Item NumberPart CodeFrequency
(MHz)
Nominal Element Size (mm)Nominal Element Size (in)Angle (°)Connector TypeEstimated ship*
U8503183
PAB-0204-60-AL-RM
2.256 x 60.250 x 0.25060° Shear Wave in SteelRight Microdot5 weeks
U8503077
PAB-0503-45-AL-RM
55 x 50.187 x 0.18745° Shear Wave in AluminumRight Microdot4 weeksPlease contact us for pricing
U8503085
PAB-0503-70-AL-RM
55 x 50.187 x 0.18770° Shear Wave in AluminumRight Microdot6 weeksPlease contact us for pricing
U8503094
PAB-0504-90-ST-RM
56 x 60.250 x 0.25090° Shear Wave in SteelRight Microdot6 weeksPlease contact us for pricing
U8503091
PAB-0504-70-AL-RM
56 x 60.250 x 0.25070° Shear Wave in AluminumRight Microdot5 weeks
U8503124
HS-225-5-45-AL-RM
53 x 60.120 x 0.25045° Shear Wave in AluminumRight Microdot5 weeks
U8503054
HS-225-5-60-AL-SM
53 x 60.120 x 0.25060° Shear Wave in AluminumStraight Microdot5 weeks
U8503092
PAB-0504-70-ST-RM
56 x 60.250 x 0.25070° Shear Wave in SteelRight Microdot5 weeks
U8435040
HS-225-5-70-ST-RM
53 x 60.120 x 0.25070° Shear Wave in SteelRight Microdot4 weeks
U8430039
PAB-0504-45-ST-RM
56 x 60.250 x 0.25045° Shear Wave in SteelRight Microdot4 weeks
U8503110
PAB-0504-60-AL-SM
56 x 60.250 x 0.25060° Shear Wave in AluminumStraight Microdot5 weeks
U8503107
PAB-0504-45-AL-RM
56 x 60.250 x 0.25045° Shear Wave in AluminumRight Microdot5 weeks
U8503053
HS-225-5-60-AL-RM
53 x 40.120 x 0.25060° Shear Wave in AluminumRight Microdot5 weeks
U8503056
HS-225-5-70-AL-SM
53 x 60.120 x 0.25070° Shear Wave in AluminumStraight Microdot14 days
U8503082
PAB-0503-60-AL-SM
55 x 50.187 x 0.18760° Shear Wave in AluminumStraight Microdot4 weeks
U8503163
PAB-0504-60-ST-RM
56 x 60.250 x 0.25060° Shear Wave in SteelRight Microdot5 weeks
U8503090
PAB-0504-60-ST-SM
56 x 60.250 x 0.25060° Shear Wave in SteelStraight Microdot5 weeks
U8435041
HS-225-5-60-ST-RM
53 x 60.120 x 0.25060° Shear Wave in SteelRight Microdot4 weeks
U8503123
HS-225-5-70-AL-RM
53 x 60.120 x 0.25070° Shear Wave in AluminumRight Microdot5 weeks
U8503106
PAB-0504-45-AL-SM
56 x 60.250 x 0.25045° Shear Wave in AluminumStraight Microdot5 weeks
U8503086
PAB-0503-70-AL-SM
55 x 50.187 x 0.18770° Shear Wave in AluminumStraight Microdot4 weeks
U8503089
PAB-0504-45-ST-SM
56 x 60.250 x 0.25045° Shear Wave in SteelStraight Microdot5 weeks
U8503127
HS-877-5-45-ST-RM
55 x 50.187 x 0.18745° Shear Wave in SteelRight Microdot5 weeks
U8503134
HS-225-5-45-AL-SM
53 x 60.120 x 0.25045° Shear in AluminumStraight Microdot5 weeks
U8503109
PAB-0504-60-AL-RM
56 x 60.250 x 0.25060° Shear Wave in AluminumStraight Microdot5 weeks
U8503093
PAB-0504-70-ST-SM
56 x 60.250 x 0.25070° Shear Wave in SteelStraight Microdot5 weeks
U8503126
HS-877-10-60-AL-SM
105 x 50.187 x 0.18760° Shear Wave in AluminumStraight Microdot5 weeksPlease contact us for pricing
U8502019
PAB-1003-60-AL-SM
105 x 50.187 x 0.18760° Shear Wave in AluminumStraight Microdot5 weeksPlease contact us for pricing
U8503177
PAB-1004-45-ST-RM
106 x 60.250 x 0.25045° Shear Wave in SteelRight Microdot5 weeks
U8503176
PAB-1004-45-AL-SM
106 x 60.250 x 0.25045° Shear Wave in AluminumStraight Microdot5 weeks
U8503096
PAB-1004-45-AL-RM
106 x 60.250 x 0.25045° Shear Wall in AluminumRight Microdot4 weeks
U8503058
HS-877-10-45-AL-SM
103 x 40.187 x 0.18745° Shear Wave in AluminumStraight Microdot5 weeks
U8503164
HS-877-10-70-AL-SM
105 x 50.187 x 0.18770° Shear Wave in AluminumStraight Microdot5 weeks

* Product lead times vary. You will receive shipping confirmation 1-2 business days after placing your order.
If you need a product sooner, please contact a sales representative for more details.

Web Store not Available

The Olympus web store is currently not available in your country. Please contact your local sales representative for further product information and purchases.