40,300 --> 00:00:42,833 or pass/fail results. 15 00:00:42,833 --> 00:00:45,133 The FOX-IQ system is compact 16 00:00:45,133 --> 00:00:47,166 and has minimal power requirements, 17 00:00:47,166 --> 00:00:48,933 making it easy to integrate 18 00:00:48,933 --> 00:00:52,800 with new or existing PLC controlled processes. 19 00:00:52,800 --> 00:00:55,533 It’s engineered to operate 24/7 20 00:00:55,533 --> 00:00:57,733 and endure high levels of vibration, 21 00:00:57,733 --> 00:01:00,466 electromagnetic and acoustical noise, 22 00:01:00,466 --> 00:01:03,000 dust, and moisture. 23 00:01:03,000 --> 00:01:04,800 The FOX-IQ analyzer 24 00:01:04,800 --> 00:01:06,600 can be controlled by a PC 25 00:01:06,600 --> 00:01:08,633 or integrated with a PLC 26 00:01:08,633 --> 00:01:10,733 for automated start/stop, 27 00:01:10,733 --> 00:01:12,333 data acquisition, 28 00:01:12,333 --> 00:01:13,766 decision-making, 29 00:01:13,766 --> 00:01:16,600 and communication to external devices. 30 00:01:16,600 --> 00:01:18,700 Here’s how it works. 31 00:01:18,700 --> 00:01:21,966 The system has 3 essential components 32 00:01:21,966 --> 00:01:23,966 the probe head, 33 00:01:23,966 --> 00:01:25,633 the control box, 34 00:01:25,633 --> 00:01:27,900 and a PC. 35 00:01:27,900 --> 00:01:30,833 The control box runs the system. 36 00:01:30,833 --> 00:01:33,233 A sample is placed over the probe head 37 00:01:33,233 --> 00:01:35,633 for analysis. 38 00:01:35,633 --> 00:01:37,533 The probe head emits X-rays 39 00:01:37,533 --> 00:01:39,833 to measure the sample material. 40 00:01:39,833 --> 00:01:42,533 X-rays cause the sample to fluoresce, 41 00:01:42,533 --> 00:01:44,166 and characteristic X-rays 42 00:01:44,166 --> 00:01:45,966 are sent back to the analyzer 43 00:01:45,966 --> 00:01:48,566 where they’re counted by the detector. 44 00:01:48,566 --> 00:01:51,066 The detector measures the energy spectrum 45 00:01:51,066 --> 00:01:53,300 and determines which elements are present 46 00:01:53,300 --> 00:01:56,133 and in what concentrations. 47 00:01:56,133 --> 00:01:57,800 Using this information, 48 00:01:57,800 --> 00:01:59,766 the FOX-IQ analyzer can display 49 00:01:59,766 --> 00:02:01,633 the material chemistry 50 00:02:01,633 --> 00:02:04,700 or determine if the material meets specification 51 00:02:04,700 --> 00:02:06,466 and display a grade match 52 00:02:06,466 --> 00:02:10,400 or make a pass/fail determination. 53 00:02:10,400 --> 00:02:12,433 If your facility is automated, 54 00:02:12,433 --> 00:02:14,633 the pass/fail result can be communicated 55 00:02:14,633 --> 00:02:20,766 to a PLC for material disposition. 56 00:02:20,766 --> 00:02:22,133 To learn more about how 57 00:02:22,133 --> 00:02:24,700 the FOX-IQ in-line XRF system 58 00:02:24,700 --> 00:02:26,666 can help implement quality control 59 00:02:26,666 --> 00:02:28,400 to your production line, 60 00:02:28,400 --> 00:02:30,866 contact your local Olympus representative 61 00:02:30,866 --> 00:02:32,666 or visit our website.